DE368537C - Verfahren zur Entfernung der Oxydschichten von Metallflaechen - Google Patents
Verfahren zur Entfernung der Oxydschichten von MetallflaechenInfo
- Publication number
- DE368537C DE368537C DEW58982D DEW0058982D DE368537C DE 368537 C DE368537 C DE 368537C DE W58982 D DEW58982 D DE W58982D DE W0058982 D DEW0058982 D DE W0058982D DE 368537 C DE368537 C DE 368537C
- Authority
- DE
- Germany
- Prior art keywords
- metal surfaces
- oxide layers
- mixture
- caustic soda
- quick lime
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Verfahren zur Entfernung der Oxydschichten von Metallflächen. Die Gegenstände werden in einem besonders dazu konstruierten Gefäße aus Eisenblech in eine Mischung gebracht, die aus Natronlauge und Ätzkalk besteht, welcher bis zu 2o Prozent Zinkstaub zugesetzt sind. Die Mischung wird entweder durch direkte Heizung oder durch Dampfrohre erhitzt und nun je nach dem Grade der Verschmutzung die Gegenstände bei Messsing, Kupfer usw. eine viertel bis eine halbe Stunde in der Mischung liegen gelassen, sodann mit Wässer abgespült und mit einer weichen Drahtbürste vollkommen gereinigt. Die reduzierte Oxydschicht läßt sich sehr rasch und leicht entfernen, mit ihr auch alle übrigen Verunreinigungen.
- Bei Eisenteilen läßtman in derselben Mischling als Elektrolyt die Reduktion der Oxyde und Oxydule mittels elektrischem Strvm vor sich gehen, wobei nach etwa einer Viertelstunde die Eisenteile durch Drahtbürste oder andere Reini-. gungsvorrichtungen sich leicht säubern lassen. Die Reinigung der Eisenteile geschieht in einem besonders konstruiertem Gefäße.
Claims (1)
- PATENT-ANSPRUG:H: Verfahren zur Entfernung der Oxydschichten von mit Farb-, Lack- oder sonstigen Überzügen versehenen oder oxydierten Metallflächen, dadurch. gekennzeichnet. daB die Metallflächen mit einem erhitzten Gemisch von Natronlauge, Ätzkalk und Zinkstaub behandelt werden.