JP3297090B2 - 降伏比上昇の少ない高張力鋼材の加工方法 - Google Patents

降伏比上昇の少ない高張力鋼材の加工方法

Info

Publication number
JP3297090B2
JP3297090B2 JP26342992A JP26342992A JP3297090B2 JP 3297090 B2 JP3297090 B2 JP 3297090B2 JP 26342992 A JP26342992 A JP 26342992A JP 26342992 A JP26342992 A JP 26342992A JP 3297090 B2 JP3297090 B2 JP 3297090B2
Authority
JP
Japan
Prior art keywords
less
yield ratio
steel
processing
phase
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
JP26342992A
Other languages
English (en)
Japanese (ja)
Other versions
JPH06116636A5 (enExample
JPH06116636A (ja
Inventor
清 内田
智也 小関
虔一 天野
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JFE Steel Corp
Original Assignee
JFE Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JFE Steel Corp filed Critical JFE Steel Corp
Priority to JP26342992A priority Critical patent/JP3297090B2/ja
Publication of JPH06116636A publication Critical patent/JPH06116636A/ja
Publication of JPH06116636A5 publication Critical patent/JPH06116636A5/ja
Application granted granted Critical
Publication of JP3297090B2 publication Critical patent/JP3297090B2/ja
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Landscapes

  • Heat Treatment Of Steel (AREA)
JP26342992A 1992-10-01 1992-10-01 降伏比上昇の少ない高張力鋼材の加工方法 Expired - Fee Related JP3297090B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP26342992A JP3297090B2 (ja) 1992-10-01 1992-10-01 降伏比上昇の少ない高張力鋼材の加工方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP26342992A JP3297090B2 (ja) 1992-10-01 1992-10-01 降伏比上昇の少ない高張力鋼材の加工方法

Publications (3)

Publication Number Publication Date
JPH06116636A JPH06116636A (ja) 1994-04-26
JPH06116636A5 JPH06116636A5 (enExample) 2001-06-19
JP3297090B2 true JP3297090B2 (ja) 2002-07-02

Family

ID=17389380

Family Applications (1)

Application Number Title Priority Date Filing Date
JP26342992A Expired - Fee Related JP3297090B2 (ja) 1992-10-01 1992-10-01 降伏比上昇の少ない高張力鋼材の加工方法

Country Status (1)

Country Link
JP (1) JP3297090B2 (enExample)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US6555253B2 (en) 1997-05-08 2003-04-29 Sanyo Electric Co., Ltd. Organic electroluminescent device

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US6555253B2 (en) 1997-05-08 2003-04-29 Sanyo Electric Co., Ltd. Organic electroluminescent device
US6743526B2 (en) 1997-05-08 2004-06-01 Sanyo Electric Co., Ltd. Organic electroluminescent device

Also Published As

Publication number Publication date
JPH06116636A (ja) 1994-04-26

Similar Documents

Publication Publication Date Title
JP2567150B2 (ja) 低温用高強度低降伏比ラインパイプ材の製造法
JP2000512346A (ja) 熱機械的制御された工程を用いて作られた降伏/引張の比が低い高強度耐候性鋼
JPH0823048B2 (ja) 焼付硬化性と加工性に優れた熱延鋼板の製造方法
JP4405026B2 (ja) 結晶粒の微細な高靱性高張力鋼の製造方法
JPH05105957A (ja) 耐熱性高強度ボルトの製造方法
JPH06128631A (ja) 低温靱性の優れた高マンガン超高張力鋼の製造方法
JP3290595B2 (ja) 靱性、溶接性に優れた高張力厚鋼板の製造方法
JP3246993B2 (ja) 低温靭性に優れた厚鋼板の製造方法
JPH0781164B2 (ja) 高張力高靭性鋼板の製造方法
JPS60121228A (ja) 調質型高張力厚鋼板の製造方法
JP3300444B2 (ja) 耐候性の良好な低降伏比高張力鋼板の製造方法
JP3229107B2 (ja) 一様伸びの優れた低降伏比高張力鋼板の製造方法
JP2828303B2 (ja) 強靭な厚鋼板の製造方法
JP2706159B2 (ja) 溶接性の良好な低降伏比高張力鋼の製造方法
JP3033459B2 (ja) 非調質高張力鋼の製造方法
JPH06116636A (ja) 降伏比上昇の少ない高張力鋼材の加工方法
JP2529042B2 (ja) 冷間成形による建築用低降伏比鋼管の製造法
JP2655956B2 (ja) 建築構造用低降伏比耐火鋼板の製造方法
JPH0641633A (ja) 降伏比上昇の少ない高張力鋼材の加工方法
JP2541389B2 (ja) 低降伏比高張力鋼の製造方法
JPH0670250B2 (ja) 靭性の優れた調質型高張力鋼板の製造方法
JPH06340924A (ja) 低降伏比高張力鋼の製造方法
JP2784207B2 (ja) 加工用熱延鋼板の製造方法及び熱延鋼板の加工熱処理法
JP2000096137A (ja) 微細結晶粒組織鋼の製造方法
JP3007246B2 (ja) 溶接性の優れた降伏比80%以下の590N/mm2級高張力鋼の製造法

Legal Events

Date Code Title Description
LAPS Cancellation because of no payment of annual fees