JPH0334401B2 - - Google Patents
Info
- Publication number
- JPH0334401B2 JPH0334401B2 JP60296611A JP29661185A JPH0334401B2 JP H0334401 B2 JPH0334401 B2 JP H0334401B2 JP 60296611 A JP60296611 A JP 60296611A JP 29661185 A JP29661185 A JP 29661185A JP H0334401 B2 JPH0334401 B2 JP H0334401B2
- Authority
- JP
- Japan
- Prior art keywords
- surface roughness
- steel sheet
- cold
- press formability
- rolled
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
- 229910000831 Steel Inorganic materials 0.000 claims description 31
- 239000010959 steel Substances 0.000 claims description 31
- 230000003746 surface roughness Effects 0.000 claims description 27
- 239000010960 cold rolled steel Substances 0.000 claims description 15
- 238000005096 rolling process Methods 0.000 description 9
- 238000000034 method Methods 0.000 description 7
- 239000010687 lubricating oil Substances 0.000 description 4
- 230000000694 effects Effects 0.000 description 3
- 238000004519 manufacturing process Methods 0.000 description 3
- 239000000463 material Substances 0.000 description 3
- 238000011160 research Methods 0.000 description 3
- 238000005422 blasting Methods 0.000 description 2
- 239000003921 oil Substances 0.000 description 2
- 238000012545 processing Methods 0.000 description 2
- 238000012360 testing method Methods 0.000 description 2
- 229910000655 Killed steel Inorganic materials 0.000 description 1
- RQMIWLMVTCKXAQ-UHFFFAOYSA-N [AlH3].[C] Chemical compound [AlH3].[C] RQMIWLMVTCKXAQ-UHFFFAOYSA-N 0.000 description 1
- 230000000052 comparative effect Effects 0.000 description 1
- 239000002131 composite material Substances 0.000 description 1
- 238000009749 continuous casting Methods 0.000 description 1
- 230000001276 controlling effect Effects 0.000 description 1
- 238000011156 evaluation Methods 0.000 description 1
- JEIPFZHSYJVQDO-UHFFFAOYSA-N iron(III) oxide Inorganic materials O=[Fe]O[Fe]=O JEIPFZHSYJVQDO-UHFFFAOYSA-N 0.000 description 1
- 239000000314 lubricant Substances 0.000 description 1
- 238000005461 lubrication Methods 0.000 description 1
- 229910052751 metal Inorganic materials 0.000 description 1
- 239000002184 metal Substances 0.000 description 1
- 239000000203 mixture Substances 0.000 description 1
- 238000010422 painting Methods 0.000 description 1
- 238000005554 pickling Methods 0.000 description 1
- 238000003825 pressing Methods 0.000 description 1
- 230000003449 preventive effect Effects 0.000 description 1
- 238000003672 processing method Methods 0.000 description 1
- 230000001105 regulatory effect Effects 0.000 description 1
- 238000002791 soaking Methods 0.000 description 1
- 238000005482 strain hardening Methods 0.000 description 1
- 239000000126 substance Substances 0.000 description 1
Landscapes
- Metal Rolling (AREA)
- Shaping Metal By Deep-Drawing, Or The Like (AREA)
Priority Applications (10)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP60296611A JPS62151205A (ja) | 1985-12-24 | 1985-12-24 | プレス成形性に優れる冷延鋼板 |
US06/944,679 US4775599A (en) | 1985-12-24 | 1986-12-19 | Cold rolled steel sheets having an improved press formability |
ZA869625A ZA869625B (en) | 1985-12-24 | 1986-12-22 | Cold rolled steel sheets having a press formability |
CN86108640A CN1011121B (zh) | 1985-12-24 | 1986-12-23 | 具有改进的压力成型性能的冷轧薄钢板 |
DE8686310099T DE3686816T2 (de) | 1985-12-24 | 1986-12-23 | Kaltgewalzte stahlbleche mit guter pressverformbarkeit. |
CA000526166A CA1275154C (en) | 1985-12-24 | 1986-12-23 | Cold rolled steel sheets having an improved press formability |
AU66907/86A AU579271B2 (en) | 1985-12-24 | 1986-12-23 | Cold rolled steel sheets having an improved press formability |
EP86310099A EP0231653B1 (en) | 1985-12-24 | 1986-12-23 | Cold rolled steel sheets having an improved press formability |
BR8606445A BR8606445A (pt) | 1985-12-24 | 1986-12-24 | Folhas de aco laminadas a frio tendo uma conformabilidade sob pressao aperfeicoada |
KR1019860011229A KR900006655B1 (ko) | 1985-12-24 | 1986-12-24 | 프레스 성형성이 우수한 냉간압연 강판 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP60296611A JPS62151205A (ja) | 1985-12-24 | 1985-12-24 | プレス成形性に優れる冷延鋼板 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS62151205A JPS62151205A (ja) | 1987-07-06 |
JPH0334401B2 true JPH0334401B2 (enrdf_load_stackoverflow) | 1991-05-22 |
Family
ID=17835794
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP60296611A Granted JPS62151205A (ja) | 1985-12-24 | 1985-12-24 | プレス成形性に優れる冷延鋼板 |
Country Status (2)
Country | Link |
---|---|
JP (1) | JPS62151205A (enrdf_load_stackoverflow) |
ZA (1) | ZA869625B (enrdf_load_stackoverflow) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
KR101493859B1 (ko) * | 2013-09-10 | 2015-02-16 | 주식회사 포스코 | 강판의 두께 제어장치 및 제어방법 |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH01148402A (ja) * | 1987-12-05 | 1989-06-09 | Kawasaki Steel Corp | 加工歪の測定容易な絞り用鋼板 |
-
1985
- 1985-12-24 JP JP60296611A patent/JPS62151205A/ja active Granted
-
1986
- 1986-12-22 ZA ZA869625A patent/ZA869625B/xx unknown
Non-Patent Citations (1)
Title |
---|
TECNIC INFO=1984 * |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
KR101493859B1 (ko) * | 2013-09-10 | 2015-02-16 | 주식회사 포스코 | 강판의 두께 제어장치 및 제어방법 |
Also Published As
Publication number | Publication date |
---|---|
ZA869625B (en) | 1987-08-26 |
JPS62151205A (ja) | 1987-07-06 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
KR900006655B1 (ko) | 프레스 성형성이 우수한 냉간압연 강판 | |
EP3204530B1 (de) | Kaltgewalztes und rekristallisierend geglühtes stahlflachprodukt und verfahren zu dessen herstellung | |
CN101622080B (zh) | 高张力冷轧钢板及其制造方法 | |
WO2023281939A1 (ja) | 高強度鋼板、高強度めっき鋼板及びそれらの製造方法並びに部材 | |
JPH0334401B2 (enrdf_load_stackoverflow) | ||
JPH0334402B2 (enrdf_load_stackoverflow) | ||
JPH0334403B2 (enrdf_load_stackoverflow) | ||
JPH0457744B2 (enrdf_load_stackoverflow) | ||
JPH0334404B2 (enrdf_load_stackoverflow) | ||
JP3068938B2 (ja) | 成形性に優れた合金化溶融亜鉛めっき鋼板の製造方法 | |
JP3069199B2 (ja) | プレス成形性に優れた高張力薄鋼板 | |
JP2500215B2 (ja) | 耐プレスしわ性の良好なほうろう用薄鋼板 | |
CN111411298B (zh) | 一种低强度耐铁皮脱落的热成型钢卷及其制备方法 | |
JPH05337560A (ja) | 絞り成形性に優れたプレス加工用薄板 | |
JPS61204320A (ja) | 耐リジング性に優れる加工用アズロ−ルド薄鋼板の製造方法 | |
JPH0691305A (ja) | 深絞り性と耐型かじり性と耐食性に優れた亜鉛系めっき鋼板 | |
JPH0668155B2 (ja) | プレス成形性とほうろう密着性に優れたほうろう鋼板の製造方法 | |
JPH0732056A (ja) | プレス成形性に優れた高張力薄鋼板 | |
JPS63307221A (ja) | プレス成形性および塗装後の鮮映性に優れる熱延鋼板 | |
JPH0250806B2 (enrdf_load_stackoverflow) | ||
JPS6210217A (ja) | 耐リジング性に優れるフエライト系ステンレス鋼板の製造方法 | |
JP2001288549A (ja) | プレス成形性に優れた冷延鋼板、めっき鋼板の製造方法 | |
JPH0784674B2 (ja) | プレス成形性、耐型かじり性もしくは塗装後鮮映性に優れるめつき鋼板 | |
CN118786234A (zh) | 钢板和部件以及它们的制造方法 | |
JPH0687002A (ja) | 深絞り性と耐かじり性に優れた亜鉛系めっき鋼板 |