JP2012256536A - 密閉型電池及びその製造方法 - Google Patents
密閉型電池及びその製造方法 Download PDFInfo
- Publication number
- JP2012256536A JP2012256536A JP2011129306A JP2011129306A JP2012256536A JP 2012256536 A JP2012256536 A JP 2012256536A JP 2011129306 A JP2011129306 A JP 2011129306A JP 2011129306 A JP2011129306 A JP 2011129306A JP 2012256536 A JP2012256536 A JP 2012256536A
- Authority
- JP
- Japan
- Prior art keywords
- thin portion
- thickness
- safety valve
- variation
- thin
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
【解決手段】密閉型電池100は、第1薄肉部151と、第1薄肉部151よりも厚みを薄くした溝状の第2薄肉部152と、を有する金属製の安全弁150を備える。第2薄肉部152には、当該第2薄肉部152を構成する金属を酸化させてなる酸化被膜155bを設けている。
【選択図】図5
Description
これに対し、本発明者は、研究の結果、第2薄肉部の厚みのバラツキ(製造バラツキ)が開弁圧のバラツキに与える影響を小さくすることを可能とした。これにより、開弁圧のバラツキを小さくすることが可能となった。
これに対し、上述の密閉型電池では、安全弁の第2薄肉部に、当該第2薄肉部を構成する金属を酸化させてなる酸化被膜(例えば、陽極酸化被膜)を設けている。これにより、安全弁の第2薄肉部の腐食を抑制することができる。従って、「第2薄肉部の腐食によって安全弁の開弁圧が変化(低下)する」ことを抑制することができる。
本実施形態にかかる密閉型電池100は、図1に示すように、電極体110と、これを収容する電池ケース120とを備える、リチウムイオン二次電池である。この密閉型電池100は、例えば、電気自動車やハイブリット自動車用の駆動電源として用いられる。
まず、正極、負極、及びセパレータを有する電極体を形成する。具体的には、まず、正極活物質(例えば、ニッケル酸リチウム)とアセチレンブラックとPVdF(結着剤)とを混合し、これにNMP(溶媒)を混合して、正極スラリを作製した。次いで、この正極スラリを、アルミニウム箔からなる正極集電部材の両面に塗工し、乾燥させた後、プレス加工を施した。これにより、正極を得た。
その後、負極と正極との間にセパレータを介在させて捲回して、捲回型の電極体110を形成した。
次に、実施形態にかかる安全弁150の開弁圧について調査した。具体的には、安全弁150について、第2薄肉部152の厚み(平均厚みT)と開弁圧の値との関係について調査した。これにより、第2薄肉部152の厚みのバラツキ(製造バラツキ)が安全弁150の開弁圧のバラツキに与える影響の程度を調査した。
具体的には、圧縮機に連結されたノズル20と安全弁150の第1薄肉部151の裏面151cの周囲との間に、シールゴム10を圧縮状態で介在させて、ノズル20と安全弁150との間を気密にする。この状態で、圧縮機からノズル20を通じて圧縮空気を流して、0.01MPa/sの速度で安全弁150を加圧していった。そして、安全弁150が開弁したときの圧力を、開弁圧として計測した。その結果を図7に示す。
110 電極体
120 電池ケース
130 電池ケース本体
140 封口蓋
150 安全弁
151 第1薄肉部
152 第2薄肉部
155、155b 酸化被膜(陽極酸化被膜)
Claims (5)
- 第1薄肉部と、上記第1薄肉部よりも厚みを薄くした溝状の第2薄肉部と、を有する金属製の安全弁、を備える
密閉型電池において、
上記第2薄肉部に、当該第2薄肉部を構成する金属を酸化させてなる酸化被膜を設けてなる
密閉型電池。 - 請求項1に記載の密閉型電池であって、
前記酸化被膜は、前記第2薄肉部の陽極酸化により形成した陽極酸化被膜である
密閉型電池。 - 請求項1または請求項2に記載の密閉型電池であって、
前記酸化被膜の厚みは、50〜300nmの範囲内である
密閉型電池。 - 第1薄肉部と、上記第1薄肉部よりも厚みを薄くした溝状の第2薄肉部と、を有する金属製の安全弁、を備える
密閉型電池の製造方法において、
上記第2薄肉部の陽極酸化により、上記第2薄肉部に陽極酸化被膜を形成する陽極酸化工程を備える
密閉型電池の製造方法。 - 請求項4に記載の密閉型電池の製造方法であって、
前記陽極酸化工程では、前記陽極酸化被膜の厚みを50〜300nmの範囲内とする
密閉型電池の製造方法。