JPH0330849Y2 - - Google Patents
Info
- Publication number
- JPH0330849Y2 JPH0330849Y2 JP15158886U JP15158886U JPH0330849Y2 JP H0330849 Y2 JPH0330849 Y2 JP H0330849Y2 JP 15158886 U JP15158886 U JP 15158886U JP 15158886 U JP15158886 U JP 15158886U JP H0330849 Y2 JPH0330849 Y2 JP H0330849Y2
- Authority
- JP
- Japan
- Prior art keywords
- concrete
- metal
- probe
- corrosion
- reinforcing bars
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Testing Resistance To Weather, Investigating Materials By Mechanical Methods (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15158886U JPH0330849Y2 (enrdf_load_stackoverflow) | 1986-10-03 | 1986-10-03 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15158886U JPH0330849Y2 (enrdf_load_stackoverflow) | 1986-10-03 | 1986-10-03 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6358746U JPS6358746U (enrdf_load_stackoverflow) | 1988-04-19 |
JPH0330849Y2 true JPH0330849Y2 (enrdf_load_stackoverflow) | 1991-06-28 |
Family
ID=31068801
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP15158886U Expired JPH0330849Y2 (enrdf_load_stackoverflow) | 1986-10-03 | 1986-10-03 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPH0330849Y2 (enrdf_load_stackoverflow) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2006337169A (ja) * | 2005-06-01 | 2006-12-14 | Taiheiyo Cement Corp | 腐食センサ、シース管、シース管継ぎ手部材および腐食センサユニット |
JP2016186483A (ja) * | 2015-03-27 | 2016-10-27 | 太平洋セメント株式会社 | 腐食状態予測方法 |
-
1986
- 1986-10-03 JP JP15158886U patent/JPH0330849Y2/ja not_active Expired
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2006337169A (ja) * | 2005-06-01 | 2006-12-14 | Taiheiyo Cement Corp | 腐食センサ、シース管、シース管継ぎ手部材および腐食センサユニット |
JP2016186483A (ja) * | 2015-03-27 | 2016-10-27 | 太平洋セメント株式会社 | 腐食状態予測方法 |
Also Published As
Publication number | Publication date |
---|---|
JPS6358746U (enrdf_load_stackoverflow) | 1988-04-19 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP3205291B2 (ja) | コンクリート中鋼材の腐食状況の予測方法 | |
Hansson | Comments on electrochemical measurements of the rate of corrosion of steel in concrete | |
Castro-Borges et al. | Performance of a 60-year-old concrete pier with stainless steel reinforcement | |
JPS6367558A (ja) | 鉄筋コンクリ−ト構造体の要修理区域の位置決め方法 | |
González et al. | Some questions on the corrosion of steel in concrete. Part II: Corrosion mechanism and monitoring, service life prediction and protection methods | |
JPH0330849Y2 (enrdf_load_stackoverflow) | ||
KR20050101676A (ko) | 철근 콘크리트 구조물의 부식감지용 센서 및 시스템 | |
Mietz et al. | Monitoring of concrete structures with respect to rebar corrosion | |
Nürnberger et al. | Stainless steel in concrete structures and in the fastening technique | |
JP2783957B2 (ja) | コンクリート内の鋼材を不動態化する方法 | |
JP2000044364A (ja) | コンクリート構造物の要補修部分を検出する方法およびその補修方法 | |
JPH0422464B2 (enrdf_load_stackoverflow) | ||
JP2511234B2 (ja) | 埋設鉄筋の腐食度検出用プロ―ブ | |
JP3397722B2 (ja) | コンクリート構造物の劣化検出方法 | |
JP2015187559A (ja) | 腐食検知方法および腐食検知システム | |
JPH10221292A (ja) | コンクリート中の鋼材の腐食検出方法 | |
JP3847300B2 (ja) | コンクリート中の鋼材の腐蝕予測装置及び腐蝕予測方法 | |
JP6851605B2 (ja) | pH検出電極ワイヤのキャリブレーション方法 | |
BETON | Corrosion of stainless steel reinforcement in cracked concrete | |
EP1745276B1 (en) | Measuring device, equipment and method for monitoring the onset of corrosion affecting steel reinforcements embedded in reinforced concrete | |
JP3516587B2 (ja) | コンクリート中の鋼材の連続性検出方法 | |
JP6618212B2 (ja) | コンクリートの脱塩処理システム、再アルカリ化処理システム、並びにこれらに用いる塩分センサ及びpHセンサ | |
JPH11230927A (ja) | 塗装鉄筋の欠陥を検出できるコンクリート構造物とその検出方法 | |
Schwarz et al. | Galvanic chloride extraction by an embedded zinc anode: Ion distribution mapped by laser induced breakdown spectroscopy (LIBS) | |
Andrade et al. | Detection of corrosion risk besides patch repairs |