DE396217C - Stromdurchfuehrungsdraht zur luftdichten Einschmelzung in Glas, insbesondere fuer elektrische Gluehlampen u. dgl. - Google Patents
Stromdurchfuehrungsdraht zur luftdichten Einschmelzung in Glas, insbesondere fuer elektrische Gluehlampen u. dgl.Info
- Publication number
- DE396217C DE396217C DEV15592D DEV0015592D DE396217C DE 396217 C DE396217 C DE 396217C DE V15592 D DEV15592 D DE V15592D DE V0015592 D DEV0015592 D DE V0015592D DE 396217 C DE396217 C DE 396217C
- Authority
- DE
- Germany
- Prior art keywords
- wire
- glass
- airtight sealing
- wires
- electric light
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
- 239000011521 glass Substances 0.000 title claims description 6
- 238000007789 sealing Methods 0.000 title claims 2
- 238000002844 melting Methods 0.000 claims description 5
- 230000008018 melting Effects 0.000 claims description 5
- 238000000034 method Methods 0.000 claims description 3
- 230000007547 defect Effects 0.000 claims 1
- 230000000149 penetrating effect Effects 0.000 claims 1
- BASFCYQUMIYNBI-UHFFFAOYSA-N platinum Chemical compound [Pt] BASFCYQUMIYNBI-UHFFFAOYSA-N 0.000 description 7
- RYGMFSIKBFXOCR-UHFFFAOYSA-N Copper Chemical compound [Cu] RYGMFSIKBFXOCR-UHFFFAOYSA-N 0.000 description 4
- 229910052802 copper Inorganic materials 0.000 description 4
- 239000010949 copper Substances 0.000 description 4
- 229910052697 platinum Inorganic materials 0.000 description 3
- 238000004519 manufacturing process Methods 0.000 description 2
- 208000034656 Contusions Diseases 0.000 description 1
- 229910001030 Iron–nickel alloy Inorganic materials 0.000 description 1
- 239000000956 alloy Substances 0.000 description 1
- 229910045601 alloy Inorganic materials 0.000 description 1
- 239000010953 base metal Substances 0.000 description 1
- 239000004020 conductor Substances 0.000 description 1
- 230000035515 penetration Effects 0.000 description 1
- IHQKEDIOMGYHEB-UHFFFAOYSA-M sodium dimethylarsinate Chemical class [Na+].C[As](C)([O-])=O IHQKEDIOMGYHEB-UHFFFAOYSA-M 0.000 description 1
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01J—ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS
- H01J5/00—Details relating to vessels or to leading-in conductors common to two or more basic types of discharge tubes or lamps
- H01J5/46—Leading-in conductors
Landscapes
- Vessels And Coating Films For Discharge Lamps (AREA)
- Joining Of Glass To Other Materials (AREA)
- Ropes Or Cables (AREA)
- Lasers (AREA)
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| HU535238X | 1920-05-26 | ||
| GB12406/21A GB184238A (en) | 1920-05-26 | 1921-04-30 | Improvements in the making of leading-in wires for electric incandescent lamps and for similar purposes |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| DE396217C true DE396217C (de) | 1924-05-28 |
Family
ID=10003997
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| DEV15592D Expired DE396217C (de) | 1920-05-26 | 1920-06-02 | Stromdurchfuehrungsdraht zur luftdichten Einschmelzung in Glas, insbesondere fuer elektrische Gluehlampen u. dgl. |
Country Status (7)
| Country | Link |
|---|---|
| AT (2) | AT95898B (enExample) |
| CH (1) | CH96563A (enExample) |
| DE (1) | DE396217C (enExample) |
| DK (1) | DK32075C (enExample) |
| FR (1) | FR535238A (enExample) |
| GB (1) | GB184238A (enExample) |
| NL (1) | NL10411C (enExample) |
-
1920
- 1920-05-29 AT AT95898D patent/AT95898B/de active
- 1920-06-02 DE DEV15592D patent/DE396217C/de not_active Expired
-
1921
- 1921-04-23 AT AT96431D patent/AT96431B/de active
- 1921-04-28 CH CH96563D patent/CH96563A/de unknown
- 1921-04-30 GB GB12406/21A patent/GB184238A/en not_active Expired
- 1921-05-07 DK DK32075D patent/DK32075C/da active
- 1921-05-09 FR FR535238D patent/FR535238A/fr not_active Expired
- 1921-05-10 NL NL19378A patent/NL10411C/xx active
Also Published As
| Publication number | Publication date |
|---|---|
| AT96431B (de) | 1924-03-26 |
| FR535238A (fr) | 1922-04-11 |
| DK32075C (da) | 1923-08-06 |
| GB184238A (en) | 1922-07-31 |
| AT95898B (de) | 1924-01-25 |
| NL10411C (enExample) | 1924-01-15 |
| CH96563A (de) | 1922-10-16 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| DE19960790A1 (de) | Elektrode zum elektrochemischen Feinbohren von Werkstücken sowie Verfahren zu ihrer Herstellung | |
| DE2158274A1 (de) | Induktionsheizspule zum tiegelfreien zonenschmelzen von staeben aus halbleitermaterial | |
| DE2529004A1 (de) | Gegenstand mit einem glasteil, in den ein metallteil eingeschmolzen ist | |
| DE69409334T2 (de) | Verfahren zur Verbindung einer Molybdän Folie mit einem Teil eines Molybdän Leiters und Herstellungsmethode eines hermetisch eingeschossenen Lampenteils unter Verwendung dieses Verfahrens | |
| EP0098858B1 (de) | Stromeinführungsleitung, insbesondere für vakuumtechnische geräte und verfahren zu deren herstellung | |
| DE1100201B (de) | Verwendung des an sich bekannten Zonenschmelzverfahrens zur Herstellung eines technischen Stoffschlusses | |
| DE19603301C2 (de) | Elektrische Lampe mit Molybdänfoliendurchführungen für ein Lampengefäß aus Quarzglas | |
| DE2348635B1 (de) | Verfahren zur Herstellung eines Grundmaterials für Brillengestelle | |
| DE426536C (de) | Verfahren und Einrichtung zum Compoundieren von Leitern fuer Unterseekabel | |
| DE893974C (de) | Elektrischer Durchfuehrungsisolator | |
| DE202017106956U1 (de) | Elektrodendraht für das Elektro-Erosionsverfahren | |
| DE582249C (de) | Verfahren zur Herstellung nicht durchhaengender schraubenfoermiger Kristalldrahtgluehkoerper fuer elektrische Gluehlampen | |
| CH96563A (de) | Stromdurchführungsdraht zur luftdichten Einschmelzung in Glas, insbesondere für elektrische Glühlampen und dergleichen und Verfahren zur Herstellung desselben. | |
| DE413202C (de) | Stromeinfuehrungsdraht zur luftdichten Einschmelzung in Glas, insbesondere fuer elektrische Gluehlampen u. dgl. | |
| DE1163975C2 (de) | Verfahren zur Verbesserung der elektrischen Eigenschaften von Halbleiteranordnungen | |
| DE414200C (de) | Verfahren zur Herstellung eines gasdichten Verschlusses zwischen einem elektrischen Leiter und dem Gehaeuse eines Quecksilberdampfgleichrichters, einer Kuehlmaschine u. dgl. | |
| DE1927796C3 (de) | Leitungsführung für elektrische Lampen und Verfahren zu ihrer Herstellung | |
| AT153927B (de) | Elektrische Entladungsröhre mit Metallwandung und Verfahren zur Herstellung einer solchen Röhre. | |
| DE911447C (de) | Aus Einzeldraehten bestehende metallische Staebe, z.B. Schweissstaebe, Loetstaebe oder Elektroden, und Verfahren zu ihrem Herstellen | |
| DE542626C (de) | Verfahren zum Aufbringen duenner magnetischer Belastungsschichten auf elektrische Leiter fuer Krarupkabel | |
| DE890102C (de) | Zuendeinrichtung fuer elektrische Entladungsgefaesse | |
| DE935975C (de) | Verfahren zur Herstellung von Kohlegriessmikrofonen | |
| DE946730C (de) | Verfahren zum vakuumdichten Einschmelzen von Stromeinfuehrungen | |
| AT99661B (de) | Verfahren zur Gewinnung von Metallen mit sehr hohem Schmelzpunkt, z. B. Wolfram. | |
| DE2348634B1 (de) | Verfahren zur Herstellung eines Grundmaterials fuer Brillengestelle |