JP2004520683A5 - - Google Patents

Download PDF

Info

Publication number
JP2004520683A5
JP2004520683A5 JP2002541736A JP2002541736A JP2004520683A5 JP 2004520683 A5 JP2004520683 A5 JP 2004520683A5 JP 2002541736 A JP2002541736 A JP 2002541736A JP 2002541736 A JP2002541736 A JP 2002541736A JP 2004520683 A5 JP2004520683 A5 JP 2004520683A5
Authority
JP
Japan
Prior art keywords
electrode composition
battery
zinc
hydroxide
concentration
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2002541736A
Other languages
English (en)
Japanese (ja)
Other versions
JP4605988B2 (ja
JP2004520683A (ja
Filing date
Publication date
Priority claimed from CA002325308A external-priority patent/CA2325308A1/en
Application filed filed Critical
Publication of JP2004520683A publication Critical patent/JP2004520683A/ja
Publication of JP2004520683A5 publication Critical patent/JP2004520683A5/ja
Application granted granted Critical
Publication of JP4605988B2 publication Critical patent/JP4605988B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

JP2002541736A 2000-11-10 2001-11-07 酸化還元電位が亜鉛電位に対して負である添加剤を有する低毒性亜鉛電極のための陰極の配合 Expired - Lifetime JP4605988B2 (ja)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
CA002325308A CA2325308A1 (en) 2000-11-10 2000-11-10 Negative electrode formulation for a low toxicity zinc electrode having additives with redox potentials negative to zinc potential
PCT/CA2001/001581 WO2002039520A2 (en) 2000-11-10 2001-11-07 Negative electrode formulation for a low toxicity zinc electrode having additives with redox potentials negative to zinc potential

Publications (3)

Publication Number Publication Date
JP2004520683A JP2004520683A (ja) 2004-07-08
JP2004520683A5 true JP2004520683A5 (enExample) 2005-12-22
JP4605988B2 JP4605988B2 (ja) 2011-01-05

Family

ID=4167578

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2002541736A Expired - Lifetime JP4605988B2 (ja) 2000-11-10 2001-11-07 酸化還元電位が亜鉛電位に対して負である添加剤を有する低毒性亜鉛電極のための陰極の配合

Country Status (8)

Country Link
US (2) US6797433B2 (enExample)
EP (1) EP1340273B1 (enExample)
JP (1) JP4605988B2 (enExample)
AT (1) ATE431623T1 (enExample)
AU (1) AU2002218079A1 (enExample)
CA (1) CA2325308A1 (enExample)
DE (1) DE60138727D1 (enExample)
WO (1) WO2002039520A2 (enExample)

Families Citing this family (23)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CA2325791A1 (en) * 2000-11-10 2002-05-10 Jeffrey Phillips Negative electrode formulation for a low toxicity zinc electrode having additives with redox potentials positive to zinc potential
CA2377065A1 (en) 2001-03-15 2002-09-15 Powergenix Systems Inc. Alkaline cells having low toxicity rechargeable zinc electrodes
US7550230B2 (en) * 2001-03-15 2009-06-23 Powergenix Systems, Inc. Electrolyte composition for nickel-zinc batteries
US6849360B2 (en) 2002-06-05 2005-02-01 Eveready Battery Company, Inc. Nonaqueous electrochemical cell with improved energy density
US20080166632A1 (en) * 2003-08-18 2008-07-10 Powergenix, Inc. Method of manufacturing nickel zinc batteries
CN101577347B (zh) * 2003-08-18 2012-05-30 鲍尔热尼系统公司 制造镍锌电池的方法
US8703330B2 (en) * 2005-04-26 2014-04-22 Powergenix Systems, Inc. Nickel zinc battery design
US7931988B2 (en) 2007-10-05 2011-04-26 Powergenix Systems, Inc. Tin and tin-zinc plated substrates to improve Ni-Zn cell performance
EP2272124B1 (en) 2008-04-02 2016-03-23 PowerGenix Systems, Inc. Cylindrical nickel-zinc cell with negative can
US8501351B2 (en) * 2009-05-18 2013-08-06 Powergenix Systems, Inc. Pasted zinc electrode for rechargeable nickel-zinc batteries
EP3432389B1 (en) 2009-08-07 2022-11-30 ZincFive Power, Inc. Carbon zinc negative electrode
EP2476156B1 (en) 2009-09-08 2017-04-05 Powergenix Systems, Inc. Selective heat sealing of separators for nickel zinc cells
JP2013507752A (ja) 2009-10-13 2013-03-04 パワージェニックス・システムズ・インコーポレーテッド 陽性の缶を有する円筒形ニッケル─亜鉛セル
EP2750225A4 (en) 2011-08-23 2015-07-29 Nippon Catalytic Chem Ind NEGATIVE ELECTRODE MIXTURE OR GEL ELECTROLYTE AND BATTERY WITH THIS NEGATIVE ELECTRODE MIXTURE OR THIS GEL ELECTROLYTE
WO2013119422A1 (en) 2012-02-07 2013-08-15 Powergenix Systems, Inc. Nickel-zinc rechargeable pencil battery
WO2014037851A2 (de) * 2012-09-07 2014-03-13 Basf Se Wiederaufladbare elektrochemische zink-sauerstoff-zellen
US9337683B2 (en) 2012-12-20 2016-05-10 Powergenix Systems, Inc. Controlling battery states of charge in systems having separate power sources
KR102036952B1 (ko) 2012-12-20 2019-10-25 징크파이브 파워, 인크. 별도의 전력원을 가진 시스템에서 배터리 충전 상태를 제어하는 방법
WO2014150890A1 (en) 2013-03-15 2014-09-25 Hyperion Catalysis International, Inc. Methods of making nanofiber electrodes for batteries
CN110364660B (zh) * 2018-04-10 2022-07-15 浙江浙能中科储能科技有限公司 一种水系锌离子电池复合隔膜及制备方法
CN111463500B (zh) * 2020-03-18 2021-06-22 山东合泰新能源有限公司 一种用于锌阳极碱性二次电池的电解液的制备方法
CN114267827A (zh) * 2020-09-16 2022-04-01 松山湖材料实验室 一种锌电极及其制备方法、二次电池
JP7600946B2 (ja) * 2021-09-29 2024-12-17 トヨタ自動車株式会社 負極活物質層およびアルカリ蓄電池

Family Cites Families (14)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5629345B2 (enExample) * 1972-02-29 1981-07-08
JPS49119127A (enExample) * 1973-03-20 1974-11-14
US3870564A (en) 1973-03-30 1975-03-11 Tokyo Shibaura Electric Co Alkaline cell
JPS5461B2 (enExample) * 1973-11-21 1979-01-05
CS167146B1 (enExample) * 1974-05-21 1976-04-29
JPS5626108B2 (enExample) * 1975-01-20 1981-06-16
US4304828A (en) * 1980-06-27 1981-12-08 Energy Research Corporation Zinc electrode
JPS60167264A (ja) 1984-02-10 1985-08-30 Sanyo Electric Co Ltd アルカリ亜鉛蓄電池
US5168018A (en) 1990-05-17 1992-12-01 Matsushita Electric Industrial Co., Ltd. Method of manufacturing zinc-alkaline batteries
US5215836A (en) 1991-07-18 1993-06-01 Electrochimica Corporation Alkaline galvanic cells
JP2918446B2 (ja) 1994-04-27 1999-07-12 富士電気化学株式会社 電池の負極亜鉛缶
US5556720A (en) * 1994-08-18 1996-09-17 Energy Research Corporation Sealed zinc secondary battery and zinc electrode therefor
JP3370486B2 (ja) 1995-07-21 2003-01-27 松下電器産業株式会社 アルカリ電池
US6261720B1 (en) 1996-09-20 2001-07-17 Matsushita Electric Industrial Co., Ltd. Positive electrode active material for alkaline storage batteries

Similar Documents

Publication Publication Date Title
JP2004520683A5 (enExample)
WO2002039520A3 (en) Negative electrode formulation for a low toxicity zinc electrode having additives with redox potentials negative to zinc potential
US7550231B2 (en) Tin-zinc secondary battery
JP4388276B2 (ja) 酸化還元電位が亜鉛電位に対して正である添加剤を有する低毒性亜鉛電極のための陰極の配合
EP1309022A3 (en) Positive electrode active material and non-aqueous electrolyte secondary battery containing the same
JP2007214125A5 (enExample)
JP2004513501A (ja) アルカリ電解液を有する亜鉛含有セルのための正負相互作用電極調合物
US5532085A (en) Additives for alkaline electrochemical cells having manganese dioxide cathodes
EP2323213A1 (en) Lead-zinc battery
US20130045415A1 (en) Lead-zinc battery
EA200201086A1 (ru) Электрохимический элемент с керамическими частицами в слое электролита
US20020192547A1 (en) Alkaline cells having positive nickel hydroxide electrodes with fluoride salt additives
US9147912B2 (en) Method of producing an electrical potential
JP2004522256A (ja) アルカリ電解液を有する充電式セルのための亜鉛負極調合物
JP2005183116A5 (enExample)
US4306005A (en) Alkaline primary cell with cathode of potassium permanganate with lithium hydroxide
JP2008547184A5 (enExample)
KR20050054870A (ko) 전지용 정극활 물질 및 그 제조 방법 그리고 그것을사용한 전지
US7033700B2 (en) Formulation of zinc negative electrode for rechargeable cells having an alkaline electrolyte
US8932753B2 (en) Lead alkaline battery
JP5279349B2 (ja) 蓄電池
CA1133578A (en) Aluminum additive for cells using divalent silver oxide electrodes
JPH01132054A (ja) 溶融炭酸塩型燃料電池用空気極電極材料
JPH0992279A (ja) アルカリ蓄電池
WO2022246590A1 (zh) 水系金属离子二次电池及水系电解液