JPH09249916A5 - - Google Patents
Info
- Publication number
- JPH09249916A5 JPH09249916A5 JP8-59255A JP5925596A JPH09249916A5 JP H09249916 A5 JPH09249916 A5 JP H09249916A5 JP 5925596 A JP5925596 A JP 5925596A JP H09249916 A5 JPH09249916 A5 JP H09249916A5
- Authority
- JP
- Japan
- Prior art keywords
- annealing
- particle size
- average particle
- mgo
- weight
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP8059255A JPH09249916A (ja) | 1996-03-15 | 1996-03-15 | 方向性けい素鋼板の製造方法及び焼鈍分離剤 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP8059255A JPH09249916A (ja) | 1996-03-15 | 1996-03-15 | 方向性けい素鋼板の製造方法及び焼鈍分離剤 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH09249916A JPH09249916A (ja) | 1997-09-22 |
| JPH09249916A5 true JPH09249916A5 (enExample) | 2001-11-09 |
Family
ID=13108102
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP8059255A Pending JPH09249916A (ja) | 1996-03-15 | 1996-03-15 | 方向性けい素鋼板の製造方法及び焼鈍分離剤 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH09249916A (enExample) |
Families Citing this family (10)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR100325534B1 (ko) * | 1997-12-27 | 2002-07-18 | 이구택 | 미려한표면특성을갖는방향성전기강판의제조방법 |
| KR100967049B1 (ko) * | 2002-11-11 | 2010-06-29 | 주식회사 포스코 | 고규소 강판 제조방법 |
| KR100946070B1 (ko) * | 2002-11-27 | 2010-03-10 | 주식회사 포스코 | 고규소 전기강판 제조방법 |
| JP6112050B2 (ja) * | 2014-03-17 | 2017-04-12 | Jfeスチール株式会社 | 方向性電磁鋼板の製造方法 |
| KR101693516B1 (ko) * | 2014-12-24 | 2017-01-06 | 주식회사 포스코 | 방향성 전기강판 및 그 제조방법 |
| JP6579078B2 (ja) * | 2016-10-18 | 2019-09-25 | Jfeスチール株式会社 | 方向性電磁鋼板の製造方法 |
| US11591668B2 (en) | 2019-01-08 | 2023-02-28 | Nippon Steel Corporation | Grain-oriented electrical steel sheet and method for manufacturing same and annealing separator |
| US12104217B2 (en) | 2019-03-29 | 2024-10-01 | Jfe Steel Corporation | Grain-oriented electrical steel sheet and production method therefor |
| WO2022158541A1 (ja) * | 2021-01-21 | 2022-07-28 | Jfeスチール株式会社 | 方向性電磁鋼板の製造方法 |
| JP7878622B1 (ja) * | 2025-03-14 | 2026-06-23 | Jfeスチール株式会社 | 焼鈍分離剤用添加剤 |
-
1996
- 1996-03-15 JP JP8059255A patent/JPH09249916A/ja active Pending
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US7833360B2 (en) | Method of producing grain-oriented electrical steel sheet very excellent in magnetic properties | |
| US4979996A (en) | Process for preparation of grain-oriented electrical steel sheet comprising a nitriding treatment | |
| JP5245277B2 (ja) | 焼鈍分離剤用のマグネシアおよび方向性電磁鋼板の製造方法 | |
| JPH032324A (ja) | 磁気特性、皮膜特性ともに優れた一方向性電磁鋼板の製造方法 | |
| JPH0717953B2 (ja) | 磁気特性の優れた方向性電磁鋼板の製造法 | |
| CN113302336B (zh) | 方向性电磁钢板的制造方法 | |
| JPH09249916A (ja) | 方向性けい素鋼板の製造方法及び焼鈍分離剤 | |
| JP3707144B2 (ja) | 被膜特性に優れる方向性けい素鋼板の製造方法 | |
| JP2603130B2 (ja) | 高磁束密度方向性電磁鋼板の製造法 | |
| JP3043975B2 (ja) | 方向性けい素鋼板用焼鈍分離剤 | |
| JP3743707B2 (ja) | 超高磁束密度一方向性電磁鋼板の製造方法 | |
| CN117203355A (zh) | 取向性电磁钢板的制造方法 | |
| CN117062921A (zh) | 取向性电磁钢板的制造方法 | |
| JP4147775B2 (ja) | 磁気特性および被膜特性に優れた方向性電磁鋼板の製造方法 | |
| JPH0832928B2 (ja) | 磁気特性およびグラス皮膜特性に優れた一方向性電磁鋼板の製造方法 | |
| JPH02228425A (ja) | 高磁束密度方向性電磁鋼板の製造方法 | |
| KR20020074312A (ko) | 그라스피막이 없는 저온가열 방향성전기강판의 제조방법 | |
| JP7816664B1 (ja) | 方向性電磁鋼板の製造方法 | |
| JP7816665B1 (ja) | 方向性電磁鋼板の製造方法 | |
| EP4793387A1 (en) | Grain-oriented electrical steel sheet | |
| KR100479994B1 (ko) | 타발특성이 우수한 저온재가열 방향성전기강판의 제조방법 | |
| JP3294977B2 (ja) | 方向性けい素鋼板の製造方法 | |
| JP3885257B2 (ja) | 方向性電磁鋼板の製造方法 | |
| JP2001192737A (ja) | グラス被膜特性及び磁気特性の優れる方向性電磁鋼板の製造方法 | |
| WO2024162442A1 (ja) | 方向性電磁鋼板の製造方法 |