JP2013204088A5 - - Google Patents

Download PDF

Info

Publication number
JP2013204088A5
JP2013204088A5 JP2012074173A JP2012074173A JP2013204088A5 JP 2013204088 A5 JP2013204088 A5 JP 2013204088A5 JP 2012074173 A JP2012074173 A JP 2012074173A JP 2012074173 A JP2012074173 A JP 2012074173A JP 2013204088 A5 JP2013204088 A5 JP 2013204088A5
Authority
JP
Japan
Prior art keywords
copper foil
electrolytic
electrolytic copper
tungsten
foil
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
JP2012074173A
Other languages
English (en)
Japanese (ja)
Other versions
JP2013204088A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2012074173A priority Critical patent/JP2013204088A/ja
Priority claimed from JP2012074173A external-priority patent/JP2013204088A/ja
Priority to KR1020157022124A priority patent/KR20150097821A/ko
Priority to TW101127554A priority patent/TWI496954B/zh
Priority to KR1020137006252A priority patent/KR101669087B1/ko
Priority to PCT/JP2012/069368 priority patent/WO2013018773A1/ja
Priority to CN201280004436.7A priority patent/CN103348041B/zh
Priority to EP12819841.3A priority patent/EP2660359A4/en
Priority to US13/965,291 priority patent/US9890463B2/en
Publication of JP2013204088A publication Critical patent/JP2013204088A/ja
Publication of JP2013204088A5 publication Critical patent/JP2013204088A5/ja
Withdrawn legal-status Critical Current

Links

JP2012074173A 2011-07-29 2012-03-28 電解銅箔製箔用電解液及び電解銅箔 Withdrawn JP2013204088A (ja)

Priority Applications (8)

Application Number Priority Date Filing Date Title
JP2012074173A JP2013204088A (ja) 2012-03-28 2012-03-28 電解銅箔製箔用電解液及び電解銅箔
EP12819841.3A EP2660359A4 (en) 2011-07-29 2012-07-30 ELECTROLYTIC COPPER ALLOY FOIL, PROCESS FOR THE PRODUCTION THEREOF, ELECTROLYTE SOLUTION USED FOR THE PRODUCTION THEREOF, NEGATIVE ELECTRODE COLLECTOR FOR SECONDARY BATTERIES THEREWITH, SECONDARY BATTERY AND ELECTRODE OF A SECONDARY BATTERY
PCT/JP2012/069368 WO2013018773A1 (ja) 2011-07-29 2012-07-30 電解銅合金箔、その製造方法、それの製造に用いる電解液、それを用いた二次電池用負極集電体、二次電池及びその電極
TW101127554A TWI496954B (zh) 2011-07-29 2012-07-30 An electrolytic copper alloy foil manufacturing method, an electrolytic solution for the production of the alloy foil, a negative electrode current collector for a secondary battery, a secondary battery and an electrode
KR1020137006252A KR101669087B1 (ko) 2011-07-29 2012-07-30 전해 동합금박, 그 제조 방법, 그것의 제조에 이용하는 전해액, 그것을 이용한 2차 전지용 음극 집전체, 2차 전지 및 그 전극
KR1020157022124A KR20150097821A (ko) 2011-07-29 2012-07-30 전해 동합금박, 그 제조 방법, 그것의 제조에 이용하는 전해액, 그것을 이용한 2차 전지용 음극 집전체, 2차 전지 및 그 전극
CN201280004436.7A CN103348041B (zh) 2011-07-29 2012-07-30 电解铜合金箔、其制备方法、制备中所用的电解液、使用该电解铜合金箔的二次电池用负极集电体、二次电池及其电极
US13/965,291 US9890463B2 (en) 2011-07-29 2013-08-13 Electrolysis copper-alloy foil, method of the same, electrolytic-solution using the production, negative electrode aggregation used the same, secondary battery, and electrode of the same

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP2012074173A JP2013204088A (ja) 2012-03-28 2012-03-28 電解銅箔製箔用電解液及び電解銅箔

Publications (2)

Publication Number Publication Date
JP2013204088A JP2013204088A (ja) 2013-10-07
JP2013204088A5 true JP2013204088A5 (cg-RX-API-DMAC7.html) 2014-02-06

Family

ID=49523517

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2012074173A Withdrawn JP2013204088A (ja) 2011-07-29 2012-03-28 電解銅箔製箔用電解液及び電解銅箔

Country Status (1)

Country Link
JP (1) JP2013204088A (cg-RX-API-DMAC7.html)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2014115681A1 (ja) * 2013-01-24 2014-07-31 古河電気工業株式会社 電解銅箔とその製造方法
JP2014101581A (ja) * 2013-12-25 2014-06-05 Furukawa Electric Co Ltd:The 電解銅合金箔、その製造方法、その製造に用いる電解液、二次電池用負極集電体、二次電池及びその電極
TWI926549B (zh) * 2024-12-17 2026-05-21 南亞塑膠工業股份有限公司 電解銅箔、其製造方法以及集流體

Similar Documents

Publication Publication Date Title
Qiu et al. Using corrosion to fabricate various nanoporous metal structures
WO2009057688A1 (ja) 電解銅箔及びその電解銅箔の製造方法
EP2759516A3 (en) Composite protective layer for photoelectrode structure, photoelectrode structure including the composite protective layer, and photoelectrochemical cell including photoelectrode structure
WO2012175301A3 (de) Chemisch behandelte stromableiterfolie aus aluminium oder einer aluminiumlegierung
MY162358A (en) Surface-treated copper foil
JP2012117142A5 (cg-RX-API-DMAC7.html)
JP2013030472A5 (ja) 蓄電装置
PH12013500969A1 (en) Electrolytic copper foil
EA201690315A1 (ru) Электродные узлы с малым сопротивлением для производства металлов
JP2016521442A5 (cg-RX-API-DMAC7.html)
GB201307692D0 (en) Acid and Alkali Resistant Nickel-Chromium-Molybdenum-Copper Alloys
TW201612997A (en) Method for permanent connection of two metal surfaces
MY174169A (en) Electro-deposited copper foil and surface-treated copper foil manufactured by using the electro-deposited copper foil
JP2012183583A5 (cg-RX-API-DMAC7.html)
BR112014013648A2 (pt) mancal deslizante
WO2013117588A3 (en) A thin film for a lead for brain applications
IN2014CN03533A (cg-RX-API-DMAC7.html)
GB201317934D0 (en) Electrolytic exfoliation of graphite
PH12017500512B1 (en) Electrode for electrochlorination processes and method of manufacturing thereof
PL2971260T3 (pl) Elektrolityczne wytwarzanie jonów manganu (iii) w mocnym kwasie siarkowym
WO2012024382A3 (en) Organic acid- or latent organic acid-functionalized polymer-coated metal powders for solder pastes
MX348141B (es) Dispositivo y metodo para recubrimiento electrolitico de objeto.
ITMI20110825A1 (it) Elemento accessorio per abbellimento
EP2670887A1 (en) Adhesion promoting composition for metal leadframes
WO2011052987A3 (ko) 식각액 조성물