JPH0646057Y2 - アルカリ亜鉛蓄電池 - Google Patents
アルカリ亜鉛蓄電池Info
- Publication number
- JPH0646057Y2 JPH0646057Y2 JP15795185U JP15795185U JPH0646057Y2 JP H0646057 Y2 JPH0646057 Y2 JP H0646057Y2 JP 15795185 U JP15795185 U JP 15795185U JP 15795185 U JP15795185 U JP 15795185U JP H0646057 Y2 JPH0646057 Y2 JP H0646057Y2
- Authority
- JP
- Japan
- Prior art keywords
- battery
- negative electrode
- zinc
- indium layer
- metal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- Y02E60/12—
Landscapes
- Sealing Battery Cases Or Jackets (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15795185U JPH0646057Y2 (ja) | 1985-10-16 | 1985-10-16 | アルカリ亜鉛蓄電池 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15795185U JPH0646057Y2 (ja) | 1985-10-16 | 1985-10-16 | アルカリ亜鉛蓄電池 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6266164U JPS6266164U (enExample) | 1987-04-24 |
| JPH0646057Y2 true JPH0646057Y2 (ja) | 1994-11-24 |
Family
ID=31080977
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP15795185U Expired - Lifetime JPH0646057Y2 (ja) | 1985-10-16 | 1985-10-16 | アルカリ亜鉛蓄電池 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH0646057Y2 (enExample) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0757717A (ja) * | 1993-08-06 | 1995-03-03 | Katayama Tokushu Kogyo Kk | 金属材料板、該金属材料板からなる電池の負極端子板および該端子板の製造方法 |
-
1985
- 1985-10-16 JP JP15795185U patent/JPH0646057Y2/ja not_active Expired - Lifetime
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6266164U (enExample) | 1987-04-24 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US3746580A (en) | Gas depolarizable galvanic cell | |
| JP2002523874A (ja) | 活性部品のための内側容積を増加させたバッテリ構造 | |
| CN101002346A (zh) | 薄片碱性电池 | |
| JP2002523878A (ja) | コレクタ組立体の容積を削減したバッテリ構造 | |
| WO1999028980A1 (en) | Gasket for miniature galvanic cells | |
| US20060127758A1 (en) | Negative electrode can, alkaline cell and production method for same | |
| US2527576A (en) | Flat primary cell | |
| CA1077131A (en) | Metal oxide cells having low internal impedance | |
| JP2000501560A (ja) | 活性部材に最適な内容積を有する化学電池 | |
| US2509249A (en) | Alkaline primary cell | |
| US3925102A (en) | Divalent silver oxide cell having a unipotential discharge level | |
| JPH11121030A (ja) | 改良された電解液保持バイポーラセル及びバッテリの製造方法 | |
| CN1270707A (zh) | 电池端盖 | |
| US3496025A (en) | Deferred action battery | |
| JP4717222B2 (ja) | アルカリ電池 | |
| JP3997804B2 (ja) | アルカリ電池 | |
| JP2001523885A (ja) | 最適な小表面積の導電性集電体を有する小型ガルヴァーニ電池 | |
| CN100573985C (zh) | 碱性电池及其生产方法 | |
| JPH11102728A (ja) | 有機電解液二次電池 | |
| JPS6146942B2 (enExample) | ||
| JPH0130258B2 (enExample) | ||
| JPH0250585B2 (enExample) | ||
| JPS60207244A (ja) | 小形密閉鉛蓄電池 | |
| JPS58150265A (ja) | 円筒型アルカリ電池 | |
| JPH0731503Y2 (ja) | 有機電解質電池 |