CN204326262U - Sy-k补偿收缩混凝土膨胀加强带 - Google Patents
Sy-k补偿收缩混凝土膨胀加强带 Download PDFInfo
- Publication number
- CN204326262U CN204326262U CN201420801030.8U CN201420801030U CN204326262U CN 204326262 U CN204326262 U CN 204326262U CN 201420801030 U CN201420801030 U CN 201420801030U CN 204326262 U CN204326262 U CN 204326262U
- Authority
- CN
- China
- Prior art keywords
- concrete
- reinforcing band
- expansion reinforcing
- expansive
- band
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型属于混凝土膨胀加强带技术领域,具体涉及一种SY-K补偿收缩混凝土膨胀加强带,其特征在于:它主要由膨胀加强带混凝土和位于该膨胀加强带混凝土两侧的补偿收缩混凝土浇筑而成,所述膨胀加强带混凝土上下侧面处设有带中拉力筋,所述带中拉力筋的两端超出膨胀加强带混凝土左右两端一定长度;所述膨胀加强带混凝土与补偿收缩混凝土的结合面上布置有密孔钢丝网,所述密孔钢丝网的上下两端分别与对应的带中拉力筋固定连接;所述膨胀加强带混凝土和补偿收缩混凝土均为SY-K补偿收缩混凝土,混凝土强度等级相同,其中膨胀加强带混凝土的SY-K膨胀纤维抗裂防水剂掺量高于补偿收缩混凝土。本实用新型结构简单牢固、施工方便、防水效果好。
Description
技术领域
本实用新型属于混凝土膨胀加强带技术领域,具体涉及一种SY-K补偿收缩混凝土膨胀加强带。
技术背景
补偿收缩混凝土是一种常见的混凝土,其应有非常广泛,土建工程中屋面防水、地下防水、基础及楼面、屋面后浇带、机械设备底座灌浆等部位,都可以用到补偿收缩混凝土。其使用的主要目的是主要为减少混凝土干缩裂缝,提高抗裂性和抗渗性,增强混凝土本身和结构构件的耐久性。现有技术中,在超长混凝土结构施工中(超长指超过60m),后浇带的不足尤为明显:(1)一般设计要求后浇带的浇筑时间需待两侧结构混凝土浇筑后2个月,因此在很多工程中这样会影响总工期,(特别是后浇带在地下结构的部位,如筏板基础在底板浇筑后还要回填土,这样会造成非常多的麻烦);(2)后浇带在两侧混凝土浇筑后需要对其进行保护、清理与凿毛,给后期施工无形中增添了一定的工程量;(3)两侧需要预埋止水带,两侧先浇筑,待达到强度后浇筑带内混凝土,因而有两道施工缝,由于有施工缝存在,在地下工程及其他有防水要求的地方,增加了渗漏隐患。
发明内容
本实用新型的目的在于提供一种结构简单牢固、施工方便、防水效果好的SY-K补偿收缩混凝土膨胀加强带。
为实现上述目的,本实用新型所采取的技术方案是:
一种SY-K补偿收缩混凝土膨胀加强带,其特征在于:它主要由膨胀加强带混凝土和位于该膨胀加强带混凝土两侧的补偿收缩混凝土浇筑而成,所述膨胀加强带混凝土上下侧面处设有带中拉力筋,所述带中拉力筋的两端超出膨胀加强带混凝土左右两端一定长度;所述膨胀加强带混凝土与补偿收缩混凝土的结合面上布置有密孔钢丝网,所述密孔钢丝网的上下两端分别与对应的带中拉力筋固定连接;所述膨胀加强带混凝土和补偿收缩混凝土均为SY-K补偿收缩混凝土,混凝土强度等级相同,其中膨胀加强带混凝土的SY-K膨胀纤维抗裂防水剂掺量高于补偿收缩混凝土。
所述膨胀加强带混凝土中的SY-K膨胀纤维抗裂防水剂掺量为10%,补偿收缩混凝土中的SY-K膨胀纤维抗裂防水剂掺量为6%。
所述膨胀加强带混凝土的长度为2m±0.2m。
所述密孔钢丝网的孔网直径为5mm。
本实用新型的有益效果是:本实用新型省去了后浇带设置,加快部分材料周转,省去后浇带、施工缝清理、支模、混凝土浇筑、养护拆模等工序工作,加快施工进度。由于不渗漏,无裂缝起到自防水作用,因此减少粉刷及防水层处理,可节约费用。因此本实用新型结构简单牢固、施工方便、防水效果好。
附图说明
图1是本实用新型的结构示意图。
图中:1-膨胀加强带混凝土、2-补偿收缩混凝土、3-密孔钢丝网、4-带中拉力筋。
具体实施方式
为了更好地理解本实用新型,下面结合实施例和附图对本实用新型的技术方案做进一步的说明(如图1)。
一种SY-K补偿收缩混凝土膨胀加强带,它主要由膨胀加强带混凝土1和位于该膨胀加强带混凝土1两侧的补偿收缩混凝土2浇筑而成,所述膨胀加强带混凝土1上下侧面处设有带中拉力筋4,所述带中拉力筋4的两端(沿膨胀加强带混凝土1长度方向)超出膨胀加强带混凝土1左右两端一定长度(即带中拉力筋4沿膨胀加强带混凝土1长度方向完全覆盖膨胀加强带混凝土1,所述一定长度优指膨胀加强带混凝土1长度的二分之一;所述膨胀加强带混凝土1与补偿收缩混凝土2的上下侧面均有配筋,带中拉力筋4的数量优选为配筋数量的一半);所述膨胀加强带混凝土1与补偿收缩混凝土2的结合面上布置有密孔钢丝网3(即膨胀加强带混凝土1与补偿收缩混凝土2的分界),所述密孔钢丝网3的上下两端分别与对应的带中拉力筋4固定连接;所述膨胀加强带混凝土1和补偿收缩混凝土2均为SY-K补偿收缩混凝土(即指添加有SY-K膨胀纤维抗裂防水剂的混凝土),混凝土强度等级相同,其中膨胀加强带混凝土1的SY-K膨胀纤维抗裂防水剂掺量(掺量指每立方SY-K补偿收缩混凝土中SY-K膨胀纤维抗裂防水剂的含量)高于补偿收缩混凝土2。
所述膨胀加强带混凝土1中的SY-K膨胀纤维抗裂防水剂掺量为10%,补偿收缩混凝土2中的SY-K膨胀纤维抗裂防水剂掺量为6%。
所述膨胀加强带混凝土1的长度为2m±0.2m。
所述密孔钢丝网3的孔网直径为5mm。
超长混凝土结构施工中(超长指超过60m)可用SY-K补偿收缩混凝土膨胀加强带替代后浇带,施工时连续浇筑,实现无缝施工,具体施工步骤如下:
(1)现场混凝土搅拌:搅拌投料顺序:石子→砂→水泥→SY-K膨胀纤维抗裂防水剂→水。投料先干拌0.5~1min再加水,水分三次加入,加水后搅拌1~2min(比普通混凝土搅拌时间延长0.5min)。混凝土搅拌前必须严格按试验室配合比通知单操作,不得擅自修改。水泥、砂、石车过磅,在雨季,砂必须每天测定含水率,调整用水量。现场搅拌坍落度控制6~8cm,泵送商品混凝土坍落度控制14~16cm;
(2)运输:混凝土运输供应保持连续均衡,间隔不应超过1.5h,夏季或运距较远可适当掺入缓凝剂,一般掺入2.5‰~3‰为宜(运输后如出现离析,浇筑前进行二次拌合);
(3)混凝土浇筑:应连续浇筑,宜不留或少留施工缝;
(4)养护:常温(20~25℃)浇筑后6~10h浇水覆盖养护,要保持混凝土表面湿润,养护不少于14天。
以上说明仅为本实用新型的应用实施例而已,当然不能以此来限定本实用新型之权利范围,因此依本实用新型申请专利范围所作的等效变化,仍属本实用新型的保护范围。
Claims (4)
1. 一种SY-K补偿收缩混凝土膨胀加强带,其特征在于:它主要由膨胀加强带混凝土(1)和位于该膨胀加强带混凝土(1)两侧的补偿收缩混凝土(2)浇筑而成,所述膨胀加强带混凝土(1)上下侧面处设有带中拉力筋(4),所述带中拉力筋(4)的两端超出膨胀加强带混凝土(1)左右两端一定长度;所述膨胀加强带混凝土(1)与补偿收缩混凝土(2)的结合面上布置有密孔钢丝网(3),所述密孔钢丝网(3)的上下两端分别与对应的带中拉力筋(4)固定连接;所述膨胀加强带混凝土(1)和补偿收缩混凝土(2)均为SY-K补偿收缩混凝土,混凝土强度等级相同,其中膨胀加强带混凝土(1)的SY-K膨胀纤维抗裂防水剂掺量高于补偿收缩混凝土(2)。
2. 根据权利要求1所述的SY-K补偿收缩混凝土膨胀加强带,其特征在于:所述膨胀加强带混凝土(1)中的SY-K膨胀纤维抗裂防水剂掺量为10%,补偿收缩混凝土(2)中的SY-K膨胀纤维抗裂防水剂掺量为6%。
3. 根据权利要求1所述的SY-K补偿收缩混凝土膨胀加强带,其特征在于:所述膨胀加强带混凝土(1)的长度为2m±0.2m。
4. 根据权利要求1所述的SY-K补偿收缩混凝土膨胀加强带,其特征在于:所述密孔钢丝网(3)的孔网直径为5mm。