JPS55134164A - Hot zinc dipping unit for strip - Google Patents
Hot zinc dipping unit for stripInfo
- Publication number
- JPS55134164A JPS55134164A JP3841479A JP3841479A JPS55134164A JP S55134164 A JPS55134164 A JP S55134164A JP 3841479 A JP3841479 A JP 3841479A JP 3841479 A JP3841479 A JP 3841479A JP S55134164 A JPS55134164 A JP S55134164A
- Authority
- JP
- Japan
- Prior art keywords
- rolls
- wiping
- strip
- nozzles
- back surfaces
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To make possible dross-gripping and uniform wiping of face and back surfaces simultaneously, by combining two rolls of different roll diameters. CONSTITUTION:Wiping rolls 4a, 4b of different diameters are so aranged that the line connecting their centers is not horizontal, hence the strip passes between the rolls, and the rolls have preliminary wiping performance that wipes face and back surfaces equally because they are installed near the upper surface of the bath. Wiping nozzles 3 are used for spraying high press. nonoxidizing gas through the nozzle slits in order to control the plating thickness. The nozzles 3 can move on toward the strip because the wiping rolls 4a, 4b correct the C-shaped warp and restrain the shake of the strip 1.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP3841479A JPS55134164A (en) | 1979-04-02 | 1979-04-02 | Hot zinc dipping unit for strip |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP3841479A JPS55134164A (en) | 1979-04-02 | 1979-04-02 | Hot zinc dipping unit for strip |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS55134164A true JPS55134164A (en) | 1980-10-18 |
JPS5755789B2 JPS5755789B2 (en) | 1982-11-26 |
Family
ID=12524638
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP3841479A Granted JPS55134164A (en) | 1979-04-02 | 1979-04-02 | Hot zinc dipping unit for strip |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS55134164A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH03125059U (en) * | 1990-03-28 | 1991-12-18 |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP4451194B2 (en) | 2004-04-13 | 2010-04-14 | 三菱日立製鉄機械株式会社 | Liquid wiping device |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS51114334A (en) * | 1975-04-01 | 1976-10-08 | Nippon Steel Corp | Method of adjusting quantity of adhesion of plated metal in continuous molten metal plating |
-
1979
- 1979-04-02 JP JP3841479A patent/JPS55134164A/en active Granted
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS51114334A (en) * | 1975-04-01 | 1976-10-08 | Nippon Steel Corp | Method of adjusting quantity of adhesion of plated metal in continuous molten metal plating |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH03125059U (en) * | 1990-03-28 | 1991-12-18 |
Also Published As
Publication number | Publication date |
---|---|
JPS5755789B2 (en) | 1982-11-26 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS54155128A (en) | Hot dipping apparatus | |
JPS55134164A (en) | Hot zinc dipping unit for strip | |
JPS57181719A (en) | Manufacture for clean cold rolling steel plate | |
JPS5558358A (en) | Hot dipping apparatus | |
JPS5695404A (en) | Manufacture of flat steel sheet | |
JPS52133008A (en) | Intrafurnace roll for process line | |
JPS6415204A (en) | Eight-stage roll mill | |
JPS5562153A (en) | Hot dipping unit in two modes | |
JPS55107767A (en) | Controlling method for plated molten metal quantity by gas spray and gas-spraying nozzle | |
JPS5575816A (en) | Preventing method for smudge of cold rolled sheet | |
Borghesi et al. | Shape control through tension distribution control in cold strip rolling | |
JPS5641366A (en) | Structure of cooling tower of continuous high speed hot dipping facility | |
JPS5374541A (en) | Coating method | |
JPS5750220A (en) | Continuous corrugated plate forming machine | |
JPS57171550A (en) | Producing device for amorphous metallic tape | |
JPS5732358A (en) | Continuous hot dipping device | |
JPS55161058A (en) | Manufacture of continuous type one side hot dipping steel plate and its apparatus | |
JPS5398372A (en) | Method of covering by roll lamination | |
JPS55110767A (en) | Hot dipping apparatus of strip | |
JPS5687461A (en) | Continuous bubble coater | |
JPS5488858A (en) | Cold rolling method for titanium sheet | |
JPS5592203A (en) | Skin pass rolling method of cold rolled steel plate | |
Nikolaev | An Installation for Acting on the Cross-Section of Rolled Strip | |
JPS53117665A (en) | Method and apparatus for controlling tension distribution in strip rolling | |
Compton | Zincgrip OS: the Development of Armco's One Side Galvanized Sheet |