JPH0422464B2 - - Google Patents
Info
- Publication number
- JPH0422464B2 JPH0422464B2 JP23450986A JP23450986A JPH0422464B2 JP H0422464 B2 JPH0422464 B2 JP H0422464B2 JP 23450986 A JP23450986 A JP 23450986A JP 23450986 A JP23450986 A JP 23450986A JP H0422464 B2 JPH0422464 B2 JP H0422464B2
- Authority
- JP
- Japan
- Prior art keywords
- concrete
- corrosion
- ammeter
- reinforcing bars
- reinforcing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
- 230000003014 reinforcing effect Effects 0.000 claims description 27
- 239000004567 concrete Substances 0.000 claims description 23
- 238000005260 corrosion Methods 0.000 claims description 22
- 230000007797 corrosion Effects 0.000 claims description 22
- 238000000034 method Methods 0.000 claims description 11
- 239000011150 reinforced concrete Substances 0.000 claims description 6
- 239000002184 metal Substances 0.000 claims description 5
- 229910052751 metal Inorganic materials 0.000 claims description 5
- 238000005259 measurement Methods 0.000 claims description 4
- RYGMFSIKBFXOCR-UHFFFAOYSA-N Copper Chemical compound [Cu] RYGMFSIKBFXOCR-UHFFFAOYSA-N 0.000 description 6
- 229910001294 Reinforcing steel Inorganic materials 0.000 description 6
- 229910052802 copper Inorganic materials 0.000 description 6
- 239000010949 copper Substances 0.000 description 6
- WABPQHHGFIMREM-UHFFFAOYSA-N lead(0) Chemical compound [Pb] WABPQHHGFIMREM-UHFFFAOYSA-N 0.000 description 5
- 229910000831 Steel Inorganic materials 0.000 description 3
- BASFCYQUMIYNBI-UHFFFAOYSA-N platinum Substances [Pt] BASFCYQUMIYNBI-UHFFFAOYSA-N 0.000 description 3
- 239000010959 steel Substances 0.000 description 3
- CURLTUGMZLYLDI-UHFFFAOYSA-N Carbon dioxide Chemical compound O=C=O CURLTUGMZLYLDI-UHFFFAOYSA-N 0.000 description 2
- XEEYBQQBJWHFJM-UHFFFAOYSA-N Iron Chemical compound [Fe] XEEYBQQBJWHFJM-UHFFFAOYSA-N 0.000 description 2
- 239000007864 aqueous solution Substances 0.000 description 2
- 150000003841 chloride salts Chemical class 0.000 description 2
- 238000011835 investigation Methods 0.000 description 2
- JEIPFZHSYJVQDO-UHFFFAOYSA-N iron(III) oxide Inorganic materials O=[Fe]O[Fe]=O JEIPFZHSYJVQDO-UHFFFAOYSA-N 0.000 description 2
- 239000010936 titanium Substances 0.000 description 2
- FAPWRFPIFSIZLT-UHFFFAOYSA-M Sodium chloride Chemical compound [Na+].[Cl-] FAPWRFPIFSIZLT-UHFFFAOYSA-M 0.000 description 1
- RTAQQCXQSZGOHL-UHFFFAOYSA-N Titanium Chemical compound [Ti] RTAQQCXQSZGOHL-UHFFFAOYSA-N 0.000 description 1
- 230000002378 acidificating effect Effects 0.000 description 1
- 229910002092 carbon dioxide Inorganic materials 0.000 description 1
- 239000001569 carbon dioxide Substances 0.000 description 1
- 238000003745 diagnosis Methods 0.000 description 1
- 238000010586 diagram Methods 0.000 description 1
- 230000000694 effects Effects 0.000 description 1
- 238000005516 engineering process Methods 0.000 description 1
- 238000000605 extraction Methods 0.000 description 1
- 229910052742 iron Inorganic materials 0.000 description 1
- 238000006386 neutralization reaction Methods 0.000 description 1
- 238000007254 oxidation reaction Methods 0.000 description 1
- 230000033116 oxidation-reduction process Effects 0.000 description 1
- 239000002245 particle Substances 0.000 description 1
- 229910052697 platinum Inorganic materials 0.000 description 1
- 230000002250 progressing effect Effects 0.000 description 1
- 238000006722 reduction reaction Methods 0.000 description 1
- 235000002639 sodium chloride Nutrition 0.000 description 1
- 239000011780 sodium chloride Substances 0.000 description 1
- 239000000243 solution Substances 0.000 description 1
- 239000000126 substance Substances 0.000 description 1
- 239000013589 supplement Substances 0.000 description 1
- 239000008399 tap water Substances 0.000 description 1
- 235000020679 tap water Nutrition 0.000 description 1
- 229910052719 titanium Inorganic materials 0.000 description 1
- 230000000007 visual effect Effects 0.000 description 1
- 238000011179 visual inspection Methods 0.000 description 1
- XLYOFNOQVPJJNP-UHFFFAOYSA-N water Substances O XLYOFNOQVPJJNP-UHFFFAOYSA-N 0.000 description 1
Landscapes
- Testing Resistance To Weather, Investigating Materials By Mechanical Methods (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP23450986A JPS6390753A (ja) | 1986-10-03 | 1986-10-03 | 鉄筋コンクリ−トの鉄筋腐食状態調査方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP23450986A JPS6390753A (ja) | 1986-10-03 | 1986-10-03 | 鉄筋コンクリ−トの鉄筋腐食状態調査方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6390753A JPS6390753A (ja) | 1988-04-21 |
JPH0422464B2 true JPH0422464B2 (enrdf_load_stackoverflow) | 1992-04-17 |
Family
ID=16972140
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP23450986A Granted JPS6390753A (ja) | 1986-10-03 | 1986-10-03 | 鉄筋コンクリ−トの鉄筋腐食状態調査方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6390753A (enrdf_load_stackoverflow) |
Families Citing this family (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP3973768B2 (ja) * | 1998-07-17 | 2007-09-12 | 株式会社太平洋コンサルタント | コンクリート構造物中の鉄筋の腐食状態の評価方法 |
KR101127500B1 (ko) * | 2009-07-28 | 2012-03-23 | 서울도시가스 주식회사 | 디씨브이지 탐측장비의 물공급장치 |
US8466695B2 (en) * | 2010-08-19 | 2013-06-18 | Southwest Research Institute | Corrosion monitoring of concrete reinforcement bars (or other buried corrodable structures) using distributed node electrodes |
CN109632559A (zh) * | 2018-12-06 | 2019-04-16 | 天能电池集团有限公司 | 一种蓄电池板栅耐腐蚀性能的测试方法 |
CN110672506B (zh) * | 2019-10-12 | 2022-07-29 | 安徽省(水利部淮河水利委员会)水利科学研究院(安徽省水利工程质量检测中心站) | 一种混凝土内钢筋加速腐蚀的电位自动监测系统 |
-
1986
- 1986-10-03 JP JP23450986A patent/JPS6390753A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS6390753A (ja) | 1988-04-21 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Hansson | Comments on electrochemical measurements of the rate of corrosion of steel in concrete | |
JP3205291B2 (ja) | コンクリート中鋼材の腐食状況の予測方法 | |
Elsener et al. | Half-cell potential measurements—Potential mapping on reinforced concrete structures | |
Gonzalez et al. | Comparison of rates of general corrosion and maximum pitting penetration on concrete embedded steel reinforcement | |
Castro-Borges et al. | Performance of a 60-year-old concrete pier with stainless steel reinforcement | |
Miranda et al. | Several questions about electrochemical rehabilitation methods for reinforced concrete structures | |
González et al. | On the effectiveness of realkalisation as a rehabilitation method for corroded reinforced concrete structures | |
JPH0743336B2 (ja) | 鉄筋コンクリ−ト構造体の要修理区域の位置決め方法 | |
González et al. | Some questions on the corrosion of steel in concrete. Part II: Corrosion mechanism and monitoring, service life prediction and protection methods | |
Kozlica et al. | In situ, real-time imaging of redox-active species on Al/Cu galvanic couple and corrosion inhibition with 2-mercaptobenzimidazole and octylphosphonic acid | |
JPH0422464B2 (enrdf_load_stackoverflow) | ||
JP2000044364A (ja) | コンクリート構造物の要補修部分を検出する方法およびその補修方法 | |
JPH09171012A (ja) | コンクリートの中性化測定方法及び装置 | |
CN212275540U (zh) | 一种测定水泥基材料中钢筋脱钝临界氯离子浓度的装置 | |
JP3397722B2 (ja) | コンクリート構造物の劣化検出方法 | |
JPH10221292A (ja) | コンクリート中の鋼材の腐食検出方法 | |
Gu et al. | Techniques for corrosion investigation in reinforced concrete | |
JPH0330849Y2 (enrdf_load_stackoverflow) | ||
JPS59217147A (ja) | コンクリ−ト中の鋼材の腐食探査方法およびその装置 | |
JP3847300B2 (ja) | コンクリート中の鋼材の腐蝕予測装置及び腐蝕予測方法 | |
JP6851605B2 (ja) | pH検出電極ワイヤのキャリブレーション方法 | |
JP2535177B2 (ja) | 鉄筋コンクリ−ト構造物の劣化判定方法 | |
JP2019066300A (ja) | 電気防食効果検出方法 | |
KR100957691B1 (ko) | 콘크리트 구조물 부식진단방법 및 그 장치 | |
JP2002365259A (ja) | コンクリートの中性化判定方法及び判定装置 |