JPH0210785B2 - - Google Patents
Info
- Publication number
- JPH0210785B2 JPH0210785B2 JP15414180A JP15414180A JPH0210785B2 JP H0210785 B2 JPH0210785 B2 JP H0210785B2 JP 15414180 A JP15414180 A JP 15414180A JP 15414180 A JP15414180 A JP 15414180A JP H0210785 B2 JPH0210785 B2 JP H0210785B2
- Authority
- JP
- Japan
- Prior art keywords
- group
- mol
- modified pva
- lower alkyl
- pva
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Joining Of Glass To Other Materials (AREA)
- Adhesives Or Adhesive Processes (AREA)
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15414180A JPS5777051A (en) | 1980-10-31 | 1980-10-31 | Resin for interlayer of safety laminated glass |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15414180A JPS5777051A (en) | 1980-10-31 | 1980-10-31 | Resin for interlayer of safety laminated glass |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5777051A JPS5777051A (en) | 1982-05-14 |
| JPH0210785B2 true JPH0210785B2 (cs) | 1990-03-09 |
Family
ID=15577771
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP15414180A Granted JPS5777051A (en) | 1980-10-31 | 1980-10-31 | Resin for interlayer of safety laminated glass |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5777051A (cs) |
Families Citing this family (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE102005022853A1 (de) * | 2005-05-18 | 2006-11-23 | Wacker Polymer Systems Gmbh & Co. Kg | Verfahren zur Herstellung von kationischen Polyvinylacetalen |
| JP5638902B2 (ja) * | 2010-09-29 | 2014-12-10 | 積水化学工業株式会社 | スラリー組成物の製造方法 |
| EP2732968A1 (de) * | 2012-11-16 | 2014-05-21 | Kuraray Europe GmbH | Penetrationsfeste Mehrschichtfolien aus weichmacherhaltigem Polyvinylacetal mit schalldämpfenden Eigenschaften |
| JP6427450B2 (ja) * | 2014-03-31 | 2018-11-21 | 積水化学工業株式会社 | 変性ポリビニルアセタール樹脂 |
-
1980
- 1980-10-31 JP JP15414180A patent/JPS5777051A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5777051A (en) | 1982-05-14 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4308189A (en) | Cationic polymer emulsion | |
| JP5684506B2 (ja) | 数個のカチオン基を含むモノマー化合物及びそれに由来する単位を含むポリマー | |
| KR20080019051A (ko) | 수성 분산액 및 용융 압출된 제품에서 사용하기 위한 비닐알콜 공중합체 | |
| GB2056997A (en) | Copolymers containing cationic groups | |
| JPH0210785B2 (cs) | ||
| JPS6411045B2 (cs) | ||
| JPH08319318A (ja) | ビニルアルコール系重合体 | |
| JP3618440B2 (ja) | ビニルアルコール系重合体 | |
| JPH0328442B2 (cs) | ||
| JPS6213963B2 (cs) | ||
| JPH0225859B2 (cs) | ||
| JPS6221361B2 (cs) | ||
| JPH09302026A (ja) | ポリアリルアミン系誘導体及びその製造方法 | |
| JPS6340419B2 (cs) | ||
| JP3784425B2 (ja) | プラスチゾル組成物の製造方法 | |
| JPH0472304A (ja) | ビニルアセタール系重合体および製法 | |
| JPS6233549A (ja) | 低リンス、高容量の弱塩基性アクリル系イオン交換樹脂およびその製法 | |
| JPH06126195A (ja) | 多孔性アニオン交換樹脂及びその製造方法 | |
| JPS5879003A (ja) | ケイ素含有変性ポリビニルアルコ−ルの製造法 | |
| JPH0147483B2 (cs) | ||
| JPS6234242B2 (cs) | ||
| JPS6345686B2 (cs) | ||
| JPS62207304A (ja) | 界面活性能を有する共重合体の製造法 | |
| JPS59136301A (ja) | 懸濁重合安定剤 | |
| JPS63225608A (ja) | 水溶性共重合体の製造方法 |