DE721683C - Elektrode fuer elektrische Widerstandspunkt- oder Nahtschweissung - Google Patents

Elektrode fuer elektrische Widerstandspunkt- oder Nahtschweissung

Info

Publication number
DE721683C
DE721683C DEB178761D DEB0178761D DE721683C DE 721683 C DE721683 C DE 721683C DE B178761 D DEB178761 D DE B178761D DE B0178761 D DEB0178761 D DE B0178761D DE 721683 C DE721683 C DE 721683C
Authority
DE
Germany
Prior art keywords
electrode
electrical resistance
copper
seam welding
chromium
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
DEB178761D
Other languages
English (en)
Inventor
Dipl-Ing Heinrich Choulant
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to DEB178761D priority Critical patent/DE721683C/de
Application granted granted Critical
Publication of DE721683C publication Critical patent/DE721683C/de
Expired legal-status Critical Current

Description

  • Elektrode für elektrische Widerstandspunkt- oder Nahtschweißung Das bisher gewöhnlich für die Elektroden von elektrischen Widerstandspunkt- und Nahtschweißmaschinen verwendete Handelskupfer oder Elektrolytkupfer hat den Nachteil, daß seine Härte nur gering ist und daher beim Schweißen leicht eine Verformung der Elektrode an ihrer Auflagefläche auf dem Schweißgut auftritt. Ferner neigen die Elektroden selbst bei Wasserkühlung, insbesondere beim Schweißen von Leichtmetallen zum Anlegieren an das Schweißgut. Die Elektrode kann dabei so stark anlegieren, daß das Schweißgut an ihr hängenbleibt.
  • Die vorliegende Erfindung betrifft eine Elektrode für elektrische Widerstandspunkt-oder Nahtschweißung, die sich dadurch auszeichnet, daß sie ganz oder an der Auflagefläche aus einer Legierung von wenigstens 94% Kupfer und der Rest Chrom und Titan besteht, die nach dem Schmelzen in kalt verformtem Zustande einige, vorzugsweise 2 bis 6 Stunden bei einer Temperatur zwischen 40o bis 6oo° C, vorzugsweise 5oo° C, angelassen und alsdann z. B. in Wasser abgeschreckt ist. Aus der auf diesem Wege hergestellten Legierung wird die Elektrode dann in der gewünschten Form herausgearbeitet. Die Elektrode wird vorzugsweise aus einer vergütbaren Legierung aus 98,7% Kupfer, 1 % Chrom und 0,3% Titan hergestellt. Die Kupfer-Chrom-Titan-Elektrode zeigte eine elektrische Leitfähigkeit von über 50m/Ohm/mm' -und eine Härte von 93 bis 100kg/mm2. An Stelle von Titan kann dabei Zirkon treten. So wurde ferner eine Elektrode aus einer Legierung von 98,8% Kupfer, i% Chrom und o,2% Zirkon hergestellt. Für die Kupfer-Chrom-Zirkon-Elektrode wurde eine elektrische Leitfähigkeit von 52m/Ohm/mm2 und eine Härte von 93 kg/mm2 gemessen. Das
    Dieses neue Elektrodenmaterial hat sick:-( infolge seiner guten elektrischen Leitfähigkeit und Härte und einer geringeren Neigung zur Legierungsbildung sowohl für Eisenschweißung als auch besonders für die Leichtmetallschweißung bewährt.

Claims (4)

  1. PATENTANSPRÜCHE: i. Elektrode für elektrische Widerstandspunkt- oder Nahtschweißung, dadurch gekennzeichnet, daß sie ganz oder an der Auflagefläche aus einer Legierung von mindestens 940;`o Kupfer und der Rest aus Chrom und Titan besteht, die nach dem Schmelzen in kalt verformtem Zustande einige, vorzugsweise 2 bis 6 Stunden bei einer Temperatur zwischen 400 bis 6oo° C, vorzugsweise 5oo° C, angelassen und danach in Wasser abgeschreckt ist. '
  2. 2. Elektrode nach Anspruch i, dadurch gekennzeichnet, daß an Stelle von Titan Zirkon tritt.
  3. 3. Elektrode nach Anspruch i, dadurch gekennzeichnet, daß der Gehalt an Kupfer 98g0'0, an Chrom 1% und Titan 0,39 beträgt.
  4. 4. Elektrode nach Anspruch 2, gekennzeichnet durch einen Gehalt an 98,80,o Kupfer, 1% Chrom und o,20;'o Zirkon.
DEB178761D 1937-06-11 1937-06-11 Elektrode fuer elektrische Widerstandspunkt- oder Nahtschweissung Expired DE721683C (de)