JP2013185239A5 - - Google Patents

Download PDF

Info

Publication number
JP2013185239A5
JP2013185239A5 JP2012053410A JP2012053410A JP2013185239A5 JP 2013185239 A5 JP2013185239 A5 JP 2013185239A5 JP 2012053410 A JP2012053410 A JP 2012053410A JP 2012053410 A JP2012053410 A JP 2012053410A JP 2013185239 A5 JP2013185239 A5 JP 2013185239A5
Authority
JP
Japan
Prior art keywords
ceramic film
alloy
film
ceramic
molten aluminum
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2012053410A
Other languages
English (en)
Japanese (ja)
Other versions
JP2013185239A (ja
JP5931516B2 (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2012053410A priority Critical patent/JP5931516B2/ja
Priority claimed from JP2012053410A external-priority patent/JP5931516B2/ja
Priority to CN201310073959.3A priority patent/CN103305826B/zh
Publication of JP2013185239A publication Critical patent/JP2013185239A/ja
Publication of JP2013185239A5 publication Critical patent/JP2013185239A5/ja
Application granted granted Critical
Publication of JP5931516B2 publication Critical patent/JP5931516B2/ja
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Links

JP2012053410A 2012-03-09 2012-03-09 アルミニウム溶湯接触部材の製造方法 Expired - Fee Related JP5931516B2 (ja)

Priority Applications (2)

Application Number Priority Date Filing Date Title
JP2012053410A JP5931516B2 (ja) 2012-03-09 2012-03-09 アルミニウム溶湯接触部材の製造方法
CN201310073959.3A CN103305826B (zh) 2012-03-09 2013-03-08 接触铝金属熔液的构件和其制造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP2012053410A JP5931516B2 (ja) 2012-03-09 2012-03-09 アルミニウム溶湯接触部材の製造方法

Publications (3)

Publication Number Publication Date
JP2013185239A JP2013185239A (ja) 2013-09-19
JP2013185239A5 true JP2013185239A5 (zh) 2015-01-29
JP5931516B2 JP5931516B2 (ja) 2016-06-08

Family

ID=49131535

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2012053410A Expired - Fee Related JP5931516B2 (ja) 2012-03-09 2012-03-09 アルミニウム溶湯接触部材の製造方法

Country Status (2)

Country Link
JP (1) JP5931516B2 (zh)
CN (1) CN103305826B (zh)

Family Cites Families (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CH621952A5 (zh) * 1977-09-01 1981-03-13 Bbc Brown Boveri & Cie
JPH1034311A (ja) * 1996-07-26 1998-02-10 Hitachi Metals Ltd 溶融金属用部材及びその製造方法
ATE235036T1 (de) * 1999-04-16 2003-04-15 Moltech Invent Sa Schutzbeschichtung für komponenten, die durch erosion während des frischens von geschmolzenen metallen angegriffen werden
JP4409067B2 (ja) * 2000-08-03 2010-02-03 東洋鋼鈑株式会社 溶融金属に対する耐食性に優れた溶融金属用部材およびその製造方法
JP2002146509A (ja) * 2000-11-09 2002-05-22 Asahi Glass Co Ltd 溶融金属用部材およびその製造方法
JP2003166027A (ja) * 2001-11-30 2003-06-13 Toshiba Mach Co Ltd Ni基耐食耐摩耗合金、この合金を用いた複合部材およびダイカストマシン用の部材、並びにこの合金用の原料粉末
JP4354315B2 (ja) * 2004-03-22 2009-10-28 東芝機械株式会社 アルミニウム溶湯接触部材およびその製造方法

Similar Documents

Publication Publication Date Title
JP2006347870A5 (zh)
CN106498355B (zh) 一种高温薄膜传感器用抗氧化复合防护层及其制造方法
WO2019109752A1 (zh) 一种钨铼热电偶高温抗氧化涂层及其应用
WO2010053687A3 (en) Thermal spray coatings for semiconductor applications
TWI526412B (zh) 抗腐蝕膜、形成有抗腐蝕層之金屬基材以及其製備方法
TW201236876A (en) Vacuum depositing articles and method for making same
KR101680864B1 (ko) 내식성 금속 산화물층이 도입된 철계 기재의 세라믹 코팅방법
CN105547535B (zh) 用于薄膜压力传感器的应变薄膜及其制备方法、薄膜压力传感器芯体
JPWO2015173843A1 (ja) 溶融めっき金属浴用部材
JP2018003163A (ja) 溶融金属めっき浴用ロール及び溶融金属めっき浴用ロールの製造方法
JP2007175881A (ja) スーパーエンプラ積層膜及び複合による溶射成膜法
JP2011153230A5 (zh)
JP2013185239A5 (zh)
MA48961B1 (fr) Substrat métallique revêtu et procédé de fabrication
JP2004346428A (ja) ケイ素基材とボンド層とを含む物品
TWI544103B (zh) 用於導電薄膜沉積設備之內部構件,及該內部構件製造方法
JP2014012873A5 (zh)
JP2020519763A5 (zh)
WO2008011627A3 (en) Method and device for controlling the results of deposition on substrate surfaces
TWI540219B (zh) The Manufacturing Method and Structure of Corrosion Resistant Film Resistors
Deyuan et al. Zinc-Aluminum Corrosion Resistance and Inactivation Process of NiCr-Cr3C2 Cermet oating
JP2012201893A (ja) 耐食性材料
HE et al. Gas hot-corrosion resistance of nanostructure and segmentation thermal barrier coatings on DZ40M superalloy
JP5876259B2 (ja) 窒化アルミニウム膜によって被覆された部材の製造方法