JPH0153334B2 - - Google Patents

Info

Publication number
JPH0153334B2
JPH0153334B2 JP58147386A JP14738683A JPH0153334B2 JP H0153334 B2 JPH0153334 B2 JP H0153334B2 JP 58147386 A JP58147386 A JP 58147386A JP 14738683 A JP14738683 A JP 14738683A JP H0153334 B2 JPH0153334 B2 JP H0153334B2
Authority
JP
Japan
Prior art keywords
temperature
less
rolling
slab
cold
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP58147386A
Other languages
English (en)
Japanese (ja)
Other versions
JPS6039126A (ja
Inventor
Noriaki Nagao
Masashi Takahashi
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Sumitomo Metal Industries Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sumitomo Metal Industries Ltd filed Critical Sumitomo Metal Industries Ltd
Priority to JP14738683A priority Critical patent/JPS6039126A/ja
Publication of JPS6039126A publication Critical patent/JPS6039126A/ja
Publication of JPH0153334B2 publication Critical patent/JPH0153334B2/ja
Granted legal-status Critical Current

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C21METALLURGY OF IRON
    • C21DMODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING
    • C21D8/00Modifying the physical properties by deformation combined with, or followed by, heat treatment
    • C21D8/02Modifying the physical properties by deformation combined with, or followed by, heat treatment during manufacturing of plates or strips
    • C21D8/04Modifying the physical properties by deformation combined with, or followed by, heat treatment during manufacturing of plates or strips to produce plates or strips for deep-drawing

Landscapes

  • Chemical & Material Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Physics & Mathematics (AREA)
  • Thermal Sciences (AREA)
  • Crystallography & Structural Chemistry (AREA)
  • Mechanical Engineering (AREA)
  • Materials Engineering (AREA)
  • Metallurgy (AREA)
  • Organic Chemistry (AREA)
  • Heat Treatment Of Steel (AREA)
  • Heat Treatment Of Sheet Steel (AREA)
JP14738683A 1983-08-12 1983-08-12 プレス成形性の優れた冷延鋼板の製造方法 Granted JPS6039126A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP14738683A JPS6039126A (ja) 1983-08-12 1983-08-12 プレス成形性の優れた冷延鋼板の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP14738683A JPS6039126A (ja) 1983-08-12 1983-08-12 プレス成形性の優れた冷延鋼板の製造方法

Publications (2)

Publication Number Publication Date
JPS6039126A JPS6039126A (ja) 1985-02-28
JPH0153334B2 true JPH0153334B2 (enrdf_load_stackoverflow) 1989-11-14

Family

ID=15429079

Family Applications (1)

Application Number Title Priority Date Filing Date
JP14738683A Granted JPS6039126A (ja) 1983-08-12 1983-08-12 プレス成形性の優れた冷延鋼板の製造方法

Country Status (1)

Country Link
JP (1) JPS6039126A (enrdf_load_stackoverflow)

Families Citing this family (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6070123A (ja) * 1983-09-26 1985-04-20 Kawasaki Steel Corp 連続鋳造アルミキルド鋼の熱間圧延方法
CN108796381B (zh) * 2017-04-26 2020-08-25 宝山钢铁股份有限公司 一种罐用高轴向承载力及优良成形性的钢板及其制造方法

Family Cites Families (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5852439A (ja) * 1981-09-21 1983-03-28 Nippon Steel Corp 非時効性で、かつ深絞り加工性が優れ、r値の板面内の異方性の少ない冷延鋼板を連続焼鈍にて製造する方法
JPS5959831A (ja) * 1982-09-30 1984-04-05 Nippon Steel Corp 肌荒の生じない冷延鋼板の製造方法
JPS59116327A (ja) * 1982-12-22 1984-07-05 Sumitomo Metal Ind Ltd 深絞り用冷延アルミキルド鋼板の製造方法

Also Published As

Publication number Publication date
JPS6039126A (ja) 1985-02-28

Similar Documents

Publication Publication Date Title
US4116729A (en) Method for treating continuously cast steel slabs
JPS5849624B2 (ja) 絞り性ならびに形状性にすぐれた高張力冷延鋼板の製造方法
JPS61113724A (ja) プレス成形性の極めて優れた冷延鋼板の製造方法
JPH0153334B2 (enrdf_load_stackoverflow)
JPS6261646B2 (enrdf_load_stackoverflow)
JP3737558B2 (ja) 無方向性電磁鋼板およびその製造方法
JP3818025B2 (ja) 異方性の小さい冷延鋼板の製造方法
JPS593528B2 (ja) 成形性のすぐれた深絞り用亜鉛めつき鋼板の製造法
JPH01191748A (ja) コイル内材質均一性に優れたプレス成形用冷延鋼板の製造方法
JP2672751B2 (ja) 打抜き加工性、成形性に優れた冷延鋼板の製造方法
JPS5913030A (ja) 深絞り性の優れたAlキルド冷延鋼板の製造法
JPS5980727A (ja) 連続焼鈍による絞り性の良好な冷延鋼板の製造方法
JPS6314817A (ja) 曲げ特性の優れた高強度薄鋼板の製造方法
JPS5858413B2 (ja) 成形性のすぐれた高張力めつき鋼板の製造法
JPS6326179B2 (enrdf_load_stackoverflow)
JPH10265845A (ja) 冷間加工性に優れた熱延合金鋼板の製造方法
JPH07100817B2 (ja) 遅時効性冷延鋼板の製造方法
JPS59575B2 (ja) 成形性のすぐれた高張力冷延鋼板の製造法
JPH0639622B2 (ja) 深絞り性と常温非時効性に優れた連続焼鈍による軟質冷延鋼板の製造方法
JPS6235462B2 (enrdf_load_stackoverflow)
JPH09263879A (ja) 加工性と耐時効性の良好な冷延鋼板及びその製造方法
JPS63103025A (ja) 薄鋳帯からの深絞り用冷延鋼板の製造方法
JPH02170921A (ja) 高成形性高張力鋼板の製造方法
JPH045733B2 (enrdf_load_stackoverflow)
JPS6067627A (ja) 連続焼鈍による耐フル−チイング性のすぐれた軟質表面処理用鋼板の製造法