JPS61262650A - ジルコニア焼結体の劣化予知方法 - Google Patents
ジルコニア焼結体の劣化予知方法Info
- Publication number
- JPS61262650A JPS61262650A JP60102546A JP10254685A JPS61262650A JP S61262650 A JPS61262650 A JP S61262650A JP 60102546 A JP60102546 A JP 60102546A JP 10254685 A JP10254685 A JP 10254685A JP S61262650 A JPS61262650 A JP S61262650A
- Authority
- JP
- Japan
- Prior art keywords
- sintered body
- deterioration
- zirconia sintered
- zirconia
- grain
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Investigating Or Analyzing Materials By The Use Of Electric Means (AREA)
- Compositions Of Oxide Ceramics (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60102546A JPS61262650A (ja) | 1985-05-16 | 1985-05-16 | ジルコニア焼結体の劣化予知方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60102546A JPS61262650A (ja) | 1985-05-16 | 1985-05-16 | ジルコニア焼結体の劣化予知方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61262650A true JPS61262650A (ja) | 1986-11-20 |
| JPH0535820B2 JPH0535820B2 (enExample) | 1993-05-27 |
Family
ID=14330243
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP60102546A Granted JPS61262650A (ja) | 1985-05-16 | 1985-05-16 | ジルコニア焼結体の劣化予知方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS61262650A (enExample) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US6240722B1 (en) | 1998-02-13 | 2001-06-05 | Daimlerchrysler Ag | Method for determining the fullness or quality of a catalytic converter that stores gases |
| JP2016039376A (ja) * | 2014-08-08 | 2016-03-22 | 三菱マテリアル株式会社 | サーミスタ素子の欠陥検出方法 |
| JP2017110967A (ja) * | 2015-12-15 | 2017-06-22 | 日本碍子株式会社 | ガスセンサの診断方法 |
-
1985
- 1985-05-16 JP JP60102546A patent/JPS61262650A/ja active Granted
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US6240722B1 (en) | 1998-02-13 | 2001-06-05 | Daimlerchrysler Ag | Method for determining the fullness or quality of a catalytic converter that stores gases |
| JP2016039376A (ja) * | 2014-08-08 | 2016-03-22 | 三菱マテリアル株式会社 | サーミスタ素子の欠陥検出方法 |
| JP2017110967A (ja) * | 2015-12-15 | 2017-06-22 | 日本碍子株式会社 | ガスセンサの診断方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0535820B2 (enExample) | 1993-05-27 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Eichler et al. | Mechanical properties of monoclinic zirconia | |
| US4193857A (en) | Oxygen sensors | |
| White et al. | Fracture behavior of cyclically loaded PZT | |
| Khajavi et al. | Double Torsion testing of thin porous zirconia supports for energy applications: Toughness and slow crack growth assessment | |
| CN101126799A (zh) | 利用铁磁材料表面杂散磁场信号监测疲劳损伤的方法 | |
| CA1229782A (en) | Ceramic testing method | |
| Feng et al. | Grain boundary and lattice fracture toughness of UO2 measured using small-scale mechanics | |
| JPS61262650A (ja) | ジルコニア焼結体の劣化予知方法 | |
| Danielson et al. | Recent Developments with High Temperature Stabilized‐Zirconia pH Sensors | |
| JP5205608B2 (ja) | 経年劣化した熱遮へいコーティングの非接触非破壊検査手法 | |
| Owen et al. | The constant stress tensile creep behaviour of a superplastic zirconia-alumina composite | |
| CN119574418A (zh) | 一种动态腐蚀试验装置和方法 | |
| Hilpert et al. | Correlation of electrical and mechanical properties of zirconia based thermal barrier coatings | |
| Braun et al. | Effect of stress on trapped cracks in Y-TZP | |
| Nowotny et al. | Charge transfer at oxygen/zirconia interface at elevated temperatures: Part 6 Work function measurements | |
| JPH04318448A (ja) | セラミックスの評価方法 | |
| Okada et al. | Mechanical degradation of silicon nitride ceramics in corrosive solutions of boiling sulphuric acid | |
| An et al. | Effect of heat treatment on structure and properties of MgO-PSZ electrolyte | |
| Kang et al. | Nonstoichiometry (δ) of (MgxFe1− x) 3− δO4 ferrite spinel | |
| Morrell | Mechanical properties of engineering ceramics: Test bars versus components | |
| Savin et al. | Complementary methods for evaluation of yttria stabilized zirconia coatings used as thermal barrier coating | |
| Wang et al. | Subcritical crack growth behavior of a perovskite‐structured Ba0. 5Sr0. 5Co0. 8Fe0. 2O3− δ oxygen transport membrane | |
| Wang et al. | Nondestructive characterisation of alumina/silicon carbide nanocomposites using impedance spectroscopy | |
| Cao et al. | Effects of MgO on the microstructure and thermal shock properties of 8YSZ | |
| Kale et al. | High‐Temperature Sensor for In‐Line Monitoring of Mg and Li in Molten Al Employing Ion‐Conducting Ceramic Electrolytes |