JPH0432037B2 - - Google Patents
Info
- Publication number
- JPH0432037B2 JPH0432037B2 JP8694287A JP8694287A JPH0432037B2 JP H0432037 B2 JPH0432037 B2 JP H0432037B2 JP 8694287 A JP8694287 A JP 8694287A JP 8694287 A JP8694287 A JP 8694287A JP H0432037 B2 JPH0432037 B2 JP H0432037B2
- Authority
- JP
- Japan
- Prior art keywords
- concrete
- epoxy resin
- water
- wet
- fibrous
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C04—CEMENTS; CONCRETE; ARTIFICIAL STONE; CERAMICS; REFRACTORIES
- C04B—LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE; CERAMICS; REFRACTORIES; TREATMENT OF NATURAL STONE
- C04B41/00—After-treatment of mortars, concrete, artificial stone or ceramics; Treatment of natural stone
- C04B41/45—Coating or impregnating, e.g. injection in masonry, partial coating of green or fired ceramics, organic coating compositions for adhering together two concrete elements
- C04B41/52—Multiple coating or impregnating multiple coating or impregnating with the same composition or with compositions only differing in the concentration of the constituents, is classified as single coating or impregnation
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Ceramic Engineering (AREA)
- Materials Engineering (AREA)
- Structural Engineering (AREA)
- Organic Chemistry (AREA)
- Aftertreatments Of Artificial And Natural Stones (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP8694287A JPH01176288A (ja) | 1987-04-10 | 1987-04-10 | 自己乳化型エポキシ樹脂を用いた水和反応熱利用による濡れ面コンクリート表面処理方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP8694287A JPH01176288A (ja) | 1987-04-10 | 1987-04-10 | 自己乳化型エポキシ樹脂を用いた水和反応熱利用による濡れ面コンクリート表面処理方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPH01176288A JPH01176288A (ja) | 1989-07-12 |
JPH0432037B2 true JPH0432037B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | 1992-05-28 |
Family
ID=13900924
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP8694287A Granted JPH01176288A (ja) | 1987-04-10 | 1987-04-10 | 自己乳化型エポキシ樹脂を用いた水和反応熱利用による濡れ面コンクリート表面処理方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPH01176288A (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN108002863B (zh) * | 2017-12-08 | 2020-03-10 | 中建西部建设湖南有限公司 | 一种对混凝土表面超疏水处理的方法 |
CN117447159A (zh) * | 2023-10-27 | 2024-01-26 | 江苏科技大学 | 一种内外协同自养护水泥混凝土及其制备方法 |
-
1987
- 1987-04-10 JP JP8694287A patent/JPH01176288A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPH01176288A (ja) | 1989-07-12 |