JP3238950B2 - アルカリ蓄電池の活性化法 - Google Patents
アルカリ蓄電池の活性化法Info
- Publication number
- JP3238950B2 JP3238950B2 JP20543492A JP20543492A JP3238950B2 JP 3238950 B2 JP3238950 B2 JP 3238950B2 JP 20543492 A JP20543492 A JP 20543492A JP 20543492 A JP20543492 A JP 20543492A JP 3238950 B2 JP3238950 B2 JP 3238950B2
- Authority
- JP
- Japan
- Prior art keywords
- cobalt
- powder
- storage battery
- battery
- positive electrode
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP20543492A JP3238950B2 (ja) | 1992-07-31 | 1992-07-31 | アルカリ蓄電池の活性化法 |
| US08/099,421 US5405714A (en) | 1992-07-31 | 1993-07-30 | Method for activating an alkaline storage cell employing a non-sintered type nickel positive electrode |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP20543492A JP3238950B2 (ja) | 1992-07-31 | 1992-07-31 | アルカリ蓄電池の活性化法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH0652858A JPH0652858A (ja) | 1994-02-25 |
| JPH0652858A5 JPH0652858A5 (enExample) | 1999-09-24 |
| JP3238950B2 true JP3238950B2 (ja) | 2001-12-17 |
Family
ID=16506806
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP20543492A Expired - Fee Related JP3238950B2 (ja) | 1992-07-31 | 1992-07-31 | アルカリ蓄電池の活性化法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3238950B2 (enExample) |
-
1992
- 1992-07-31 JP JP20543492A patent/JP3238950B2/ja not_active Expired - Fee Related
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0652858A (ja) | 1994-02-25 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP3191751B2 (ja) | アルカリ蓄電池及びその正極活物質の表面処理方法 | |
| US6740450B2 (en) | Hydrogen-absorbing alloy for battery, method for producing the same, and alkaline storage battery using the same | |
| JP3238949B2 (ja) | アルカリ蓄電池の活性化法 | |
| JP2899849B2 (ja) | アルカリ二次電池用水素吸蔵合金の表面処理法とその表面処理法を施した水素吸蔵合金を電極として備えたアルカリ二次電池 | |
| JP3433008B2 (ja) | アルカリ蓄電池用水素吸蔵合金の製造方法 | |
| JPH0652858A (ja) | アルカリ蓄電池の活性化法 | |
| JP3188000B2 (ja) | 非焼結式ニッケル正極 | |
| JPH03272563A (ja) | アルカリ亜鉛蓄電池 | |
| JP3238986B2 (ja) | アルカリ蓄電池の活性化法 | |
| JP3530309B2 (ja) | 水素吸蔵合金電極の製造方法 | |
| JP2558759B2 (ja) | アルカリ蓄電池用カドミウム負極の製造法 | |
| JP3316946B2 (ja) | アルカリ蓄電池用焼結式カドミウム陰極板及びその製造方法 | |
| JP2614486B2 (ja) | アルカリ亜鉛蓄電池 | |
| JP2931316B2 (ja) | アルカリ亜鉛蓄電池の製造方法 | |
| JPH05190175A (ja) | アルカリ二次電池用水素吸蔵合金の表面処理法 | |
| JPH1074510A (ja) | アルカリ蓄電池用水素吸蔵合金の製造方法 | |
| JPH0410181B2 (enExample) | ||
| JP2001202956A (ja) | アルカリ蓄電池用ニッケル電極活物質、アルカリ蓄電池およびアルカリ蓄電池の初期化成処理方法 | |
| JP3530327B2 (ja) | 水素吸蔵合金電極の製造方法 | |
| JP2865397B2 (ja) | アルカリ蓄電池の製造方法 | |
| JPH1021905A (ja) | アルカリ蓄電池用非焼結式ニッケル極 | |
| JPS5929364A (ja) | 鉛蓄電池用電極の製造法 | |
| JPS63174273A (ja) | アルカリ蓄電池用亜鉛極の製法 | |
| KR100331439B1 (ko) | 아연전극,그제조방법및이를채용한니켈아연2차전지 | |
| JPH10106620A (ja) | アルカリ蓄電池 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |