JP2002358952A - 非水電解質電池及びその製造方法、並びに正極の評価方法 - Google Patents
非水電解質電池及びその製造方法、並びに正極の評価方法Info
- Publication number
- JP2002358952A JP2002358952A JP2001163125A JP2001163125A JP2002358952A JP 2002358952 A JP2002358952 A JP 2002358952A JP 2001163125 A JP2001163125 A JP 2001163125A JP 2001163125 A JP2001163125 A JP 2001163125A JP 2002358952 A JP2002358952 A JP 2002358952A
- Authority
- JP
- Japan
- Prior art keywords
- positive electrode
- less
- particulate metal
- ppm
- particulate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Secondary Cells (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2001163125A JP2002358952A (ja) | 2001-05-30 | 2001-05-30 | 非水電解質電池及びその製造方法、並びに正極の評価方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2001163125A JP2002358952A (ja) | 2001-05-30 | 2001-05-30 | 非水電解質電池及びその製造方法、並びに正極の評価方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JP2002358952A true JP2002358952A (ja) | 2002-12-13 |
| JP2002358952A5 JP2002358952A5 (enExample) | 2005-04-07 |
Family
ID=19006152
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2001163125A Pending JP2002358952A (ja) | 2001-05-30 | 2001-05-30 | 非水電解質電池及びその製造方法、並びに正極の評価方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP2002358952A (enExample) |
Cited By (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2005183142A (ja) * | 2003-12-18 | 2005-07-07 | Mitsubishi Chemicals Corp | リチウム二次電池用電極材料の異物の検出方法 |
| JP2010033786A (ja) * | 2008-07-25 | 2010-02-12 | Mitsui Mining & Smelting Co Ltd | リチウム二次電池用正極活物質の評価方法及び製造方法 |
| WO2011122663A1 (ja) * | 2010-03-30 | 2011-10-06 | 三井金属鉱業株式会社 | リチウムイオン電池用正極活物質材料及びリチウムイオン電池 |
| CN102217121A (zh) * | 2008-09-18 | 2011-10-12 | 日本瑞翁株式会社 | 二次电池电极用粘合剂组合物及其制造方法 |
| US8470056B2 (en) | 2007-01-24 | 2013-06-25 | Panasonic Corporation | Non-aqueous electrolyte secondary battery and method for producing the same |
| CN109314229A (zh) * | 2016-06-07 | 2019-02-05 | 住友金属矿山株式会社 | 锂化合物、该锂化合物的制造方法以及非水系电解质二次电池用正极活性物质的制造方法 |
-
2001
- 2001-05-30 JP JP2001163125A patent/JP2002358952A/ja active Pending
Cited By (14)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2005183142A (ja) * | 2003-12-18 | 2005-07-07 | Mitsubishi Chemicals Corp | リチウム二次電池用電極材料の異物の検出方法 |
| US8470056B2 (en) | 2007-01-24 | 2013-06-25 | Panasonic Corporation | Non-aqueous electrolyte secondary battery and method for producing the same |
| JP2010033786A (ja) * | 2008-07-25 | 2010-02-12 | Mitsui Mining & Smelting Co Ltd | リチウム二次電池用正極活物質の評価方法及び製造方法 |
| CN102217121A (zh) * | 2008-09-18 | 2011-10-12 | 日本瑞翁株式会社 | 二次电池电极用粘合剂组合物及其制造方法 |
| GB2491535A (en) * | 2010-03-30 | 2012-12-05 | Mitsui Mining & Smelting Co | Positive electrode active material for lithium-ion battery and lithium-ion battery |
| JP2013041840A (ja) * | 2010-03-30 | 2013-02-28 | Mitsui Mining & Smelting Co Ltd | リチウムイオン電池用正極活物質材料及びリチウムイオン電池 |
| WO2011122663A1 (ja) * | 2010-03-30 | 2011-10-06 | 三井金属鉱業株式会社 | リチウムイオン電池用正極活物質材料及びリチウムイオン電池 |
| GB2491535B (en) * | 2010-03-30 | 2013-07-03 | Mitsui Mining & Smelting Co | Positive electrode active material for lithium-ion battery and lithium-ion battery |
| JPWO2011122663A1 (ja) * | 2010-03-30 | 2013-07-08 | 三井金属鉱業株式会社 | リチウムイオン電池用正極活物質材料及びリチウムイオン電池 |
| KR101325165B1 (ko) | 2010-03-30 | 2013-11-07 | 미쓰이 긴조꾸 고교 가부시키가이샤 | 리튬 이온 전지용 양극 활물질 재료 및 리튬 이온 전지 |
| US8728343B2 (en) | 2010-03-30 | 2014-05-20 | Mitsui Mining & Smelting Co., Ltd. | Positive electrode active material for lithium-ion battery and lithium-ion battery |
| CN109314229A (zh) * | 2016-06-07 | 2019-02-05 | 住友金属矿山株式会社 | 锂化合物、该锂化合物的制造方法以及非水系电解质二次电池用正极活性物质的制造方法 |
| US11056688B2 (en) * | 2016-06-07 | 2021-07-06 | Sumitomo Metal Mining Co., Ltd. | Lithium compound, method for producing the lithium compound, and method for producing positive active material for nonaqueous electrolyte secondary battery |
| CN109314229B (zh) * | 2016-06-07 | 2022-03-01 | 住友金属矿山株式会社 | 锂化合物、该锂化合物的制造方法以及非水系电解质二次电池用正极活性物质的制造方法 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR101009625B1 (ko) | 리튬 이차 전지용 음극 재료 및 이를 포함하는 리튬 이차전지 | |
| US10707539B2 (en) | Battery | |
| EP2197069A1 (en) | Rechargeable battery with nonaqueous electrolyte and process for producing the rechargeable battery | |
| US10326129B2 (en) | Active material, electrode, nonaqueous electrolyte secondary battery, battery pack and production method of active material | |
| CN101485034B (zh) | 锂二次电池 | |
| EP3731314B1 (en) | Positive electrode active material and lithium ion battery | |
| JP3492173B2 (ja) | 非水系電池 | |
| JP4882220B2 (ja) | 二次電池 | |
| EP2330662A1 (en) | Nonaqueous electrolyte secondary battery and method for manufacturing the same | |
| JP2949705B2 (ja) | 非水電解液二次電池の放電容量回復方法とそのための回路 | |
| JP3642487B2 (ja) | 二次電池およびそれに用いる電解質 | |
| EP2323201A1 (en) | Nonaqueous electrolyte secondary battery and method for manufacturing the same | |
| JP2001006730A (ja) | 非水電解質電池 | |
| US6686087B2 (en) | Non-aqueous electrolyte secondary cell with a spirally wound electrode unit | |
| JP2002358952A (ja) | 非水電解質電池及びその製造方法、並びに正極の評価方法 | |
| JP4798420B2 (ja) | 二次電池 | |
| JP5109349B2 (ja) | 二次電池 | |
| JP6090743B2 (ja) | 電気化学セル用負極の選別方法、及び、電気化学セルの製造方法 | |
| JP5141940B2 (ja) | 二次電池 | |
| JP2004342459A (ja) | 非水電解質電池 | |
| JP4333103B2 (ja) | 非水電解質電池及びその製造方法 | |
| JP2000251893A (ja) | 非水電解液二次電池、負極材料の製造方法、黒鉛材料評価装置、および黒鉛材料製造装置 | |
| JP4952968B2 (ja) | 二次電池用負極および二次電池 | |
| JP2006114425A (ja) | 非水電解質電池及びその製造方法、並びに正極の評価方法 | |
| EP3780166A1 (en) | Electrode, non-aqueous electrolyte battery, and battery pack |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| A521 | Written amendment |
Free format text: JAPANESE INTERMEDIATE CODE: A523 Effective date: 20040428 |
|
| A621 | Written request for application examination |
Free format text: JAPANESE INTERMEDIATE CODE: A621 Effective date: 20040428 |
|
| A977 | Report on retrieval |
Free format text: JAPANESE INTERMEDIATE CODE: A971007 Effective date: 20050120 |
|
| A131 | Notification of reasons for refusal |
Free format text: JAPANESE INTERMEDIATE CODE: A131 Effective date: 20050125 |
|
| A521 | Written amendment |
Free format text: JAPANESE INTERMEDIATE CODE: A523 Effective date: 20050328 |
|
| A02 | Decision of refusal |
Free format text: JAPANESE INTERMEDIATE CODE: A02 Effective date: 20050419 |
|
| A521 | Written amendment |
Free format text: JAPANESE INTERMEDIATE CODE: A523 Effective date: 20050616 |
|
| A911 | Transfer of reconsideration by examiner before appeal (zenchi) |
Free format text: JAPANESE INTERMEDIATE CODE: A911 Effective date: 20050715 |
|
| A912 | Removal of reconsideration by examiner before appeal (zenchi) |
Free format text: JAPANESE INTERMEDIATE CODE: A912 Effective date: 20050826 |