Prior art keywords
sintered body
strength
deterioration
zirconia
complex impedance
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP60102546A
Other languages
English (en)
Japanese (ja)
Other versions
JPS61262650A (ja
Inventor
Makoto Kuwabara
Yoshitaka Kubota
Takaaki Tsukidate
Masahiro Ashizuka
Takanobu Murakami
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Tosoh Corp
Original Assignee
Tosoh Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tosoh Corp filed Critical Tosoh Corp
Priority to JP60102546A priority Critical patent/JPS61262650A/ja
Publication of JPS61262650A publication Critical patent/JPS61262650A/ja
Publication of JPH0535820B2 publication Critical patent/JPH0535820B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Compositions Of Oxide Ceramics (AREA)
  • Investigating Or Analyzing Materials By The Use Of Electric Means (AREA)
JP60102546A 1985-05-16 1985-05-16 ジルコニア焼結体の劣化予知方法 Granted JPS61262650A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP60102546A JPS61262650A (ja) 1985-05-16 1985-05-16 ジルコニア焼結体の劣化予知方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP60102546A JPS61262650A (ja) 1985-05-16 1985-05-16 ジルコニア焼結体の劣化予知方法

Publications (2)

Publication Number Publication Date
JPS61262650A JPS61262650A (ja) 1986-11-20
JPH0535820B2 true JPH0535820B2 (enExample) 1993-05-27

Family

ID=14330243

Family Applications (1)

Application Number Title Priority Date Filing Date
JP60102546A Granted JPS61262650A (ja) 1985-05-16 1985-05-16 ジルコニア焼結体の劣化予知方法

Country Status (1)

Country Link
JP (1) JPS61262650A (enExample)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
DE19805928C2 (de) 1998-02-13 2002-12-05 Daimler Chrysler Ag Verfahren zur Bestimmung des Füllgrads oder der Güte eines Gase speichernden Katalysators
JP2016039376A (ja) * 2014-08-08 2016-03-22 三菱マテリアル株式会社 サーミスタ素子の欠陥検出方法
JP6539197B2 (ja) * 2015-12-15 2019-07-03 日本碍子株式会社 ガスセンサの診断方法

Also Published As

Publication number Publication date
JPS61262650A (ja) 1986-11-20

Similar Documents

Publication Publication Date Title
JPS6041736B2 (ja) 酸素検出器
Eichler et al. Mechanical properties of monoclinic zirconia
White et al. Fracture behavior of cyclically loaded PZT
US4328294A (en) Solid electrolyte for use in oxygen concentration sensor
CA1229782A (en) Ceramic testing method
Hagen et al. Selective laser flash sintering of 8‐YSZ
CN101126799A (zh) 利用铁磁材料表面杂散磁场信号监测疲劳损伤的方法
US4328295A (en) Solid electrolyte for use in oxygen concentration sensor
JPS61262650A (ja) ジルコニア焼結体の劣化予知方法
TW200925600A (en) Method for determining the thermal shock robustness and material strength of brittle failure materials
JP2007303956A (ja) 経年劣化した熱遮へいコーティングの非接触非破壊検査手法
CN119574418A (zh) 一种动态腐蚀试验装置和方法
CN116735361B (zh) 一种高温处理脆性固体材料的断裂强度评价方法
Owen et al. The constant stress tensile creep behaviour of a superplastic zirconia-alumina composite
RU2169914C2 (ru) Способ определения диффузионных констант в поликристаллических телах
JPH04318448A (ja) セラミックスの評価方法
Okada et al. Mechanical degradation of silicon nitride ceramics in corrosive solutions of boiling sulphuric acid
US3958176A (en) Method for measuring suitability of aluminum for use in certain propellants
Kang et al. Nonstoichiometry (δ) of (MgxFe1− x) 3− δO4 ferrite spinel
Hemrick et al. Thermal conductivity of alumina measured with three techniques
An et al. Effect of heat treatment on structure and properties of MgO-PSZ electrolyte
Morrell Mechanical properties of engineering ceramics: Test bars versus components
Allen et al. Solid state bonding of ceramics with platinum foil
Kozielski et al. Impedance spectroscopy structural analysis: Ca-dopant segregation in (Pb0. 75Ba0. 25)(Zr0. 70Ti0. 30) O3
Wang et al. Subcritical crack growth behavior of a perovskite‐structured Ba0. 5Sr0. 5Co0. 8Fe0. 2O3− δ oxygen transport membrane