DE834267C - Verfahren zum Reifen von Alkalicellulose - Google Patents
Verfahren zum Reifen von AlkalicelluloseInfo
- Publication number
- DE834267C DE834267C DE1949P0035370 DEP0035370D DE834267C DE 834267 C DE834267 C DE 834267C DE 1949P0035370 DE1949P0035370 DE 1949P0035370 DE P0035370 D DEP0035370 D DE P0035370D DE 834267 C DE834267 C DE 834267C
- Authority
- DE
- Germany
- Prior art keywords
- ripening
- alkali cellulose
- cellulose
- alkali
- frequencies
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Verfahren zum Reifen von Alkalicellulose Der Reifeprozeß von Alkalicellulose wurde in der viscoseverarbeitenden Industrie bisher so durchgeführt, daR die alkalisierte Cellulose auf Transportbändern, in Bunkerwagen oder großen Bunkern auf die Dauer von etwa 20 bis 30 Stunden Temperaturen zwischen 20 und' 300 ausgesetzt wurde. Man hat sich seit langem bemüht, den Abbauvorgang vor allem durch Erhöhung der Temperatur zu beschleunigen.
- Dabei ergeben sich wesentliche Schwierigkeiten dadurch, daß infolge des schlechten Wärmeüberganges eine gleichmäßige Temperierung der Alkalicellulose, die für einen homogenen Abbau unbedingt notwendig ist, nur in intensiv wirkenden Mischaggregaten vorgenommen werden kann, die bei Produktion von z. B. 60 t Viscosefasern ganz erhebliche Ausmaße haben müssen. Auch ein Schnellabbau durch die Einwirkung von Oxydationsmitteln in der Tauchlauge hat sich bis jetzt als wirtschaftlich nicht tragbar erwiesen.
- Aus diesem Grunde sind alle Versuche, eine Schnellreife von Alkalicellulose in größerem Maßstab durchzuführen, gescheitert.
- Gemäß der vorliegenden Erfindung zeigt es sich nun, daß in einfacher Weise und ohne irgendwie beachtlichen Apparaturaufwand ein außerordentlich schneller und absolut homogener Abbau der Cellulose erreicht wird, wenn man die alkalisierte Celltilose z. B. auf einem endlosen Band und in jeder beliebigen Schütthöhe durch ein hochfrequentes Feld schickt, dessen Frequenzen vorzugsweise unter 70 MHz liegen. Die Einwirkungszeit des Feldes kann dabei außerordentlich gering bemessen sein, z. B. wenige Sekunden. Die Frequenz des Feldes richtet sich nach dem Abbaugrad, welcher auf diese Weise genau eingestellt werden kann.
Claims (1)
- PATENTANSPnUCH Verfahren zum Reifen von Alkalicellulose, diadurch gekennzeichnet, daß diese in beliebiger Schütthöhe durch ein hochfrequentes Feld geführt wird, dessen Frequenlzen vorzugsweise unter 70 IHz liegen.