JPH032361B2 - - Google Patents
Info
- Publication number
- JPH032361B2 JPH032361B2 JP5770583A JP5770583A JPH032361B2 JP H032361 B2 JPH032361 B2 JP H032361B2 JP 5770583 A JP5770583 A JP 5770583A JP 5770583 A JP5770583 A JP 5770583A JP H032361 B2 JPH032361 B2 JP H032361B2
- Authority
- JP
- Japan
- Prior art keywords
- nozzle
- coagulating
- substrate
- latex
- coagulation
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP5770583A JPS59182801A (ja) | 1983-03-31 | 1983-03-31 | 重合体ラテツクスの凝固方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP5770583A JPS59182801A (ja) | 1983-03-31 | 1983-03-31 | 重合体ラテツクスの凝固方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS59182801A JPS59182801A (ja) | 1984-10-17 |
| JPH032361B2 true JPH032361B2 (cg-RX-API-DMAC10.html) | 1991-01-14 |
Family
ID=13063351
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP5770583A Granted JPS59182801A (ja) | 1983-03-31 | 1983-03-31 | 重合体ラテツクスの凝固方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS59182801A (cg-RX-API-DMAC10.html) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2021010861A (ja) * | 2019-07-04 | 2021-02-04 | 国立研究開発法人日本原子力研究開発機構 | 液相噴出用ノズル |
-
1983
- 1983-03-31 JP JP5770583A patent/JPS59182801A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS59182801A (ja) | 1984-10-17 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN103502323B (zh) | 生产各种尺寸的均匀聚合物珠粒的方法 | |
| US4429114A (en) | Method for treating emulsified latex | |
| JPWO2007114468A1 (ja) | 噴霧乾燥器、噴霧乾燥方法及び重合体粉体 | |
| EP1408053A1 (en) | Controlled suspension polymerization process without mechanical agitation | |
| US4744744A (en) | Extrusion nozzle for coagulation of polymer latices | |
| JPH032361B2 (cg-RX-API-DMAC10.html) | ||
| JPH032362B2 (cg-RX-API-DMAC10.html) | ||
| JPH0365376B2 (cg-RX-API-DMAC10.html) | ||
| JPH032363B2 (cg-RX-API-DMAC10.html) | ||
| US4277426A (en) | Method for production of coagulated synthetic polymer latex | |
| JPH0365375B2 (cg-RX-API-DMAC10.html) | ||
| CN112142881A (zh) | 一种abs接枝胶乳的凝聚方法及其所用装置 | |
| JP3411070B2 (ja) | 重合体粉体の製造方法 | |
| CA1042127A (en) | Continuous method of agglomerating aqueous latices and apparatus therefor | |
| JPS60127311A (ja) | 熱可塑性樹脂粉末の製造方法 | |
| JPH043414B2 (cg-RX-API-DMAC10.html) | ||
| CN114642942B (zh) | 一种四氟乙烯聚合反应釜回收气的纯化方法及装置 | |
| JPS6042428A (ja) | 熱可塑性樹脂の製造装置 | |
| JPH0224295B2 (cg-RX-API-DMAC10.html) | ||
| JP2560032B2 (ja) | 粒状体の製造方法 | |
| JP6255648B2 (ja) | 無機粒子の連続反応装置及び無機粒子の連続反応晶析方法 | |
| JPS60124626A (ja) | 重合体粉末の製造方法 | |
| CN113145036A (zh) | 一种粒径均一聚合物微球的制备装置及方法 | |
| JPH07157502A (ja) | ゴムラテックスの連続凝集肥大化方法 | |
| JPS62227706A (ja) | 重合体ラテツクスの凝固法及び装置 |