JPH05106022A - 耐摩耗性硬質被膜の製造方法 - Google Patents

耐摩耗性硬質被膜の製造方法

Info

Publication number
JPH05106022A
JPH05106022A JP29500791A JP29500791A JPH05106022A JP H05106022 A JPH05106022 A JP H05106022A JP 29500791 A JP29500791 A JP 29500791A JP 29500791 A JP29500791 A JP 29500791A JP H05106022 A JPH05106022 A JP H05106022A
Authority
JP
Japan
Prior art keywords
target
alloy
film
resistant hard
metallic material
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP29500791A
Other languages
English (en)
Japanese (ja)
Other versions
JPH05106022A5 (enExample
Inventor
Yuji Chiba
祐二 千葉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Sumitomo Metal Mining Co Ltd
Original Assignee
Sumitomo Metal Mining Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sumitomo Metal Mining Co Ltd filed Critical Sumitomo Metal Mining Co Ltd
Priority to JP29500791A priority Critical patent/JPH05106022A/ja
Publication of JPH05106022A publication Critical patent/JPH05106022A/ja
Publication of JPH05106022A5 publication Critical patent/JPH05106022A5/ja
Pending legal-status Critical Current

Links

Landscapes

  • Physical Vapour Deposition (AREA)
JP29500791A 1991-10-15 1991-10-15 耐摩耗性硬質被膜の製造方法 Pending JPH05106022A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP29500791A JPH05106022A (ja) 1991-10-15 1991-10-15 耐摩耗性硬質被膜の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP29500791A JPH05106022A (ja) 1991-10-15 1991-10-15 耐摩耗性硬質被膜の製造方法

Publications (2)

Publication Number Publication Date
JPH05106022A true JPH05106022A (ja) 1993-04-27
JPH05106022A5 JPH05106022A5 (enExample) 1994-12-13

Family

ID=17815132

Family Applications (1)

Application Number Title Priority Date Filing Date
JP29500791A Pending JPH05106022A (ja) 1991-10-15 1991-10-15 耐摩耗性硬質被膜の製造方法

Country Status (1)

Country Link
JP (1) JPH05106022A (enExample)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CH688863A5 (de) * 1994-06-24 1998-04-30 Balzers Hochvakuum Verfahren zum Beschichten mindestens eines Werkstueckes und Anlage hierfuer.
US6143142A (en) * 1999-05-10 2000-11-07 Nanyang Technological University Composite coatings
CN102899613A (zh) * 2012-10-29 2013-01-30 西安浩元涂层技术有限公司 AlTiN高速切削刀具涂层的制备方法

Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS63255358A (ja) * 1987-03-23 1988-10-21 シーメンス、アクチエンゲゼルシヤフト 少くとも2種類の金属窒化物混合層とその形成方法

Patent Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS63255358A (ja) * 1987-03-23 1988-10-21 シーメンス、アクチエンゲゼルシヤフト 少くとも2種類の金属窒化物混合層とその形成方法

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CH688863A5 (de) * 1994-06-24 1998-04-30 Balzers Hochvakuum Verfahren zum Beschichten mindestens eines Werkstueckes und Anlage hierfuer.
US6602390B1 (en) * 1994-06-24 2003-08-05 Unaxis Balzers Aktiengesellschaft Coating a workpiece and operating a cathodic arc discharge
US6143142A (en) * 1999-05-10 2000-11-07 Nanyang Technological University Composite coatings
US6387443B1 (en) 1999-05-10 2002-05-14 Nanyang Technological University Composite coatings
US6899828B2 (en) 1999-05-10 2005-05-31 Nanyang Technological University Composite coatings
CN102899613A (zh) * 2012-10-29 2013-01-30 西安浩元涂层技术有限公司 AlTiN高速切削刀具涂层的制备方法
CN102899613B (zh) * 2012-10-29 2014-06-18 西安浩元涂层技术有限公司 AlTiN高速切削刀具涂层的制备方法

Similar Documents

Publication Publication Date Title
JP4482160B2 (ja) イットリウムを使用する硬質材料コーティングおよびその蒸着方法
JPH02138459A (ja) 複合硬質材料及びその製造方法
US8440327B2 (en) Method of producing a layer by arc-evaporation from ceramic cathodes
CN111757948A (zh) 具有增强热稳定性的Al-Cr基陶瓷涂层
JP3980053B2 (ja) 硬質物質層の製造方法
CA1324928C (en) Corrosion-resistant and heat-resistant aluminum-based alloy thin film and process for producing the same
JP2018510070A (ja) TiAlN−ZrNコーティングを有する固体炭化物エンドミリングカッター
JP2893498B2 (ja) 非化学量論的窒化チタンコーティング
US8293386B2 (en) Al-Ti-Ru-N-C hard material coating
US20250305110A1 (en) Metal free coating comprising tetrahedral hydrogen-free amorphous carbon
JPH04297568A (ja) 耐摩耗性のすぐれた表面被覆部材及び皮膜形成方法
JP2024047170A (ja) 被覆切削工具
JP3638332B2 (ja) 被覆硬質合金
JP3546967B2 (ja) 被覆硬質合金
GB2385062A (en) Method of Applying Hard Coatings
JP3712241B2 (ja) 被覆切削工具・被覆耐摩耗工具
JPH08199340A (ja) 被覆硬質合金
JP7796750B2 (ja) セラミックターゲットからPVDによって製造された硬質立方晶AlリッチAlTiNコーティング層
JPS63166957A (ja) 表面被覆鋼製品
JPH06316756A (ja) 耐食・耐摩耗性被膜
JP2633622B2 (ja) 工作工具用耐摩耗性複合部材
JP2927098B2 (ja) 物理蒸着硬質層被覆ドリルおよびその製造法
JP2012507635A (ja) 摩耗保護層およびそれを製造するための方法
JP3351054B2 (ja) 耐酸化性および耐摩耗性に優れた硬質皮膜
JPH0250948A (ja) 複合超硬材料