- Publication number
- JP2010520149A5 JP2010520149A5 JP2009552783A JP2009552783A JP2010520149A5 JP 2010520149 A5 JP2010520149 A5 JP 2010520149A5 JP 2009552783 A JP2009552783 A JP 2009552783A JP 2009552783 A JP2009552783 A JP 2009552783A JP 2010520149 A5 JP2010520149 A5 JP 2010520149A5
- Authority
- JP
- Japan
- Prior art keywords
- oxide
- refractory material
- rare earth
- blend
- protective
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US11/683,260 US8105683B2 (en) | 2007-03-07 | 2007-03-07 | Treated refractory material and methods of making |
| US11/683,260 | 2007-03-07 | ||
| PCT/US2008/053136 WO2008109222A2 (en) | 2007-03-07 | 2008-02-06 | Treated refractory material and methods of making |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2010520149A JP2010520149A (ja) | 2010-06-10 |
| JP2010520149A5 true JP2010520149A5 (enExample) | 2012-03-15 |
| JP5503297B2 JP5503297B2 (ja) | 2014-05-28 |
Family
ID=39387154
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2009552783A Expired - Fee Related JP5503297B2 (ja) | 2007-03-07 | 2008-02-06 | 処理耐火材及び製造方法 |
Country Status (7)
| Country | Link |
|---|---|
| US (1) | US8105683B2 (enExample) |
| EP (1) | EP2121539B1 (enExample) |
| JP (1) | JP5503297B2 (enExample) |
| CN (1) | CN101626995B (enExample) |
| AU (1) | AU2008223302B2 (enExample) |
| CA (1) | CA2679382C (enExample) |
| WO (1) | WO2008109222A2 (enExample) |
Families Citing this family (23)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US20090188347A1 (en) * | 2007-03-07 | 2009-07-30 | General Electric Company | Treated refractory material and methods of making |
| US8481152B2 (en) * | 2008-08-14 | 2013-07-09 | General Electric Company | Refractory material with improved resistance to molten slag |
| US8197566B2 (en) * | 2008-12-08 | 2012-06-12 | General Electric Company | Gasifier additives for improved refractory life |
| US20110033613A1 (en) * | 2009-08-04 | 2011-02-10 | Battelle Memorial Institute | Method and Composition for Protection of Refractory Materials in Aggressive Environments |
| DE102009045698A1 (de) * | 2009-10-14 | 2011-04-21 | Evonik Degussa Gmbh | Verfahren zum Infiltrieren von porösen keramischen Bauteilen |
| DE112011103740A5 (de) | 2010-11-12 | 2013-08-08 | Technische Universität Bergakademie Freiberg | Auskleidungsmaterial für Vergasungsanlagen bestehend aus einem alkalikorrosionsbeständigen und temperaturwechselbeständigen chromoxid- und kohlenstofffreien oxidkeramischen Werkstoff und seine Verwendung |
| FR2974081B1 (fr) | 2011-04-15 | 2016-02-26 | Saint Gobain Ct Recherches | Produit d'oxydes de chrome, de zirconium et d'hafnium |
| DE102011115759B4 (de) * | 2011-10-12 | 2015-10-01 | Thyssenkrupp Industrial Solutions Ag | Keramikkörper, Verfahren zu seiner Herstellung und Verwendung eines Beschichtungsmaterials |
| CN102514293B (zh) * | 2011-11-16 | 2014-09-24 | 中钢集团洛阳耐火材料研究院有限公司 | 一种纳米多孔高效隔热板的制备方法 |
| DE102012003478B4 (de) | 2012-02-21 | 2015-08-06 | Technische Universität Bergakademie Freiberg | Verwendung eines oxidkeramischen Werkstoffes aus CaZrO3 als Auskleidungsmaterial für Vergasungsanlagen |
| JP5747127B2 (ja) * | 2012-06-15 | 2015-07-08 | 株式会社ノリタケカンパニーリミテド | アルミナ多孔質体およびその製造方法 |
| MX2015002365A (es) | 2012-08-21 | 2015-09-24 | Stellar Materials Inc | Composicion refractaria y proceso para formar un articulo con ella. |
| FR2996843B1 (fr) | 2012-10-15 | 2020-01-03 | Saint-Gobain Centre De Recherches Et D'etudes Europeen | Produit d'oxyde de chrome. |
| CN103011817B (zh) * | 2012-12-24 | 2014-06-11 | 中国科学院金属研究所 | 一种钇硅氧多孔高温陶瓷材料的制备方法 |
| CN103496992B (zh) * | 2013-09-22 | 2015-04-01 | 郑州亨瑞达新材料有限公司 | 一种铬锆莫来石耐火材料及其制备方法 |
| DE102016220246A1 (de) * | 2016-10-17 | 2018-04-19 | Siemens Aktiengesellschaft | Keramische Hitzeschilde mit Infiltrationscoating |
| CN106747157A (zh) * | 2016-11-24 | 2017-05-31 | 天津航空机电有限公司 | 一种用于探测器腔体的填充材料 |
| CN110294633B (zh) * | 2018-03-23 | 2021-11-09 | 国家能源投资集团有限责任公司 | 多孔陶瓷以及气化渣制备多孔陶瓷的方法 |
| CN108637231B (zh) * | 2018-07-30 | 2023-09-12 | 广东中天创展球铁有限公司 | 一种球化处理用铁水包及其制作工艺 |
| CN112811448A (zh) * | 2021-01-18 | 2021-05-18 | 朱广东 | 一种氧化镁还原渣的回收工艺 |
| CN114891376B (zh) * | 2022-05-07 | 2023-04-25 | 武汉科技大学 | 基于铬化工渣的高发射率红外辐射涂料、涂层及其制备方法 |
| CN116422339B (zh) * | 2023-03-21 | 2024-09-27 | 榆林学院 | 一种改性气化渣载镍锡催化剂及其在环己醇脱氢中的应用 |
| CN117362015B (zh) * | 2023-10-27 | 2024-04-12 | 河南省瑞泰科实业集团有限公司 | 高纯刚玉砖及其制备方法 |
Family Cites Families (34)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3031340A (en) * | 1957-08-12 | 1962-04-24 | Peter R Girardot | Composite ceramic-metal bodies and methods for the preparation thereof |
| GB1087035A (en) | 1964-11-27 | 1967-10-11 | Shinagawa Fire Brick Co Ltd | A process for the manufacture of refractory brick |
| US3789096A (en) | 1967-06-01 | 1974-01-29 | Kaman Sciences Corp | Method of impregnating porous refractory bodies with inorganic chromium compound |
| US3734767A (en) * | 1970-06-18 | 1973-05-22 | Kaman Sciences Corp | Ceramic treating process and product produced thereby |
| US3888790A (en) * | 1971-11-24 | 1975-06-10 | Du Pont | Process for preparing a catalytically active ceramic coatings |
| US3992161A (en) * | 1973-01-22 | 1976-11-16 | The International Nickel Company, Inc. | Iron-chromium-aluminum alloys with improved high temperature properties |
| GB1569474A (en) * | 1976-03-26 | 1980-06-18 | Centre Rech Metallurgique | Method of the quality of refractory bricks |
| FR2345408A1 (fr) | 1976-03-26 | 1977-10-21 | Centre Rech Metallurgique | Procede pour ameliorer la qualite des briques refractaires |
| JPS6042184B2 (ja) | 1977-10-12 | 1985-09-20 | 東芝セラミツクス株式会社 | 緻密質酸化クロム耐火物の製造方法 |
| JPS6025396B2 (ja) | 1978-12-08 | 1985-06-18 | 日本化学工業株式会社 | 改質セラミツクスの製造法 |
| US4374897A (en) * | 1980-03-04 | 1983-02-22 | Nippon Chemical Industrial Co., Ltd. | Chromium oxide-based sintered bodies and process for production thereof |
| US4568652A (en) | 1984-10-15 | 1986-02-04 | The United States Of America As Represented By The Secretary Of The Interior | Soluble additives to improve high temperature properties of alumina refractories |
| JPS6270258A (ja) | 1985-09-20 | 1987-03-31 | 日本特殊陶業株式会社 | 酸化クロム質焼結体 |
| FR2647437B1 (fr) | 1989-05-26 | 1991-10-04 | Savoie Refractaires | Nouvelles compositions refractaires contenant de la zircone monoclinique et articles formes a partir de ces compositions presentant une resistance mecanique a chaud et une resistance aux chocs thermiques ameliorees |
| JPH03228860A (ja) | 1990-01-31 | 1991-10-09 | Nippon Steel Corp | マグクロ質耐火れんがの製造方法 |
| FR2665434B1 (fr) | 1990-08-03 | 1993-09-24 | Prod Cellulosiques Isolants | Procede pour la fabrication d'un materiau refractaire isolant et materiau ainsi obtenu. |
| JP2951432B2 (ja) | 1991-05-16 | 1999-09-20 | 黒崎窯業株式会社 | マグネシア含有不焼成耐火物 |
| JPH0543306A (ja) | 1991-08-16 | 1993-02-23 | Kurosaki Refract Co Ltd | マグネシア−クロミア質焼成耐火物 |
| DE4140417C1 (enExample) * | 1991-12-07 | 1993-04-29 | Dyko Industriekeramik Gmbh, 4000 Duesseldorf, De | |
| JPH07165461A (ja) | 1993-12-14 | 1995-06-27 | Harima Ceramic Co Ltd | マグネシア−クロム質焼成レンガおよびその製造方法 |
| JPH07291716A (ja) | 1994-04-15 | 1995-11-07 | Nippon Steel Corp | 塩基性耐火物 |
| JPH0859345A (ja) * | 1994-08-25 | 1996-03-05 | Shinagawa Refract Co Ltd | ジルコニア質複合焼結体及びその製造方法。 |
| JPH08245261A (ja) | 1995-03-08 | 1996-09-24 | Okayama Ceramics Gijutsu Shinko Zaidan | 耐アルカリ性クロム系耐火材料及びそれを用いた耐火煉瓦の製造方法 |
| JP3943139B2 (ja) * | 1996-12-10 | 2007-07-11 | シーメンス アクチエンゲゼルシヤフト | 高温ガスに曝される製品ならびにその製造方法 |
| US6200631B1 (en) | 1997-10-27 | 2001-03-13 | Praxair Technology, Inc. | Method for producing corrosion resistant refractories |
| JP2000327406A (ja) | 1999-05-11 | 2000-11-28 | Nippon Steel Corp | 耐スラグ浸潤性に優れたクロミア含有れんがおよび溶融金属容器 |
| JP2002020161A (ja) | 2000-07-03 | 2002-01-23 | Mitsubishi Heavy Ind Ltd | 高耐食性耐火物用バインダー材 |
| JP3723093B2 (ja) | 2001-04-20 | 2005-12-07 | 三菱重工業株式会社 | 高耐食性耐火物材の製造方法 |
| US6815386B1 (en) | 2002-10-23 | 2004-11-09 | Kyei-Sing Kwong | Use of phosphates to reduce slag penetration in Cr2O3-based refractories |
| JP4178239B2 (ja) * | 2003-10-09 | 2008-11-12 | 独立行政法人産業技術総合研究所 | 高密着性酸化物皮膜及びその製造方法 |
| CN1296323C (zh) | 2004-04-30 | 2007-01-24 | 洛阳耐火材料研究院 | 以Cr2O3为基的耐火复合材料 |
| US7666512B2 (en) * | 2004-08-09 | 2010-02-23 | United Technologies Corporation | Thermal resistant environmental barrier coating |
| KR101157047B1 (ko) | 2004-12-24 | 2012-06-21 | 주식회사 포스코 | 마그네시아-크롬질 내화벽돌 및 그 제조방법 |
| FR2883282B1 (fr) | 2005-03-15 | 2007-05-25 | Saint Gobain Ct Recherches | Revetement interne de reacteur de gazeificateur |
-
2007
- 2007-03-07 US US11/683,260 patent/US8105683B2/en not_active Expired - Fee Related
-
2008
- 2008-02-06 CN CN200880007318.5A patent/CN101626995B/zh not_active Expired - Fee Related
- 2008-02-06 EP EP20080729125 patent/EP2121539B1/en active Active
- 2008-02-06 CA CA2679382A patent/CA2679382C/en active Active
- 2008-02-06 AU AU2008223302A patent/AU2008223302B2/en not_active Ceased
- 2008-02-06 WO PCT/US2008/053136 patent/WO2008109222A2/en not_active Ceased
- 2008-02-06 JP JP2009552783A patent/JP5503297B2/ja not_active Expired - Fee Related
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2010520149A5 (enExample) | ||
| JP2022040270A5 (enExample) | ||
| JP5503297B2 (ja) | 処理耐火材及び製造方法 | |
| JP5677977B2 (ja) | シリコンを含有する耐熱性基材用の環境バリア | |
| JP2016515088A5 (enExample) | ||
| US20090188347A1 (en) | Treated refractory material and methods of making | |
| CN105814144B (zh) | 在聚合物凝胶下沉积可磨损涂层的方法 | |
| JP2013515664A5 (enExample) | ||
| EP2138474B1 (en) | Sic material | |
| JP2018530503A (ja) | 高密度耐環境性コーティング組成物 | |
| ATE506332T1 (de) | Keramisches pulver, keramische schicht und schichtsystem mit einer gadolinium-mischkristall- pyrochlorphase und oxiden | |
| CA2711343A1 (en) | Methods of improving surface roughness of an environmental barrier coating and components comprising environmental barrier coatings having improved surface roughness | |
| JP2008169481A5 (enExample) | ||
| JP7319269B2 (ja) | Ebc層及びcmc層を保護するための耐侵食性且つcmas耐性コーティング並びに溶射コーティング方法 | |
| JP2016500046A5 (enExample) | ||
| JP2007167780A5 (enExample) | ||
| ATE472517T1 (de) | Feuerfester kohlenstoffgebundener magnesiastein sowie verfahren zu seiner herstellung | |
| CN102471172A (zh) | 生产用作催化剂床基质的具有增强机械强度的多孔陶瓷的方法 | |
| TW201033155A (en) | Process for producing an aluminum titanate-based fired body | |
| JP2015506265A5 (enExample) | ||
| JP4960453B2 (ja) | 改善されたディーゼル粒子フィルター | |
| WO2012116188A3 (en) | Sintering aids for lanthanide ceramics | |
| JP5162180B2 (ja) | 焼結成形体、その製造方法及びその使用 | |
| WO2013146594A1 (ja) | セラミックフィルタ | |
| RU2463279C1 (ru) | ЗАЩИТНОЕ СТЕКЛОКРИСТАЛЛИЧЕСКОЕ ПОКРЫТИЕ ДЛЯ SiC-СОДЕРЖАЩИХ МАТЕРИАЛОВ И СПОСОБ ЕГО ПОЛУЧЕНИЯ |