JP3490339B2 - 吸水性樹脂の製造装置 - Google Patents
吸水性樹脂の製造装置Info
- Publication number
- JP3490339B2 JP3490339B2 JP13500999A JP13500999A JP3490339B2 JP 3490339 B2 JP3490339 B2 JP 3490339B2 JP 13500999 A JP13500999 A JP 13500999A JP 13500999 A JP13500999 A JP 13500999A JP 3490339 B2 JP3490339 B2 JP 3490339B2
- Authority
- JP
- Japan
- Prior art keywords
- absorbent resin
- water
- monomer mixture
- belt
- support belt
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Solid-Sorbent Or Filter-Aiding Compositions (AREA)
- Polymerisation Methods In General (AREA)
- Other Resins Obtained By Reactions Not Involving Carbon-To-Carbon Unsaturated Bonds (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13500999A JP3490339B2 (ja) | 1998-05-15 | 1999-05-14 | 吸水性樹脂の製造装置 |
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13377198 | 1998-05-15 | ||
| JP10-133771 | 1998-05-15 | ||
| JP13500999A JP3490339B2 (ja) | 1998-05-15 | 1999-05-14 | 吸水性樹脂の製造装置 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2000034305A JP2000034305A (ja) | 2000-02-02 |
| JP2000034305A5 JP2000034305A5 (enExample) | 2001-11-20 |
| JP3490339B2 true JP3490339B2 (ja) | 2004-01-26 |
Family
ID=26468025
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP13500999A Expired - Lifetime JP3490339B2 (ja) | 1998-05-15 | 1999-05-14 | 吸水性樹脂の製造装置 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3490339B2 (enExample) |
Families Citing this family (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP4782261B2 (ja) * | 1998-08-24 | 2011-09-28 | 株式会社日本触媒 | 吸水性樹脂含水ゲル状物の製造方法 |
| JP4087682B2 (ja) | 2002-11-07 | 2008-05-21 | 株式会社日本触媒 | 吸水性樹脂の製造方法および製造装置 |
| JP2006160845A (ja) * | 2004-12-06 | 2006-06-22 | Asahi Kasei Chemicals Corp | 吸水性樹脂の製造方法 |
| JP4602746B2 (ja) * | 2004-12-06 | 2010-12-22 | 旭化成ケミカルズ株式会社 | 吸水性樹脂の製造装置及び製造方法 |
| JP4713167B2 (ja) | 2005-01-21 | 2011-06-29 | 株式会社日本触媒 | 吸水性樹脂の製造方法 |
| CN104231144B (zh) | 2009-02-17 | 2018-05-15 | 株式会社日本触媒 | 聚丙烯酸系吸水性树脂粉末及其制造方法 |
| CN110041449B (zh) * | 2019-04-24 | 2023-09-26 | 山东昊月新材料股份有限公司 | 一种高吸收树脂连续聚合设备及其使用方法 |
-
1999
- 1999-05-14 JP JP13500999A patent/JP3490339B2/ja not_active Expired - Lifetime
Also Published As
| Publication number | Publication date |
|---|---|
| JP2000034305A (ja) | 2000-02-02 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR100476170B1 (ko) | 흡수성수지 함수겔상물의 제조방법 | |
| US6241928B1 (en) | Method for production of shaped hydrogel of absorbent resin | |
| EP0289338B1 (en) | Hydrophilic polymer and method for production | |
| EP2269720A1 (en) | Method for manufacturing water-absorbing resin via surface crosslinking | |
| Kishi et al. | Thermo-responsive devices using poly (vinyl methyl ether) hydrogels | |
| JP6029800B2 (ja) | 吸水性樹脂粒子 | |
| US9447203B2 (en) | Method for producing water absorbent polyacrylic acid (salt) resin powder, and water absorbent polyacrylic acid (salt) resin powder | |
| EP1589040B1 (en) | Method for continuous production of water absorbent resin | |
| CN102762616B (zh) | 制备吸水性聚合物颗粒的方法 | |
| EP1683813B1 (en) | Production method of water-absorbent resin | |
| CA1231318A (en) | Method for manufacturing microporous membrane | |
| CA1268295A (en) | Water absorbent acrylic copolymers | |
| JP5128098B2 (ja) | 粒子状吸水剤の製造方法および粒子状吸水剤 | |
| CN105026638B (zh) | 通气插件 | |
| JP2004352940A (ja) | 吸水性樹脂の製造方法および鋤型混合装置 | |
| JP2000034305A (ja) | 吸水性樹脂の製造装置 | |
| JP3597597B2 (ja) | 吸水性樹脂及びその製造方法 | |
| JP4782261B2 (ja) | 吸水性樹脂含水ゲル状物の製造方法 | |
| JPH11147902A (ja) | 吸水性樹脂の製造方法、吸水剤およびその製造方法 | |
| US9255190B2 (en) | Process for the continuous preparation of water-absorbent polymers | |
| JP2000017004A (ja) | 吸水性樹脂の連続製造装置 | |
| JP2567453B2 (ja) | 水溶性重合体および水膨潤性重合体の製造方法 | |
| JP2004352849A (ja) | 吸水性樹脂の製造装置および製造方法 | |
| EP0206808A2 (en) | Continuous method for preparing polyacrylate resins | |
| EP1440984B1 (en) | Method of manufacturing water-absorbing shaped body |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| A01 | Written decision to grant a patent or to grant a registration (utility model) |
Free format text: JAPANESE INTERMEDIATE CODE: A01 Effective date: 20031021 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20081107 Year of fee payment: 5 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20081107 Year of fee payment: 5 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20091107 Year of fee payment: 6 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20091107 Year of fee payment: 6 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20101107 Year of fee payment: 7 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20101107 Year of fee payment: 7 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20111107 Year of fee payment: 8 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20121107 Year of fee payment: 9 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20131107 Year of fee payment: 10 |
|
| EXPY | Cancellation because of completion of term |