JPH0329085B2 - - Google Patents

Info

Publication number
JPH0329085B2
JPH0329085B2 JP14474983A JP14474983A JPH0329085B2 JP H0329085 B2 JPH0329085 B2 JP H0329085B2 JP 14474983 A JP14474983 A JP 14474983A JP 14474983 A JP14474983 A JP 14474983A JP H0329085 B2 JPH0329085 B2 JP H0329085B2
Authority
JP
Japan
Prior art keywords
polymer
casing
weight
drying
dehydration
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP14474983A
Other languages
English (en)
Japanese (ja)
Other versions
JPS6036502A (ja
Inventor
Kenichiro Nishiwaki
Tomio Sakai
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Denka Co Ltd
Original Assignee
Denki Kagaku Kogyo KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Denki Kagaku Kogyo KK filed Critical Denki Kagaku Kogyo KK
Priority to JP14474983A priority Critical patent/JPS6036502A/ja
Publication of JPS6036502A publication Critical patent/JPS6036502A/ja
Publication of JPH0329085B2 publication Critical patent/JPH0329085B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Processes Of Treating Macromolecular Substances (AREA)
  • Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
JP14474983A 1983-08-08 1983-08-08 高分子ラテツクスから乾燥ポリマ−の連続製造方法 Granted JPS6036502A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP14474983A JPS6036502A (ja) 1983-08-08 1983-08-08 高分子ラテツクスから乾燥ポリマ−の連続製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP14474983A JPS6036502A (ja) 1983-08-08 1983-08-08 高分子ラテツクスから乾燥ポリマ−の連続製造方法

Publications (2)

Publication Number Publication Date
JPS6036502A JPS6036502A (ja) 1985-02-25
JPH0329085B2 true JPH0329085B2 (enExample) 1991-04-23

Family

ID=15369473

Family Applications (1)

Application Number Title Priority Date Filing Date
JP14474983A Granted JPS6036502A (ja) 1983-08-08 1983-08-08 高分子ラテツクスから乾燥ポリマ−の連続製造方法

Country Status (1)

Country Link
JP (1) JPS6036502A (enExample)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2002187901A (ja) * 2000-12-21 2002-07-05 Denki Kagaku Kogyo Kk カルボキシル基含有ゴムの製造方法

Families Citing this family (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
DE59600302D1 (de) * 1995-03-27 1998-08-06 Basf Ag Verfahren zur Herstellung von Thermoplasten
EP0735077B1 (de) * 1995-03-27 1998-07-29 BASF Aktiengesellschaft Verfahren zur Herstellung von Thermoplasten
KR100851085B1 (ko) 2001-09-04 2008-08-08 더블유.알.그레이스 앤드 캄파니-콘 초흡수성-소수성 중합체 2 상 조성물
CN114502640B (zh) * 2019-10-16 2023-12-08 电化株式会社 丙烯酸酯橡胶、橡胶组合物及其交联物、橡胶软管及密封部件

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2002187901A (ja) * 2000-12-21 2002-07-05 Denki Kagaku Kogyo Kk カルボキシル基含有ゴムの製造方法

Also Published As

Publication number Publication date
JPS6036502A (ja) 1985-02-25

Similar Documents

Publication Publication Date Title
JP4653380B2 (ja) プラスチック/水混合物の脱水によって、排水中のポリマー含量を減少させる方法
JP2004131654A (ja) 重合体の回収方法及び回収装置
JP2002284811A (ja) エチレン−ビニルアルコール共重合体樹脂の製造方法
JP4505038B1 (ja) ウェットマスターバッチの製造方法
JPH0329085B2 (enExample)
JPS6054974B2 (ja) ゴムカ−ボンマスタ−バツチの製造方法
JP2012131943A (ja) ウェットマスターバッチの製造方法及びタイヤ用ゴム組成物及び空気入りタイヤ
JPS61264005A (ja) 重合体ラテツクスから重合体を回収する方法
JP3721442B2 (ja) ゴム状重合体の製造方法と製造装置
JPS6010884B2 (ja) ゴム系ラテツクスからの乾燥ゴムの連続製造方法
US4028302A (en) Process for preparing concentrated acrylonitrile polymer solutions
CN102993690B (zh) 一种abs改性的尼龙pa66粒子料及其制备方法及在汽车上的应用
JPS6153364B2 (enExample)
JPH03203610A (ja) 有機繊維充填剤をsbr中に混合するための予備凝固方法
JPS5927776B2 (ja) 成形用樹脂組成物
KR101279244B1 (ko) (고무 강화)스티렌계 수지 조성물의 회수 방법 및 장치
US2854426A (en) Process of milling synthetic rubber latex coagulum containing water
CN112454721B (zh) 一种圆柱状八溴醚颗粒的制备方法
CN109263006B (zh) 一种多阶混合机连续高效制备低成本高性能橡塑共混微孔渗灌管的方法
JP2001200062A (ja) 乾燥樹脂粉末の製造方法
JPS5618604A (en) Continuous recovery of polymer from polymer latex
CN114619689A (zh) 连续制备再生天然高分子膜的方法
JP2002284888A (ja) エチレン−ビニルアルコール共重合体樹脂組成物の製造方法
JP2639123B2 (ja) 熱可塑性樹脂の脱水方法
KR102479891B1 (ko) 2축 스크류형 압출건조기를 이용한 아크릴 고무 펠렛의 제조방법