DE528807C - Verfahren zum Dichten von Zementmoertel, Beton o. dgl. - Google Patents
Verfahren zum Dichten von Zementmoertel, Beton o. dgl.Info
- Publication number
- DE528807C DE528807C DEM112468D DEM0112468D DE528807C DE 528807 C DE528807 C DE 528807C DE M112468 D DEM112468 D DE M112468D DE M0112468 D DEM0112468 D DE M0112468D DE 528807 C DE528807 C DE 528807C
- Authority
- DE
- Germany
- Prior art keywords
- concrete
- cement mortar
- cement
- sealing cement
- sealing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Verfahren zum Dichten von Zementmörtel, Beton o. dgl. Bekanntlich wird Zementmörtel oder Beton schon durch kohlensäurehaltige Wasser und ganz schwache Salzlösungen, namentlich solche von Sulfaten, stark angegriffen.
- Man verwendet daher für Bauten, die solchen Wässern ausgesetzt sind, fette Zementmischungen, etwa roo Zement auf Zoo Sand.. Aber auch das reicht nicht aus, und man ergreift meist in solchen Fällen besondere Dichtungsmaßnahmen.
- Man bestreicht dabei entweder die Zementtnauer mit einer Isolierschicht, meist aus Asphalt, oder man setzt dem Zement vor der Verarbeitung bituminöse Stoffe, oft in Verbindung mit Kalkseifen und Tonseifen, zu.
- Es wurde nun gefunden, daß die Aluminiumnaphthenate, dem Zement vor der Verarbeitung in feinster Verteilung zugesetzt, eine ganz hervorragende Wasserdichtigkeit verleihen. Beispiel Mit roo Teilen trockenem Zement werden 2 Teile naphthensaures Aluminium innigst vermischt.
Claims (1)
- hATL:NTANSHIZUCII: Verfahren zum Dichten von Zementmörtel, Beton o. dgl., dadurch gekennzeichnet, daß man dem Zement vor der Verarbeitung Aluminiumnaphthenat zusetzt.