JP2016503387A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2016503387A5 JP2016503387A5 JP2015544122A JP2015544122A JP2016503387A5 JP 2016503387 A5 JP2016503387 A5 JP 2016503387A5 JP 2015544122 A JP2015544122 A JP 2015544122A JP 2015544122 A JP2015544122 A JP 2015544122A JP 2016503387 A5 JP2016503387 A5 JP 2016503387A5
- Authority
- JP
- Japan
- Prior art keywords
- bonded
- zircon
- component
- substrate
- refractory
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US13/685,149 | 2012-11-26 | ||
| US13/685,149 US8956484B2 (en) | 2012-11-26 | 2012-11-26 | Method for bonding zircon substrates |
| PCT/US2013/071119 WO2014081904A1 (en) | 2012-11-26 | 2013-11-21 | Method for bonding zircon substrates |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2016503387A JP2016503387A (ja) | 2016-02-04 |
| JP2016503387A5 true JP2016503387A5 (https=) | 2017-09-14 |
| JP6246226B2 JP6246226B2 (ja) | 2017-12-13 |
Family
ID=50772222
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2015544122A Expired - Fee Related JP6246226B2 (ja) | 2012-11-26 | 2013-11-21 | ジルコン基板を結合させる方法 |
Country Status (7)
| Country | Link |
|---|---|
| US (1) | US8956484B2 (https=) |
| EP (1) | EP2923351B1 (https=) |
| JP (1) | JP6246226B2 (https=) |
| KR (1) | KR20150089068A (https=) |
| CN (1) | CN105122333A (https=) |
| TW (1) | TWI588103B (https=) |
| WO (1) | WO2014081904A1 (https=) |
Families Citing this family (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR20180130535A (ko) * | 2016-04-07 | 2018-12-07 | 마테리온 코포레이션 | 산화 베릴륨 일체형 저항 히터 |
| CN108368761A (zh) * | 2016-10-21 | 2018-08-03 | 康明斯排放处理公司 | 包括板的催化剂基底和过滤器结构及其形成方法 |
| KR102069423B1 (ko) * | 2017-12-19 | 2020-01-22 | 주식회사 티씨케이 | 접합 세라믹 및 이의 제조방법 |
| KR102069422B1 (ko) * | 2017-12-19 | 2020-01-22 | 주식회사 티씨케이 | 유체 흐름이 가능한 유로가 형성된 접합 세라믹 및 이의 제조방법 |
Family Cites Families (20)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3338696A (en) | 1964-05-06 | 1967-08-29 | Corning Glass Works | Sheet forming apparatus |
| BE757057A (fr) | 1969-10-06 | 1971-04-05 | Corning Glass Works | Procede et appareil de controle d'epaisseur d'une feuille de verre nouvellement etiree |
| US4925608A (en) * | 1988-09-27 | 1990-05-15 | Norton Company | Joining of SiC parts by polishing and hipping |
| JPH08118467A (ja) * | 1994-10-21 | 1996-05-14 | Matsushita Electric Ind Co Ltd | スクリーン印刷用グリーンシート |
| JP4370624B2 (ja) * | 1997-09-22 | 2009-11-25 | 嘉信 本橋 | アルミナ部材の接合方法 |
| TW508600B (en) * | 2000-03-30 | 2002-11-01 | Taiyo Yuden Kk | Laminated ceramic capacitor and its manufacturing method |
| CN102992592A (zh) * | 2000-12-01 | 2013-03-27 | 康宁股份有限公司 | 熔融法生产平板玻璃所用的等静压板的下沉控制 |
| US7722731B2 (en) * | 2001-08-07 | 2010-05-25 | Uchicago Argonne, Llc | Joining of advanced materials by plastic deformation |
| US7943241B2 (en) * | 2004-11-29 | 2011-05-17 | Kyocera Corporation | Composite ceramic body |
| JP2007119262A (ja) * | 2005-10-25 | 2007-05-17 | Hideaki Inoue | アルミナセラミックス物品の製造方法 |
| CN2874389Y (zh) * | 2006-01-07 | 2007-02-28 | 段红 | 一种氮窑用承烧板 |
| CN101108775B (zh) | 2007-08-27 | 2010-10-13 | 中钢集团洛阳耐火材料研究院有限公司 | 一种氧化锆制品的制造方法 |
| WO2009070230A1 (en) | 2007-11-29 | 2009-06-04 | Corning Incorporated | Creep resistant multiple layer refractory used in a glass manufacturing system |
| US7988804B2 (en) * | 2008-05-02 | 2011-08-02 | Corning Incorporated | Material and method for bonding zircon blocks |
| JP5727929B2 (ja) | 2008-05-20 | 2015-06-03 | コーニング インコーポレイテッド | 低歪み速度の改良されたジルコン材料および物品 |
| JP5841329B2 (ja) * | 2009-12-25 | 2016-01-13 | 株式会社日本セラテック | セラミックス接合体の製造方法 |
| EP2539141A1 (en) * | 2010-02-24 | 2013-01-02 | Corning Incorporated | Method of making a densified body by isostatically pressing in deep sea |
| TWI535672B (zh) | 2010-05-28 | 2016-06-01 | 康寧公司 | 複合隔離管 |
| US8652281B2 (en) * | 2011-01-31 | 2014-02-18 | The United States Of America, As Represented By The Secretary Of The Navy | Spinel ceramics via edge bonding |
| TWI541208B (zh) | 2011-04-29 | 2016-07-11 | 康寧公司 | 用於製造玻璃物件的設備與方法 |
-
2012
- 2012-11-26 US US13/685,149 patent/US8956484B2/en not_active Expired - Fee Related
-
2013
- 2013-11-21 WO PCT/US2013/071119 patent/WO2014081904A1/en not_active Ceased
- 2013-11-21 JP JP2015544122A patent/JP6246226B2/ja not_active Expired - Fee Related
- 2013-11-21 EP EP13856812.6A patent/EP2923351B1/en not_active Not-in-force
- 2013-11-21 CN CN201380067900.1A patent/CN105122333A/zh active Pending
- 2013-11-21 TW TW102142486A patent/TWI588103B/zh not_active IP Right Cessation
- 2013-11-21 KR KR1020157016997A patent/KR20150089068A/ko not_active Withdrawn
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2016503387A5 (https=) | ||
| PH12012501893A1 (en) | Method for manufacturing glass blank for magnetic recording medium glass substrate, method of manufacturing magnetic recording medium glass substrate, and method of manufacturing magnetic recording medium | |
| JP2017525650A5 (https=) | ||
| JP2014179160A5 (https=) | ||
| JP2009533855A5 (https=) | ||
| WO2011094300A3 (en) | Process and structure for high temperature selective fusion bonding | |
| JPWO2014156507A1 (ja) | 複合基板及び弾性波デバイス | |
| JP2015224143A5 (https=) | ||
| CN104550959A (zh) | 一种金属复合材料零件的成形方法 | |
| MY163806A (en) | Manufacturing method of glass substrate for magnetic disk, manufacturing method of glass blank, glass substrate for magnetic disk, and glass blank | |
| JP2012195095A5 (https=) | ||
| WO2012113651A3 (de) | Verfahren zur herstellung von leichtbaustrukturelementen | |
| WO2010139499A3 (de) | Mikromechanisches bauelement mit eutektischer verbindung zwischen zwei substraten und verfahren zum herstellen eines derartigen mikromechanischen bauelements | |
| EP3040322A3 (en) | Process and formulation to join ceramic foams while maintaining structural and physical characteristics across the bond surface | |
| AU2015243024A1 (en) | Bonding dissimilar ceramic components | |
| JP5553793B2 (ja) | ロータリーキルンの内張り煉瓦 | |
| JP6246226B2 (ja) | ジルコン基板を結合させる方法 | |
| CN103912655A (zh) | 一种耐高温耐磨损齿轮 | |
| JP2016507396A5 (https=) | ||
| CN104209323B (zh) | 一种复合轧制法生产厚板用碳钢板坯结合表面预处理方法 | |
| WO2009034654A1 (ja) | 鉄鋼部材の接合方法、鉄鋼部材からなる接合体における接合力強化方法、鉄鋼製品及びダイカスト製品 | |
| JP2011240470A5 (https=) | ||
| JP2005179160A (ja) | 陶器補修又は造形変更用粘土および陶器補修又は造形変更方法 | |
| NZ701323A (en) | Worktop for pieces of furniture and method for joining slabs so as to obtain said worktop | |
| WO2008129622A1 (ja) | 鉄鋼部材の接合方法、鉄鋼部材からなる接合体における接合力強化方法及び鉄鋼製品 |