JP2006221817A - 捲回形鉛蓄電池 - Google Patents
捲回形鉛蓄電池 Download PDFInfo
- Publication number
- JP2006221817A JP2006221817A JP2005031199A JP2005031199A JP2006221817A JP 2006221817 A JP2006221817 A JP 2006221817A JP 2005031199 A JP2005031199 A JP 2005031199A JP 2005031199 A JP2005031199 A JP 2005031199A JP 2006221817 A JP2006221817 A JP 2006221817A
- Authority
- JP
- Japan
- Prior art keywords
- electrode plate
- wound
- paste
- slit
- hole
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
【解決手段】正極板と負極板およびセパレータを渦巻き状に捲回した捲回型鉛蓄電池において、正極板および負極板はそれぞれ集電のためのペースト未塗布部1を異方向に有し、前記ペースト未塗布部に少なくとも1つの穴を有することを特徴とする。前記穴の形状は捲回軸方向のスリット4であり、該スリットの開口部が前記ペースト未塗布部の上端縁に到らないことを特徴とする。
【選択図】図4
Description
(比較例)
負極は、鉛粉と鉛粉に対して13重量%の希硫酸(比重1.26:20℃)と、鉛粉に対して12重量%の水とを混練して負極活物質ペーストを作製する。これを長さ900mm、幅110mm、厚さ0.2mmの鉛又は鉛合金箔からなる集電体に100g(片面50g)塗布した。図1に示すように塗布幅は90mmで塗布後の厚さは0.5mmとなるように調整した。このように極板はペーストが塗布されている部分(ペースト塗布部2)とペーストが塗布されてない端部(ペースト未塗布部1)を有している。
(実施例1)
図3にペースト未塗布部1を加工し穴3を開けた極板を示す。穴3の中心は未塗布部の水平方向の中心線に沿うようにし、直径7mm、ピッチ60mmで等間隔に配置した。その後の工程は比較例と同じにして実施例1の電池を得た。
(実施例2)
図4にペースト未塗布部1を加工し、開口部が前記未塗布部の上端縁に到らないようなスリット4を開けた極板を示す。スリット4は上端部に至らないので、これは前記穴3の1つの形態となる。スリット4は高さ10mm、幅2mmで下端がペースト塗布部2にかかるようにピッチ31mmで等間隔に配置した。その後の工程は比較例と同じにして実施例2の電池を得た。
2 ペースト塗布部
3 穴
4 スリット
5 捲回群
6 ストラップ
Claims (2)
- 正極板と負極板およびセパレータから成り、正極板および負極板はそれぞれ集電のためのペースト未塗布部を異方向に有し、正極板と負極板およびセパレータを渦巻き状に捲回したものであって、前記ペースト未塗布部に少なくとも1つの穴を有することを特徴とする捲回形鉛蓄電池。
- 前記穴の形状は捲回軸方向のスリットであり、該スリットの開口部が前記未塗布部の上端縁に到らないことを特徴とする請求項1記載の捲回形鉛蓄電池。