JP2501773Y2 - 薄形鉛蓄電池 - Google Patents
薄形鉛蓄電池Info
- Publication number
- JP2501773Y2 JP2501773Y2 JP1990077249U JP7724990U JP2501773Y2 JP 2501773 Y2 JP2501773 Y2 JP 2501773Y2 JP 1990077249 U JP1990077249 U JP 1990077249U JP 7724990 U JP7724990 U JP 7724990U JP 2501773 Y2 JP2501773 Y2 JP 2501773Y2
- Authority
- JP
- Japan
- Prior art keywords
- acid battery
- elastic body
- thin lead
- air passage
- resin films
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02P—CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02P70/00—Climate change mitigation technologies in the production process for final industrial or consumer products
- Y02P70/50—Manufacturing or production processes characterised by the final manufactured product
Landscapes
- Gas Exhaust Devices For Batteries (AREA)
- Secondary Cells (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1990077249U JP2501773Y2 (ja) | 1990-07-20 | 1990-07-20 | 薄形鉛蓄電池 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1990077249U JP2501773Y2 (ja) | 1990-07-20 | 1990-07-20 | 薄形鉛蓄電池 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH0435350U JPH0435350U (enExample) | 1992-03-24 |
| JP2501773Y2 true JP2501773Y2 (ja) | 1996-06-19 |
Family
ID=31619462
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1990077249U Expired - Lifetime JP2501773Y2 (ja) | 1990-07-20 | 1990-07-20 | 薄形鉛蓄電池 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP2501773Y2 (enExample) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP4604535B2 (ja) * | 2004-03-30 | 2011-01-05 | トヨタ自動車株式会社 | ラミネート型二次電池 |
| JP5633032B2 (ja) * | 2009-03-26 | 2014-12-03 | エリーパワー株式会社 | 二次電池 |
| JP7121905B2 (ja) * | 2018-09-04 | 2022-08-19 | トヨタ自動車株式会社 | 密閉型電池 |
-
1990
- 1990-07-20 JP JP1990077249U patent/JP2501773Y2/ja not_active Expired - Lifetime
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0435350U (enExample) | 1992-03-24 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS62147652A (ja) | 密閉形鉛蓄電池 | |
| JPH023267B2 (enExample) | ||
| EP1061601A4 (en) | THIN BATTERY AND PRODUCTION METHOD | |
| JP2501773Y2 (ja) | 薄形鉛蓄電池 | |
| JPS63174265A (ja) | 薄形密閉式鉛蓄電池の製造方法 | |
| JPH0828209B2 (ja) | 鉛蓄電池のパック構造 | |
| US3741810A (en) | Battery construction | |
| JPS6345737Y2 (enExample) | ||
| JP2000156211A5 (enExample) | ||
| US3681145A (en) | Fuel cell battery for reacting a reactant,such as hydrazine especially,dissolved in electrolyte | |
| JPS62131469A (ja) | 薄形密閉鉛蓄電池 | |
| JP3008722B2 (ja) | 密閉形蓄電池 | |
| CN221486564U (zh) | 二次电池及电池包 | |
| JPH0451938B2 (enExample) | ||
| JPS59143282A (ja) | ボタン型空気電池の製造法 | |
| JPS62122050A (ja) | 密閉形鉛蓄電池 | |
| JP2003123711A (ja) | 蓄電池 | |
| JPH05129009A (ja) | 密閉形鉛蓄電池 | |
| JPS61181059A (ja) | 密閉型鉛蓄電池 | |
| JPS63291354A (ja) | 電池の製造法 | |
| JPS63187561A (ja) | シ−ル形鉛蓄電池製造法 | |
| JPH0193066A (ja) | 密閉形鉛蓄電池の製造法 | |
| JP2727559B2 (ja) | 密閉形鉛電池の製造方法 | |
| JPS6247972A (ja) | シ−ル型鉛蓄電池 | |
| JPS5866257A (ja) | 密閉電池 |