JP2000136325A - 錆止め塗料及び錆止め下地塗料 - Google Patents

錆止め塗料及び錆止め下地塗料

Info

Publication number
JP2000136325A
JP2000136325A JP10349292A JP34929298A JP2000136325A JP 2000136325 A JP2000136325 A JP 2000136325A JP 10349292 A JP10349292 A JP 10349292A JP 34929298 A JP34929298 A JP 34929298A JP 2000136325 A JP2000136325 A JP 2000136325A
Authority
JP
Japan
Prior art keywords
rust
coating material
inhibiting
surfacer
water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP10349292A
Other languages
English (en)
Inventor
Takuo Shiga
拓夫 志賀
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to JP10349292A priority Critical patent/JP2000136325A/ja
Publication of JP2000136325A publication Critical patent/JP2000136325A/ja
Pending legal-status Critical Current

Abstract

(57)【要約】 茶カテキン類などタンニン類(ポリフェノール類)を含
ませる事を特徴とする、錆止め及び錆防止塗料並びに下
地塗料 【目的】現在市販されている錆防止塗料が鉄内部の錆に
は働かず、表面のマスキング、固定を主としている為に
経時再び発錆を見る事が有り、その改善を計った

Description

【発明の詳細な説明】 [産業上の利用分野]建築用の鉄材を始め、日常生活に
鉄製品、鉄部材の利用は多い。しかし当初鉄材に焼き付
け塗装したりプラスチック・コーティングしていても、
湿気の多い日本では経時どうしても錆が出て品質、使用
上の問題が出る事が多い。この問題の解決は広範にわた
り、産業上の貢献は大きい。
[従来の技術及び発明が解決しようとする課題]従来の
錆止め又は錆防止塗料は錆表面を樹脂分などで密着コー
ティングする事により空気を遮断し錆を止める機能のも
のが多く、これらは錆そのものが鉄材に入り込み錆が浮
き上がるのを防げず、経時再び錆が浮き、生ずるのを防
げない。
[課題を解決する為の手段]発明者は先にタンニン酸類
(ポリフェノール類)が鉄錆と常温で反応し、水に不溶
性の錯体を作る事を見出だし「給水配管壁の鉄錆による
赤水の防止剤」を出願している(特願平9−32191
5)。錆の生成した鉄材の錆の深部までタンニン酸類が
浸透し錯化、固定し表面の錆のみならず、鉄材内部の錆
も固定し、その拡散を止める事により、長期に錆止め、
防止の効果が持続する。
[実施例]実施例1.市販の塗料に茶カテキン抽出物を
重量で0.2%相当量を、水性の場合は水に溶かして、
非水性の場合はアルコールに溶かして加え、よく混ぜて
から通常の様に錆部に塗布固化させる。又、始めて塗料
を塗る場合に、このカテキン処理塗料を使えば錆の発生
が長く防止される。
実施例2.エチルアルコール10g、茶カテキン抽出物
をカテキン量として0.1g、ポリビニル・アルコール
0.05g、水5gを含む塗料下地液を作る。これを通
常の塗料を塗る前に錆部分又は全体に塗布し24時間放
置した後、通常の塗料を塗る時、長期間にわたり錆の発
生を見ない。
実施例3.市販の塗料にタンニン酸5%を含むエチルア
ルコール液を1%相当量混合良く掻き混ぜる。これを錆
を有する鉄部に塗布する時、長期間にわたり錆の増殖、
発生を見ない。

Claims (1)

    【特許請求の範囲】
  1. 【請求項1】塗料又は下地塗料にタンニン類(ポリフェ
    ノール類)を配合する事を特徴とする錆止め、錆防止効
    果を有する塗料
JP10349292A 1998-11-02 1998-11-02 錆止め塗料及び錆止め下地塗料 Pending JP2000136325A (ja)