JPH1091921A5 - - Google Patents
Info
- Publication number
- JPH1091921A5 JPH1091921A5 JP8-242043A JP24204396A JPH1091921A5 JP H1091921 A5 JPH1091921 A5 JP H1091921A5 JP 24204396 A JP24204396 A JP 24204396A JP H1091921 A5 JPH1091921 A5 JP H1091921A5
- Authority
- JP
- Japan
- Prior art keywords
- layer
- magnetic
- pin
- alloy
- magnetic layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (5)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP24204396A JP3181512B2 (ja) | 1996-09-12 | 1996-09-12 | デュアルスピンバルブ型素子および薄膜磁気ヘッド |
| US08/922,937 US5869963A (en) | 1996-09-12 | 1997-09-03 | Magnetoresistive sensor and head |
| KR1019970047138A KR100297043B1 (ko) | 1996-09-12 | 1997-09-12 | 듀얼스핀밸브형박막소자 |
| US09/208,354 US6153062A (en) | 1996-09-12 | 1998-12-10 | Magnetoresistive sensor and head |
| US09/640,971 US6352621B1 (en) | 1996-09-12 | 2000-08-17 | Method of manufacturing film laminate having exchange anisotropic magnetic field |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP24204396A JP3181512B2 (ja) | 1996-09-12 | 1996-09-12 | デュアルスピンバルブ型素子および薄膜磁気ヘッド |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH1091921A JPH1091921A (ja) | 1998-04-10 |
| JPH1091921A5 true JPH1091921A5 (enExample) | 2001-04-13 |
| JP3181512B2 JP3181512B2 (ja) | 2001-07-03 |
Family
ID=17083426
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP24204396A Expired - Fee Related JP3181512B2 (ja) | 1996-09-12 | 1996-09-12 | デュアルスピンバルブ型素子および薄膜磁気ヘッド |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3181512B2 (enExample) |
Families Citing this family (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US6424506B1 (en) | 1998-07-21 | 2002-07-23 | Alps Electric Co., Ltd. | Spin-valve magnetoresistive thin film element |
| JP3212567B2 (ja) | 1999-01-27 | 2001-09-25 | アルプス電気株式会社 | 磁気抵抗効果型薄膜磁気素子を備えた薄膜磁気ヘッドおよびその製造方法 |
| JP3212569B2 (ja) | 1999-01-27 | 2001-09-25 | アルプス電気株式会社 | デュアルスピンバルブ型薄膜磁気素子及び薄膜磁気ヘッド及びデュアルスピンバルブ型薄膜磁気素子の製造方法 |
| JP2003520378A (ja) * | 1999-04-28 | 2003-07-02 | シーゲイト テクノロジー エルエルシー | ピンニング層を有する巨大磁気抵抗効果センサー |
| JP2001307308A (ja) | 2000-04-24 | 2001-11-02 | Fujitsu Ltd | 磁気抵抗効果型ヘッドおよび情報再生装置 |
| JP3474523B2 (ja) | 2000-06-30 | 2003-12-08 | Tdk株式会社 | 薄膜磁気ヘッドおよびその製造方法 |
-
1996
- 1996-09-12 JP JP24204396A patent/JP3181512B2/ja not_active Expired - Fee Related
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US6430015B2 (en) | Method of fabrication of striped magnetoresistive (SMR) and dual stripe magnetoresistive (DSMR) heads with anti-parallel exchange configuration | |
| US6313973B1 (en) | Laminated magnetorestrictive element of an exchange coupling film, an antiferromagnetic film and a ferromagnetic film and a magnetic disk drive using same | |
| JP4421822B2 (ja) | ボトムスピンバルブ磁気抵抗効果センサ素子およびその製造方法 | |
| US6301089B1 (en) | Spin-valve type magnetoresistive thin film element comprising free magnetic layer having nife alloy layer | |
| JP3219713B2 (ja) | 磁気抵抗効果素子の製造方法 | |
| JP2004524708A5 (enExample) | ||
| JPH10341048A (ja) | スピンバルブ型薄膜素子 | |
| JPH10284321A (ja) | 交換結合膜とそれを用いた磁気抵抗効果素子、磁気ヘッドおよび磁気記憶装置 | |
| JPS63273372A (ja) | 磁気抵抗センサ | |
| JP2001143223A (ja) | スピンバルブ型薄膜磁気素子及び薄膜磁気ヘッド | |
| JPH11191647A5 (enExample) | ||
| WO2020137558A1 (ja) | 交換結合膜ならびにこれを用いた磁気抵抗効果素子および磁気検出装置 | |
| CN109716548B (zh) | 交换耦合膜以及使用该交换耦合膜的磁阻效应元件及磁检测装置 | |
| US7029770B2 (en) | Exchange-coupled film, spin valve film, thin film magnetic head, magnetic head apparatus, and magnetic recording/reproducing apparatus | |
| JP2001056924A5 (enExample) | ||
| JP2001118217A (ja) | スピンバルブ型薄膜磁気素子及び薄膜磁気ヘッド及びスピンバルブ型薄膜磁気素子の製造方法 | |
| US6683762B2 (en) | CPP GMR device with inverse GMR material | |
| JP3227116B2 (ja) | スピンバルブ型薄膜素子およびその製造方法 | |
| US6661623B1 (en) | Magnetic transducer with interlayer thin-film magnetic head and method of manufacturing thereof | |
| US20020044397A1 (en) | Spin valve magnetoresistance effect head and compound magnetic head using it and magnetic recording medium drive unit | |
| CN1284144C (zh) | 磁电阻效应膜,磁电阻效应磁头和固态存储器 | |
| JP3585807B2 (ja) | 磁気抵抗効果素子、磁気ヘッド、磁気ヘッドアセンブリ及び磁気記録装置 | |
| JP2001167410A (ja) | スピンバルブ型薄膜磁気素子及び薄膜磁気ヘッド | |
| JP3710324B2 (ja) | スピンバルブ型薄膜磁気素子及び薄膜磁気ヘッド及びスピンバルブ型薄膜磁気素子の製造方法 | |
| JPH11273033A (ja) | 磁気抵抗効果多層膜及び該磁気抵抗効果多層膜を備えた薄膜磁気ヘッド |