JPS54158699A - High dielectric constant ceramic compound - Google Patents

High dielectric constant ceramic compound

Info

Publication number
JPS54158699A
JPS54158699A JP6803978A JP6803978A JPS54158699A JP S54158699 A JPS54158699 A JP S54158699A JP 6803978 A JP6803978 A JP 6803978A JP 6803978 A JP6803978 A JP 6803978A JP S54158699 A JPS54158699 A JP S54158699A
Authority
JP
Japan
Prior art keywords
dielectric constant
high dielectric
mno
compound
pbo
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP6803978A
Other languages
Japanese (ja)
Inventor
Hitoshi Tanaka
Shinobu Fujiwara
Nobuaki Kikuchi
Osamu Iizawa
Kiyoshi Furukawa
Hisayoshi Kamioka
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
TDK Corp
Original Assignee
TDK Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TDK Corp filed Critical TDK Corp
Priority to JP6803978A priority Critical patent/JPS54158699A/en
Publication of JPS54158699A publication Critical patent/JPS54158699A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To obtain a ceramic compound enable of low temperature sintering and haivng high dielectric constant excellent of dielectric loss and dielectric strength, by adding specific amount of MnO into a compound containing specific ratio of PbO, Fe2O3, Nb2O5, MgO, WO3.
CONSTITUTION: 0.001W1.0 wt% of MnO is added into a compound containing 64.80W67.42 wt% of PbO, 5.81W11.46 wt% of Fe2O5, 9.65W19.07 wt% of Nb2O5, 0.3W2.93 wt% of MgO, 1.75W16.83 wt% of WO3. For example a material compound having said composition is wet mixed and temporarily burnt for 2 hours under 700W850°C then chemically reactioned and crushed again. Then proper amount of binder (PVA) is added and formed into a disc under approximately 3 ton/cm2 pressure thereafter it is enclosed in a magnetia ceramic container and burnt for 2 hours under approximately 850W950°C to obtain high dielectric constant ceramic body of Pb(Fe1/2Nb1/2)O3-Pb(Mg1/2W1/2)O3-MnO system.
COPYRIGHT: (C)1979,JPO&Japio
JP6803978A 1978-06-06 1978-06-06 High dielectric constant ceramic compound Pending JPS54158699A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP6803978A JPS54158699A (en) 1978-06-06 1978-06-06 High dielectric constant ceramic compound

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP6803978A JPS54158699A (en) 1978-06-06 1978-06-06 High dielectric constant ceramic compound

Publications (1)

Publication Number Publication Date
JPS54158699A true JPS54158699A (en) 1979-12-14

Family

ID=13362248

Family Applications (1)

Application Number Title Priority Date Filing Date
JP6803978A Pending JPS54158699A (en) 1978-06-06 1978-06-06 High dielectric constant ceramic compound

Country Status (1)

Country Link
JP (1) JPS54158699A (en)

Similar Documents

Publication Publication Date Title
JPS5593671A (en) Manufacturing method of positive electrode for nonaqueous electrolyte cell
JPS54158699A (en) High dielectric constant ceramic compound
JPS54158700A (en) High dielectric constant ceramic compound
JPS54158698A (en) High dielectric constant ceramic compound
JPS54145000A (en) High dielectric system porcelain composite
JPS5614449A (en) Binder glass composition for coating phosphor
JPS55154534A (en) Iron ore porous pellet and its manufacture
JPS5218482A (en) Blue luminescent composition
JPS5678428A (en) Magnetic oxide material
JPS54134399A (en) High dielectric constant system ceramic composite
JPS5632399A (en) Single crystal ferrite
JPS5678429A (en) Magnetic oxide material
JPS5538923A (en) Manufacture of fired pellet for production of ferroalloy
GB1299667A (en) Memory cores having rectangular hysteresis loop characteristics and method of manufacturing the same
JPS54161099A (en) High dielectric constant ceramic composition
JPS573719A (en) Preparation of gamma-type ferric oxide
JPS5614402A (en) Manufacture of stable potassium hypochlorite composition
JPS57149896A (en) Manufacture of gadolinium-gallium-garnet single crystal
JPS54126604A (en) Iron ore pellet
JPS54136697A (en) High dielectric porcelain composite
JPS56115360A (en) Preparation of blue pigment with copper
JPS54136698A (en) High dielectric porcelain composite
GB1310264A (en) Magnetic garnets
JPS54161100A (en) High dielectric constant ceramic composition
Bakhtina Phase composition and properties of refractories in the system ZrO sub 2- CaO (MgO)-Nd sub 2 O sub 5- Cr sub 2 O sub 3