JP3407983B2 - アルカリ蓄電池用非焼結式正極の製造方法 - Google Patents

アルカリ蓄電池用非焼結式正極の製造方法

Info

Publication number
JP3407983B2
JP3407983B2 JP17912094A JP17912094A JP3407983B2 JP 3407983 B2 JP3407983 B2 JP 3407983B2 JP 17912094 A JP17912094 A JP 17912094A JP 17912094 A JP17912094 A JP 17912094A JP 3407983 B2 JP3407983 B2 JP 3407983B2
Authority
JP
Japan
Prior art keywords
nickel
lithium
positive electrode
hydroxide
nickel hydroxide
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
JP17912094A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0845506A5 (enExample
JPH0845506A (ja
Inventor
謙二 有澤
雅行 寺坂
浩三 大槻
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Sanyo Electric Co Ltd
Original Assignee
Sanyo Electric Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sanyo Electric Co Ltd filed Critical Sanyo Electric Co Ltd
Priority to JP17912094A priority Critical patent/JP3407983B2/ja
Publication of JPH0845506A publication Critical patent/JPH0845506A/ja
Publication of JPH0845506A5 publication Critical patent/JPH0845506A5/ja
Application granted granted Critical
Publication of JP3407983B2 publication Critical patent/JP3407983B2/ja
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Classifications

    • Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
    • Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
    • Y02E60/10—Energy storage using batteries

Landscapes

  • Battery Electrode And Active Subsutance (AREA)
JP17912094A 1994-07-29 1994-07-29 アルカリ蓄電池用非焼結式正極の製造方法 Expired - Fee Related JP3407983B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP17912094A JP3407983B2 (ja) 1994-07-29 1994-07-29 アルカリ蓄電池用非焼結式正極の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP17912094A JP3407983B2 (ja) 1994-07-29 1994-07-29 アルカリ蓄電池用非焼結式正極の製造方法

Publications (3)

Publication Number Publication Date
JPH0845506A JPH0845506A (ja) 1996-02-16
JPH0845506A5 JPH0845506A5 (enExample) 2001-03-16
JP3407983B2 true JP3407983B2 (ja) 2003-05-19

Family

ID=16060360

Family Applications (1)

Application Number Title Priority Date Filing Date
JP17912094A Expired - Fee Related JP3407983B2 (ja) 1994-07-29 1994-07-29 アルカリ蓄電池用非焼結式正極の製造方法

Country Status (1)

Country Link
JP (1) JP3407983B2 (enExample)

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP4100736B2 (ja) * 1996-09-27 2008-06-11 シャープ株式会社 非水系二次電池用正極活物質ニッケル酸リチウムの製造方法

Also Published As

Publication number Publication date
JPH0845506A (ja) 1996-02-16

Similar Documents

Publication Publication Date Title
EP3719885A1 (en) Ternary precursor material and preparation method therefor
KR100454542B1 (ko) 알칼리축전지용비소결식니켈전극
JPH0777129B2 (ja) ニッケル電極用活物質及びその製造方法、ニッケル電極及びそれを用いたアルカリ電池の製造方法
JPH0559546B2 (enExample)
CN1187853C (zh) 碱性蓄电池的正极活性材料
CN103109402B (zh) 碱蓄电池
JP3976482B2 (ja) アルカリ蓄電池用正極活物質の製造方法およびこの正極活物質を用いたニッケル電極ならびにこのニッケル電極を用いたアルカリ蓄電池
JP3356628B2 (ja) アルカリ蓄電池用のβ−水酸化コバルト層で覆われた水酸化ニッケル及びその製造法
JP2000077068A (ja) アルカリ二次電池用ニッケル正極
CN102471091A (zh) 钴铈化合物、碱蓄电池和钴铈化合物的制造方法
CN107251284B (zh) 用于碱性可充电电池的镍氢氧化物正极
CN119092658B (zh) 正极活性材料、镍电极和碱性蓄电池
JP2002208400A (ja) アルカリ二次電池正極活物質用水酸化ニッケル、それを用いたアルカリ二次電池、その特性評価方法およびその製造方法
JP3253476B2 (ja) アルカリ蓄電池用非焼結式ニッケル極
CN116573680A (zh) 一种钴酸锂材料及其制备方法与应用
US9899676B2 (en) Nickel hydroxide positive electrode for alkaline rechargeable battery
JPH0950805A (ja) アルカリ蓄電池用ニッケル電極及びニッケル電極用活物質並びにその製造方法、アルカリ蓄電池
US20160233505A1 (en) Nickel Hydroxide Positive Electrode for Alkaline Rechargeable Battery
JPH10284075A (ja) アルカリ電池用正極活物質の製造方法
JPH10302788A (ja) アルカリ蓄電池用ニッケル電極活物質の製造方法
JP3229800B2 (ja) アルカリ蓄電池用非焼結式ニッケル極
JPH0845506A (ja) アルカリ蓄電池用非焼結式正極の製造方法
JPH1012236A (ja) アルカリ蓄電池用のα−水酸化コバルト層で覆われた水酸化ニッケル及びその製造法
JPH08203522A (ja) アルカリ蓄電池用ニッケル活物質及びその製法
JPH11307093A (ja) Mn含有複合水酸化ニッケル活物質及びその製造方法

Legal Events

Date Code Title Description
LAPS Cancellation because of no payment of annual fees