ID26600A - Metoda dari pengelasan pipa - Google Patents
Metoda dari pengelasan pipaInfo
- Publication number
- ID26600A ID26600A IDP20000627D ID20000627D ID26600A ID 26600 A ID26600 A ID 26600A ID P20000627 D IDP20000627 D ID P20000627D ID 20000627 D ID20000627 D ID 20000627D ID 26600 A ID26600 A ID 26600A
- Authority
- ID
- Indonesia
- Prior art keywords
- weight
- welding
- phosphorous
- sulfur
- maintaining
- Prior art date
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K9/00—Arc welding or cutting
- B23K9/02—Seam welding; Backing means; Inserts
- B23K9/028—Seam welding; Backing means; Inserts for curved planar seams
- B23K9/0282—Seam welding; Backing means; Inserts for curved planar seams for welding tube sections
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K9/00—Arc welding or cutting
- B23K9/12—Automatic feeding or moving of electrodes or work for spot or seam welding or cutting
- B23K9/133—Means for feeding electrodes, e.g. drums, rolls, motors
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K35/00—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting
- B23K35/22—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting characterised by the composition or nature of the material
- B23K35/24—Selection of soldering or welding materials proper
- B23K35/30—Selection of soldering or welding materials proper with the principal constituent melting at less than 1550 degrees C
- B23K35/3053—Fe as the principal constituent
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K9/00—Arc welding or cutting
- B23K9/10—Other electric circuits therefor; Protective circuits; Remote controls
- B23K9/1006—Power supply
- B23K9/1043—Power supply characterised by the electric circuit
- B23K9/1056—Power supply characterised by the electric circuit by using digital means
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K2101/00—Articles made by soldering, welding or cutting
- B23K2101/04—Tubular or hollow articles
- B23K2101/06—Tubes
Landscapes
- Engineering & Computer Science (AREA)
- Mechanical Engineering (AREA)
- Physics & Mathematics (AREA)
- Plasma & Fusion (AREA)
- Arc Welding In General (AREA)
- Butt Welding And Welding Of Specific Article (AREA)
- Heat Treatment Of Articles (AREA)
- Arc Welding Control (AREA)
- Metal Extraction Processes (AREA)
- Rigid Pipes And Flexible Pipes (AREA)
- Nonmetallic Welding Materials (AREA)
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US09/359,377 US6093906A (en) | 1999-07-23 | 1999-07-23 | Method of pipe welding |
Publications (1)
Publication Number | Publication Date |
---|---|
ID26600A true ID26600A (id) | 2001-01-25 |
Family
ID=23413551
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
IDP20000627D ID26600A (id) | 1999-07-23 | 2000-07-24 | Metoda dari pengelasan pipa |
Country Status (17)
Country | Link |
---|---|
US (2) | US6093906A (id) |
EP (1) | EP1070564B1 (id) |
JP (1) | JP3459396B2 (id) |
KR (1) | KR100378309B1 (id) |
CN (1) | CN1177664C (id) |
AT (1) | ATE348682T1 (id) |
AU (1) | AU736892B2 (id) |
BR (1) | BR0003107A (id) |
CA (1) | CA2314058C (id) |
DE (1) | DE60032416T2 (id) |
DZ (1) | DZ3057A1 (id) |
ES (1) | ES2278563T3 (id) |
ID (1) | ID26600A (id) |
MY (1) | MY133493A (id) |
RU (1) | RU2193478C2 (id) |
SG (1) | SG78417A1 (id) |
TW (1) | TW458843B (id) |
Families Citing this family (42)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US6093906A (en) * | 1999-07-23 | 2000-07-25 | Lincoln Global, Inc. | Method of pipe welding |
CA2427073A1 (en) * | 2000-10-27 | 2002-05-02 | Milliken & Company | Thermal textile |
US6649870B1 (en) * | 2001-08-31 | 2003-11-18 | Lincoln Global, Inc. | System and method facilitating fillet weld performance |
US6942139B2 (en) * | 2003-04-29 | 2005-09-13 | Lincoln Global, Inc. | Robotic cylinder welding |
US6974931B2 (en) * | 2003-05-07 | 2005-12-13 | Illinois Tool Works Inc. | Method and apparatus for pulse and short circuit arc welding |
US7053334B2 (en) * | 2004-03-01 | 2006-05-30 | Lincoln Global, Inc. | Electric arc welder system with waveform profile control |
US7842903B2 (en) | 2005-10-31 | 2010-11-30 | Lincoln Global, Inc. | Short arc welding system |
US20070221643A1 (en) * | 2004-04-29 | 2007-09-27 | Lincoln Global, Inc. | Gas-less process and system for girth welding in high strength applications including liquefied natural gas storage tanks |
US7166817B2 (en) * | 2004-04-29 | 2007-01-23 | Lincoln Global, Inc. | Electric ARC welder system with waveform profile control for cored electrodes |
US8704135B2 (en) * | 2006-01-20 | 2014-04-22 | Lincoln Global, Inc. | Synergistic welding system |
US8759715B2 (en) * | 2004-10-06 | 2014-06-24 | Lincoln Global, Inc. | Method of AC welding with cored electrode |
US9333580B2 (en) * | 2004-04-29 | 2016-05-10 | Lincoln Global, Inc. | Gas-less process and system for girth welding in high strength applications |
US7304269B2 (en) * | 2004-06-04 | 2007-12-04 | Lincoln Global, Inc. | Pulse welder and method of using same |
US9393635B2 (en) | 2004-06-04 | 2016-07-19 | Lincoln Global, Inc. | Adaptive GMAW short circuit frequency control and high deposition arc welding |
US8203099B2 (en) * | 2004-06-04 | 2012-06-19 | Lincoln Global, Inc. | Method and device to build-up, clad, or hard-face with minimal admixture |
US7495193B2 (en) * | 2005-03-15 | 2009-02-24 | Lincoln Global, Inc. | Pipe seam tack welding methods and apparatus using modified series arc welding |
US20060231540A1 (en) * | 2005-04-19 | 2006-10-19 | Lincoln Global, Inc. | Method and apparatus for short-circuit welding |
US8975558B2 (en) * | 2005-04-27 | 2015-03-10 | Lincoln Global, Inc. | Selector device for electric arc welder |
US7989732B2 (en) * | 2005-06-15 | 2011-08-02 | Lincoln Global, Inc. | Method of AC welding using a flux cored electrode |
US7304268B2 (en) * | 2006-02-16 | 2007-12-04 | Lincoln Global, Inc. | Method for rating stick electrodes for pipe welding |
US7397015B2 (en) | 2006-04-13 | 2008-07-08 | Lincoln Global, Inc. | Metal cored electrode for open root pass welding |
CN100450688C (zh) * | 2007-07-04 | 2009-01-14 | 中国石油天然气集团公司 | 薄壁不锈钢复层与碳钢基层的复合管环焊缝焊接方法 |
US20090045172A1 (en) * | 2007-08-13 | 2009-02-19 | Lincoln Global, Inc. | Method of open root welding |
US20090261073A1 (en) * | 2008-04-22 | 2009-10-22 | Lincoln Global, Inc. | System and methods of using variable waveform ac arc welding to achieve specific weld metal chemistries |
US9085041B2 (en) | 2009-01-13 | 2015-07-21 | Lincoln Global, Inc. | Method and system to start and use combination filler wire feed and high intensity energy source for welding |
US10086461B2 (en) * | 2009-01-13 | 2018-10-02 | Lincoln Global, Inc. | Method and system to start and use combination filler wire feed and high intensity energy source for welding |
US9403233B2 (en) | 2011-12-16 | 2016-08-02 | Illinois Tool Works Inc. | DC electrode negative rotating arc welding method and system |
JP5787798B2 (ja) * | 2012-03-09 | 2015-09-30 | 株式会社神戸製鋼所 | ソリッドワイヤおよびこれを用いたガスシールドアーク溶接方法 |
US9511442B2 (en) | 2012-07-27 | 2016-12-06 | Illinois Tool Works Inc. | Adaptable rotating arc welding method and system |
US9527152B2 (en) * | 2012-07-30 | 2016-12-27 | Illinois Tool Works Inc. | Root pass welding solution |
US10543551B2 (en) | 2013-09-16 | 2020-01-28 | Illinois Tool Works Inc. | Synchronized rotating arc welding method and system |
US10953484B2 (en) | 2013-09-16 | 2021-03-23 | Illinois Tool Works Inc. | Narrow groove welding method and system |
US10464168B2 (en) | 2014-01-24 | 2019-11-05 | Lincoln Global, Inc. | Method and system for additive manufacturing using high energy source and hot-wire |
WO2015147684A1 (ru) | 2014-03-28 | 2015-10-01 | Открытое акционерное общество "Акционерная компания по транспорту нефти "ТРАНСНЕФТЬ" | Способ сварки трубопроводов из высокопрочных труб с контролируемым тепловложением |
CN104858555A (zh) * | 2015-06-10 | 2015-08-26 | 江苏力沛电力工程技术服务有限公司 | 压力管道焊接工艺 |
JP6795290B2 (ja) | 2015-07-31 | 2020-12-02 | 株式会社神戸製鋼所 | ガスシールドアーク溶接方法 |
US10179369B2 (en) | 2015-10-27 | 2019-01-15 | Lincoln Global, Inc. | Welding system for AC welding with reduced spatter |
US10086462B2 (en) * | 2016-06-27 | 2018-10-02 | Caterpillar Inc. | Hardfacing with low carbon steel electrode |
US11027362B2 (en) | 2017-12-19 | 2021-06-08 | Lincoln Global, Inc. | Systems and methods providing location feedback for additive manufacturing |
CN110773903A (zh) * | 2018-07-30 | 2020-02-11 | 宝山钢铁股份有限公司 | 适合超低热输入自动焊接的co2气体保护焊丝及其制造方法 |
CN110773902A (zh) * | 2018-07-30 | 2020-02-11 | 宝山钢铁股份有限公司 | 适合超低热输入自动焊接的经济型co2气体保护焊丝及制造方法 |
CN110948136A (zh) * | 2018-09-27 | 2020-04-03 | 宝山钢铁股份有限公司 | 适合超低热输入自动焊接的超低碳气体保护焊丝及其制造方法 |
Family Cites Families (10)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US3179781A (en) * | 1961-04-18 | 1965-04-20 | Union Carbide Canada Ltd | Pipe welding machine and process |
US3802874A (en) * | 1971-10-01 | 1974-04-09 | Union Carbide Corp | Consumable welding wire |
US4087674A (en) * | 1974-08-26 | 1978-05-02 | Nippon Steel Corporation | Steel wire for gas shielded welding |
JPS59215297A (ja) * | 1983-05-20 | 1984-12-05 | Mitsubishi Heavy Ind Ltd | 溶接棒 |
US5676857A (en) * | 1995-08-11 | 1997-10-14 | Sabre International, Inc. | Method of welding the end of a first pipe to the end of a second pipe |
JPH09239583A (ja) * | 1996-03-04 | 1997-09-16 | Nippon Steel Weld Prod & Eng Co Ltd | 連続溶接性に優れたパルスアーク溶接用鋼ワイヤ |
US5742029A (en) * | 1996-07-15 | 1998-04-21 | The Lincoln Electric Company | Method of welding wallpaper alloy an arc welder modified to practice same |
US5945014A (en) * | 1998-01-05 | 1999-08-31 | Lincoln Global, Inc. | Method of arc welding heavy steel plates |
US5961863A (en) * | 1998-01-09 | 1999-10-05 | Lincoln Global, Inc. | Short circuit pipe welding |
US6093906A (en) * | 1999-07-23 | 2000-07-25 | Lincoln Global, Inc. | Method of pipe welding |
-
1999
- 1999-07-23 US US09/359,377 patent/US6093906A/en not_active Expired - Lifetime
-
2000
- 2000-05-10 US US09/567,906 patent/US6204478B1/en not_active Expired - Lifetime
- 2000-07-18 EP EP00115437A patent/EP1070564B1/en not_active Expired - Lifetime
- 2000-07-18 ES ES00115437T patent/ES2278563T3/es not_active Expired - Lifetime
- 2000-07-18 RU RU2000118898/02A patent/RU2193478C2/ru not_active IP Right Cessation
- 2000-07-18 SG SG200004046A patent/SG78417A1/en unknown
- 2000-07-18 DE DE60032416T patent/DE60032416T2/de not_active Expired - Lifetime
- 2000-07-18 CA CA002314058A patent/CA2314058C/en not_active Expired - Fee Related
- 2000-07-18 AT AT00115437T patent/ATE348682T1/de not_active IP Right Cessation
- 2000-07-19 AU AU48696/00A patent/AU736892B2/en not_active Ceased
- 2000-07-21 TW TW089114580A patent/TW458843B/zh not_active IP Right Cessation
- 2000-07-21 MY MYPI20003341 patent/MY133493A/en unknown
- 2000-07-21 CN CNB001214349A patent/CN1177664C/zh not_active Expired - Fee Related
- 2000-07-22 KR KR10-2000-0042110A patent/KR100378309B1/ko not_active IP Right Cessation
- 2000-07-23 DZ DZ000123A patent/DZ3057A1/xx active
- 2000-07-24 JP JP2000221697A patent/JP3459396B2/ja not_active Expired - Fee Related
- 2000-07-24 ID IDP20000627D patent/ID26600A/id unknown
- 2000-07-24 BR BR0003107-0A patent/BR0003107A/pt not_active IP Right Cessation
Also Published As
Publication number | Publication date |
---|---|
DE60032416T2 (de) | 2007-10-11 |
JP2001058265A (ja) | 2001-03-06 |
DE60032416D1 (de) | 2007-02-01 |
ES2278563T3 (es) | 2007-08-16 |
EP1070564A2 (en) | 2001-01-24 |
US6093906A (en) | 2000-07-25 |
ATE348682T1 (de) | 2007-01-15 |
CN1281766A (zh) | 2001-01-31 |
EP1070564B1 (en) | 2006-12-20 |
BR0003107A (pt) | 2001-03-13 |
DZ3057A1 (fr) | 2005-05-02 |
RU2193478C2 (ru) | 2002-11-27 |
CN1177664C (zh) | 2004-12-01 |
CA2314058A1 (en) | 2001-01-23 |
JP3459396B2 (ja) | 2003-10-20 |
SG78417A1 (en) | 2001-02-20 |
AU4869600A (en) | 2001-02-15 |
EP1070564A3 (en) | 2002-03-20 |
TW458843B (en) | 2001-10-11 |
KR100378309B1 (ko) | 2003-03-29 |
CA2314058C (en) | 2004-09-28 |
KR20010015407A (ko) | 2001-02-26 |
AU736892B2 (en) | 2001-08-02 |
MY133493A (en) | 2007-11-30 |
US6204478B1 (en) | 2001-03-20 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
ID26600A (id) | Metoda dari pengelasan pipa | |
WO2009022213A3 (en) | Method of open root welding | |
TW200635691A (en) | Modified flux system in cored electrode | |
MX2007004576A (es) | Metodos para extender la vida de las juntas soldadas de aleacion de acero mediante la eliminacion y reduccion del haz. | |
MX370950B (es) | Sistemas y metodos para electrodos de soldadura. | |
FR2865152B1 (fr) | Procede de soudage hybride arc-laser des aciers ferritiques | |
MX339100B (es) | Metodo de soldeo hibrido con arco electrico/laser para partes de acero aluminizado utilizando elementos gammagenos y un gas que contiene mendo del 10% de nitrogeno u oxigeno. | |
PL1775060T3 (pl) | Drut rdzeniowy bezżużlowy do spawania w pozycji pionowej z góry na dół | |
MX361051B (es) | Sistemas y métodos para electrodos de soldadura. | |
ATE476274T1 (de) | Al-mg-mn-füllmetalllegierung zum schweissen | |
NO995859L (no) | Nikkelbasert legering, sveiseelektrode fremstilt av en nikkelbasert legering og fremgangsmÕte for sveising | |
DE60140361D1 (de) | Schweissverfahren, metallzusammensetzung und daraus hergestellter gegenstand | |
EP1281785A3 (fr) | Acier inoxydable austénique pour déformation à froid pouvant être suivi d'un usinage | |
WO2008138304A3 (de) | Verfahren und vorrichtung zum hybridschweissen mit nachfolgendem mag-schweissen | |
WO2004113007A3 (en) | Filler composition for high yield strength base metals | |
PL1778432T3 (pl) | Spawalniczy bezzużlowy drut rdzeniowy z dużą zawartością krzemu do spawania stali ferrytowych | |
NO344915B1 (no) | Flukskjerntetråd for gass-skjermet lysbuesveisising av stål med høy strekkstyrke. | |
WO2005051587A8 (en) | Welding stud | |
GB2434217A (en) | Cables | |
TW564197B (en) | Method for joining metal and metal and joined product | |
CN103252594A (zh) | 一种适用于x70ms/x65ms钢级的耐h2s腐蚀管线钢焊接用焊丝 | |
DE602008003827D1 (de) | Geschweisste kabel- und halteranordnung | |
WO2006111660A3 (fr) | Procede de soudage de canalisations metalliques du type pipeline avec variation d ' une variable electrique relative a l ' arc au cours du mouvement oscillant transverse de la torche dans le joint etroit ; dispositif de mise en oeuvre d ' un tel procede | |
IN2014KN00981A (en) | An overhead electric power cable | |
SE0102901D0 (sv) | Welding of a wearing piece to a metal work piece |