DE2838022C2 - Verfahren und Vorrichtung zum Elektropolieren von metallischen Oberflächen ausgedehnter Werkstücke - Google Patents
Verfahren und Vorrichtung zum Elektropolieren von metallischen Oberflächen ausgedehnter WerkstückeInfo
- Publication number
- DE2838022C2 DE2838022C2 DE2838022A DE2838022A DE2838022C2 DE 2838022 C2 DE2838022 C2 DE 2838022C2 DE 2838022 A DE2838022 A DE 2838022A DE 2838022 A DE2838022 A DE 2838022A DE 2838022 C2 DE2838022 C2 DE 2838022C2
- Authority
- DE
- Germany
- Prior art keywords
- cathode
- electropolishing
- bath
- polished
- bath tank
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
- 238000000034 method Methods 0.000 title claims description 23
- 238000005498 polishing Methods 0.000 description 14
- 239000007788 liquid Substances 0.000 description 7
- 239000002184 metal Substances 0.000 description 7
- 239000007789 gas Substances 0.000 description 6
- 239000011810 insulating material Substances 0.000 description 5
- 238000007517 polishing process Methods 0.000 description 5
- 239000004020 conductor Substances 0.000 description 4
- 239000000463 material Substances 0.000 description 3
- 230000003746 surface roughness Effects 0.000 description 3
- 241000270728 Alligator Species 0.000 description 2
- 238000007789 sealing Methods 0.000 description 2
- 239000000126 substance Substances 0.000 description 2
- 230000006978 adaptation Effects 0.000 description 1
- 235000013361 beverage Nutrition 0.000 description 1
- 230000015572 biosynthetic process Effects 0.000 description 1
- 238000004140 cleaning Methods 0.000 description 1
- 239000011248 coating agent Substances 0.000 description 1
- 238000000576 coating method Methods 0.000 description 1
- 238000005260 corrosion Methods 0.000 description 1
- 230000007797 corrosion Effects 0.000 description 1
- 230000001419 dependent effect Effects 0.000 description 1
- 230000000694 effects Effects 0.000 description 1
- 239000012530 fluid Substances 0.000 description 1
- 238000002955 isolation Methods 0.000 description 1
- 230000004048 modification Effects 0.000 description 1
- 238000012986 modification Methods 0.000 description 1
- 230000000630 rising effect Effects 0.000 description 1
- 239000000565 sealant Substances 0.000 description 1
- 230000007704 transition Effects 0.000 description 1
- 238000009736 wetting Methods 0.000 description 1
- 239000002023 wood Substances 0.000 description 1
Classifications
-
- C—CHEMISTRY; METALLURGY
- C25—ELECTROLYTIC OR ELECTROPHORETIC PROCESSES; APPARATUS THEREFOR
- C25F—PROCESSES FOR THE ELECTROLYTIC REMOVAL OF MATERIALS FROM OBJECTS; APPARATUS THEREFOR
- C25F7/00—Constructional parts, or assemblies thereof, of cells for electrolytic removal of material from objects; Servicing or operating
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Electrical Discharge Machining, Electrochemical Machining, And Combined Machining (AREA)
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US05/829,668 US4127459A (en) | 1977-09-01 | 1977-09-01 | Method and apparatus for incremental electro-polishing |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| DE2838022A1 DE2838022A1 (de) | 1979-03-15 |
| DE2838022C2 true DE2838022C2 (de) | 1984-11-15 |
Family
ID=25255190
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| DE2838022A Expired DE2838022C2 (de) | 1977-09-01 | 1978-08-31 | Verfahren und Vorrichtung zum Elektropolieren von metallischen Oberflächen ausgedehnter Werkstücke |
Country Status (5)
| Country | Link |
|---|---|
| US (1) | US4127459A (https=) |
| JP (1) | JPS5448644A (https=) |
| BR (1) | BR7805688A (https=) |
| CA (1) | CA1127997A (https=) |
| DE (1) | DE2838022C2 (https=) |
Families Citing this family (18)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4290867A (en) * | 1980-06-30 | 1981-09-22 | Jumer John F | Means for and method of producing smooth electro-polished surfaces |
| US4820390A (en) * | 1987-07-06 | 1989-04-11 | The Interlake Companies, Inc. | Apparatus and method for continuous electrochemical machining of strip material |
| US4941955A (en) * | 1987-07-06 | 1990-07-17 | The Interlake Companies, Inc. | Apparatus and method for electrochemical machining of flat plates or sheets |
| US5217586A (en) * | 1992-01-09 | 1993-06-08 | International Business Machines Corporation | Electrochemical tool for uniform metal removal during electropolishing |
| US5567300A (en) * | 1994-09-02 | 1996-10-22 | Ibm Corporation | Electrochemical metal removal technique for planarization of surfaces |
| JP2000297397A (ja) | 1999-02-10 | 2000-10-24 | Canon Inc | 電析方法 |
| JP2000277478A (ja) * | 1999-03-25 | 2000-10-06 | Canon Inc | 陽極化成装置、陽極化成システム、基板の処理装置及び処理方法、並びに基板の製造方法 |
| US6638863B2 (en) | 2001-04-24 | 2003-10-28 | Acm Research, Inc. | Electropolishing metal layers on wafers having trenches or vias with dummy structures |
| JP4717021B2 (ja) * | 2007-02-05 | 2011-07-06 | シャープ株式会社 | スピーカ装置 |
| US11298251B2 (en) | 2010-11-17 | 2022-04-12 | Abbott Cardiovascular Systems, Inc. | Radiopaque intraluminal stents comprising cobalt-based alloys with primarily single-phase supersaturated tungsten content |
| US9724494B2 (en) | 2011-06-29 | 2017-08-08 | Abbott Cardiovascular Systems, Inc. | Guide wire device including a solderable linear elastic nickel-titanium distal end section and methods of preparation therefor |
| US9145619B2 (en) | 2012-09-14 | 2015-09-29 | Abbott Cardiovascular Systems, Inc. | Electropolishing method including multi-finger contacts |
| US9045843B2 (en) * | 2012-09-14 | 2015-06-02 | Abbott Cardiovascular Systems, Inc. | Electropolishing fixture with lever arm |
| US9133563B2 (en) | 2012-09-14 | 2015-09-15 | Abbott Cardiovascular Systems, Inc. | Electropolishing device and method |
| US9850589B2 (en) * | 2014-05-12 | 2017-12-26 | United Technologies Corporation | System and methods for electrochemical grinding with a screen |
| ITUA20162060A1 (it) * | 2016-03-07 | 2017-09-07 | Condoroil Stainless Srl | Unita' per il trattamento elettrolitico in automatico di tubi in acciaio inossidabile di medio - piccolo diametro |
| CN111465722B (zh) * | 2017-09-28 | 2022-07-12 | 南韩商奥森里德股份有限公司 | 电解研磨用电极框架、电解研磨用可变型电极框架及包括其的电解研磨装置 |
| US12151049B2 (en) | 2019-10-14 | 2024-11-26 | Abbott Cardiovascular Systems, Inc. | Methods for manufacturing radiopaque intraluminal stents comprising cobalt-based alloys with supersaturated tungsten content |
Family Cites Families (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| NL44583C (https=) * | 1934-11-24 | |||
| US2861937A (en) * | 1954-09-15 | 1958-11-25 | John F Jumer | Apparatus for electropolishing interior surfaces of vessels |
| DE1192522B (de) * | 1960-05-17 | 1965-05-06 | Chemische Maschb Werke Veb | Verfahren und Vorrichtung zur Entseuchung radioaktiv verseuchter Gegenstaende und Flaechen |
| US3857764A (en) * | 1971-08-20 | 1974-12-31 | J Jumer | Electrochemical processing of inner surfaces of large vessels |
| US4001094A (en) * | 1974-09-19 | 1977-01-04 | Jumer John F | Method for incremental electro-processing of large areas |
| DE2528942A1 (de) * | 1975-06-28 | 1976-12-30 | Hoechst Ag | Verfahren zum zonenweisen elektropolieren der inneren oberflaeche grossraeumiger behaelter |
-
1977
- 1977-09-01 US US05/829,668 patent/US4127459A/en not_active Expired - Lifetime
-
1978
- 1978-08-18 CA CA309,667A patent/CA1127997A/en not_active Expired
- 1978-08-31 DE DE2838022A patent/DE2838022C2/de not_active Expired
- 1978-08-31 BR BR7805688A patent/BR7805688A/pt unknown
- 1978-09-01 JP JP10742178A patent/JPS5448644A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| BR7805688A (pt) | 1979-05-29 |
| JPS5448644A (en) | 1979-04-17 |
| DE2838022A1 (de) | 1979-03-15 |
| US4127459A (en) | 1978-11-28 |
| CA1127997A (en) | 1982-07-20 |
| JPS6147920B2 (https=) | 1986-10-21 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| DE2838022C2 (de) | Verfahren und Vorrichtung zum Elektropolieren von metallischen Oberflächen ausgedehnter Werkstücke | |
| DE2538584A1 (de) | Verfahren und vorrichtung zum stufenweisen elektrolytischen behandeln einer grossen metallflaeche | |
| DE3001726C2 (de) | Vorrichtung zum Behandeln einer Leiterplatte | |
| DE3323306A1 (de) | Halterung fuer hohlzylindrische koerper | |
| DE2846726C3 (de) | Vorrichtung zum elektrolytischen Ätzen eines Werkstückes aus Aluminium oder einer Aluminiumlegierung | |
| DE1546930B2 (de) | Vorrichtung zum elektrophoretischen ueberziehen von gegenstaenden mit einem organischen filmbildner | |
| DE2051578A1 (de) | Methode des Elektrofassonierens und Mittel des Verfahrens | |
| DE3889187T2 (de) | Unlösliche Elektrode. | |
| DE69413794T2 (de) | Verbesserungen an oder bezugnehmend auf Klammern die Verwendung derselben | |
| DE3246690A1 (de) | Verfahren und vorrichtung fuer die elektrolytische behandlung von metallbahnen | |
| EP0205822B1 (de) | Vorrichtung zur Herstellung von Aufreissdeckeln | |
| DE4106733C2 (https=) | ||
| EP0213137A1 (de) | Haltevorrichtung zum farbigen beschichten von metallbauteilen. | |
| DE3419503C2 (https=) | ||
| DE2519542C3 (de) | Vorrichtung zur Behandlung von stückigen Gegenständen mit einer Flüssigkeit und Verfahren zur Auffüllung der Poren von Gegenständen mit einer Flüssigkeit | |
| DE3202442C2 (de) | Galvanisierapparat zur lokalen galvanischen Behandlung eines Werkstückes | |
| DE3719440C1 (en) | Anode cell for electrophoretic metal-coating baths | |
| DE2618437A1 (de) | Plattenfilterpresse | |
| DE1771953B2 (de) | Vorrichtung zur elektrobeschichtung von hohlkoerpern | |
| DE2811245A1 (de) | Vorrichtung und verfahren zur bearbeitung der innenflaechen grosser behaelter durch elektrische entladungsvorgaenge | |
| DE1954024A1 (de) | Verfahren und Vorrichtung fuer die Oberflaechenbehandlung von Glasgegenstaenden | |
| DE2651359C2 (de) | Elektrolytisches Poliergerät | |
| DE10235117B3 (de) | Anlage zur kataphoretischen Tauchlackierung von Gegenständen | |
| DE2538585A1 (de) | Verfahren und vorrichtung zum polieren der innenflaeche eines laenglichen behaelters | |
| DE3001255A1 (de) | Verfahren und einrichtung zum elektropolieren von tabletten-presswerkzeug |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| 8110 | Request for examination paragraph 44 | ||
| D2 | Grant after examination | ||
| 8364 | No opposition during term of opposition | ||
| 8339 | Ceased/non-payment of the annual fee |