JPH0557710B2 - - Google Patents
Info
- Publication number
- JPH0557710B2 JPH0557710B2 JP1151997A JP15199789A JPH0557710B2 JP H0557710 B2 JPH0557710 B2 JP H0557710B2 JP 1151997 A JP1151997 A JP 1151997A JP 15199789 A JP15199789 A JP 15199789A JP H0557710 B2 JPH0557710 B2 JP H0557710B2
- Authority
- JP
- Japan
- Prior art keywords
- sheet
- tensile strength
- lead
- expanded
- effect
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Cell Electrode Carriers And Collectors (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1151997A JPH0317955A (ja) | 1989-06-13 | 1989-06-13 | 鉛蓄電池 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1151997A JPH0317955A (ja) | 1989-06-13 | 1989-06-13 | 鉛蓄電池 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH0317955A JPH0317955A (ja) | 1991-01-25 |
| JPH0557710B2 true JPH0557710B2 (cg-RX-API-DMAC7.html) | 1993-08-24 |
Family
ID=15530810
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1151997A Granted JPH0317955A (ja) | 1989-06-13 | 1989-06-13 | 鉛蓄電池 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH0317955A (cg-RX-API-DMAC7.html) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5508125A (en) * | 1994-03-21 | 1996-04-16 | Globe-Union Inc. | Battery straps made of a lead-based alloy containing antimony, arsenic, tin and selenium |
-
1989
- 1989-06-13 JP JP1151997A patent/JPH0317955A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0317955A (ja) | 1991-01-25 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4939051A (en) | Grid for use in lead acid batteries and process for producing same | |
| KR100305423B1 (ko) | 납축전지극판용익스팬드격자 | |
| JPH1197032A (ja) | 二次電池用アルミニウム箔製集電体 | |
| JPS609061A (ja) | 鉛蓄電池基板用鉛合金板の製造方法 | |
| JPH0481307B2 (cg-RX-API-DMAC7.html) | ||
| JP3113895B2 (ja) | 蓄電池用鉛合金 | |
| JPH0317955A (ja) | 鉛蓄電池 | |
| CA1044923A (en) | Ternary calcium-tin-lead alloy | |
| JPH0213425B2 (cg-RX-API-DMAC7.html) | ||
| JP4423837B2 (ja) | 蓄電池用圧延鉛合金およびそれを用いた鉛蓄電池 | |
| JPH0146995B2 (cg-RX-API-DMAC7.html) | ||
| JP2001028267A (ja) | 鉛蓄電池用格子の製造方法 | |
| JP3651852B2 (ja) | マンガン乾電池 | |
| JP2008084676A (ja) | エキスパンド正極格子用圧延鉛合金シートおよび鉛蓄電池 | |
| JP2004186013A (ja) | 電極集電体及びその製造方法とシール鉛蓄電池 | |
| CA1162424A (en) | Low antimony lead-based alloys and use thereof | |
| JP3141426B2 (ja) | 鉛蓄電池用極板とその製造方法 | |
| Lam et al. | Influence of bismuth on the age-hardening and corrosion behaviour of low-antimony lead alloys in lead/acid battery systems | |
| JPH03245462A (ja) | 鉛蓄電池用格子体の製造法 | |
| JP4678117B2 (ja) | 鉛蓄電池 | |
| JP3156333B2 (ja) | 鉛蓄電池用格子体の製造法 | |
| JP2002246031A (ja) | 鉛蓄電池 | |
| KR970031040A (ko) | 알칼리 축전지용 수소 흡장 합금 전극 및 그 제조방법 | |
| GB2055896A (en) | Lead alloys | |
| JPS59177864A (ja) | 鉛蓄電池用電極材 |