JPH0116283B2 JP59275263A JP27526384A JPH0116283B2 JP H0116283 B2 JPH0116283 B2 JP H0116283B2 JP 59275263 A JP59275263 A JP 59275263A JP 27526384 A JP27526384 A JP 27526384A JP H0116283 B2 JPH0116283 B2 JP H0116283B2
Authority
JP
Japan
Prior art keywords
temperature
less
steel
toughness
weldability
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP59275263A
Other languages
English (en)
Japanese (ja)
Other versions
JPS61149430A (ja
Inventor
Asao Narimoto
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JFE Steel Corp
Original Assignee
Kawasaki Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kawasaki Steel Corp filed Critical Kawasaki Steel Corp
Priority to JP27526384A priority Critical patent/JPS61149430A/ja
Publication of JPS61149430A publication Critical patent/JPS61149430A/ja
Publication of JPH0116283B2 publication Critical patent/JPH0116283B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Heat Treatment Of Steel (AREA)
JP27526384A 1984-12-25 1984-12-25 低温じん性および溶接性の優れた低C−Cu析出型高張力鋼の製造方法 Granted JPS61149430A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP27526384A JPS61149430A (ja) 1984-12-25 1984-12-25 低温じん性および溶接性の優れた低C−Cu析出型高張力鋼の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP27526384A JPS61149430A (ja) 1984-12-25 1984-12-25 低温じん性および溶接性の優れた低C−Cu析出型高張力鋼の製造方法

Publications (2)

Publication Number Publication Date
JPS61149430A JPS61149430A (ja) 1986-07-08
JPH0116283B2 true JPH0116283B2 (enrdf_load_html_response) 1989-03-23

Family

ID=17552976

Family Applications (1)

Application Number Title Priority Date Filing Date
JP27526384A Granted JPS61149430A (ja) 1984-12-25 1984-12-25 低温じん性および溶接性の優れた低C−Cu析出型高張力鋼の製造方法

Country Status (1)

Country Link
JP (1) JPS61149430A (enrdf_load_html_response)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH0668126B2 (ja) * 1988-07-15 1994-08-31 川崎製鉄株式会社 溶接継手部の靭性に優れた鋼板の製造方法
JP5284075B2 (ja) * 2008-12-25 2013-09-11 株式会社神戸製鋼所 脆性亀裂伝播停止特性に優れた構造用厚鋼板
JP6242415B2 (ja) 2016-02-25 2017-12-06 株式会社日本製鋼所 強度−低温靱性バランスに優れたCu含有低合金鋼およびその製造方法

Family Cites Families (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6059018A (ja) * 1983-08-03 1985-04-05 Nippon Steel Corp 溶接性および低温靭性の優れたCu添加鋼の製造法

Also Published As

Publication number Publication date
JPS61149430A (ja) 1986-07-08

Similar Documents

Publication Publication Date Title
JPH0432514A (ja) 圧延ままで表面異常相のない軟質線材の製造方法
JPS6410564B2 (enrdf_load_html_response)
JPS5810442B2 (ja) 加工性のすぐれた高靭性高張力鋼の製造法
JPS6141968B2 (enrdf_load_html_response)
JPS6223929A (ja) 冷間鍛造用鋼の製造方法
KR20000043762A (ko) 연성이 향상된 초고강도 냉연강판의 제조방법
JPH0116283B2 (enrdf_load_html_response)
JPH0225968B2 (enrdf_load_html_response)
JPH0718326A (ja) オンライン熱処理による高強度高靭性レールの製造方法
JPS6286122A (ja) 高強度高溶接性構造用鋼の製造方法
JPH02310313A (ja) 耐候性鋼の製造方法
JPH09291312A (ja) 高強度非調質ボルト用線材の製法
JPS6365021A (ja) 低温靭性の優れたb含有非調質高張力鋼板の製造方法
JPS62149814A (ja) 直接焼入法による低炭素高強度継目無鋼管の製造方法
JPS6213523A (ja) 低温用棒鋼の製造方法
JPS6046318A (ja) 耐硫化物割れ性の優れた鋼の製造方法
JP2626421B2 (ja) 溶接性に優れた高張力鋼の製造方法
JPH027368B2 (enrdf_load_html_response)
JPH03229818A (ja) 低温用鋼の製造方法
JP2024530982A (ja) 水素誘起割れ抵抗性及び低温衝撃靭性に優れた鋼材及びその製造方法
JPS63128117A (ja) 非調質高張力鋼の製造方法
KR100514813B1 (ko) 중고온용 Cr-Mo강의 제조방법
JPS58120727A (ja) セパレ−シヨンが少なく溶接性に優れた高靭性非調質高張力鋼板の製造方法
JPH0570885A (ja) 球状船首用低降伏点焼入れ鋼とその製造法
JPS62164821A (ja) 伸線加工用Si―Mn系低合金鋼線材の製造方法