CN203356560U - 一种清除连铸坯表面积渣的装置 - Google Patents

一种清除连铸坯表面积渣的装置 Download PDF

Info

Publication number
CN203356560U
CN203356560U CN 201320464984 CN201320464984U CN203356560U CN 203356560 U CN203356560 U CN 203356560U CN 201320464984 CN201320464984 CN 201320464984 CN 201320464984 U CN201320464984 U CN 201320464984U CN 203356560 U CN203356560 U CN 203356560U
Authority
CN
China
Prior art keywords
continuous casting
conveying rollers
red hot
casting billet
accumulated slag
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 201320464984
Other languages
English (en)
Inventor
郭庆华
周文胜
王豫东
于挥
王会海
李世晨
黄旭东
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Xinjiang Bayi Iron and Steel Co Ltd
Original Assignee
Xinjiang Bayi Iron and Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Xinjiang Bayi Iron and Steel Co Ltd filed Critical Xinjiang Bayi Iron and Steel Co Ltd
Priority to CN 201320464984 priority Critical patent/CN203356560U/zh
Application granted granted Critical
Publication of CN203356560U publication Critical patent/CN203356560U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型属于炼钢厂连铸车间板坯连铸生产中,清除连铸坯表面积渣的装置,包括连铸机均布的输送辊和与输送辊相配合的红热铸坯,在均布输送辊之间的红热铸坯上面分别通过支架设置着相对应的吹扫管道,在吹扫管道的出口上设置着金属喷头。本实用新型结构合理,可以在线清除连铸机输送辊道上红热铸坯表面的积渣,改善产品质量,提高设备的使用寿命,减低工人的劳动强度。

Description

一种清除连铸坯表面积渣的装置
技术领域
本实用新型属于炼钢厂连铸车间板坯连铸生产中,清除连铸坯表面积渣的装置。
背景技术
铸坯表面积渣事故对铸坯质量有很大影响,首先,表面积渣影响铸坯外观,还可能划伤铸坯,从而影响铸坯质量;其次,表面积渣过多会产生堆积,可能损坏铸机设备。因此表面积渣是决定铸坯表面质量的一项重要因素。
铸坯发生积渣后,铸坯表面和扇段辊子之间的摩擦力加大,容易导致以下现象发生:
1、    铸坯表面划伤。
2、    扇段积渣严重,导致在积渣处出现因机械擦刮而产生的刨花状铁条,因此对扇段损害极大。
划伤造成铸坯外观质量不合格,严重影响铸坯轧制质量;积渣发生后,需要停机处理,从而影响生产,打断正常的生产节奏。
实用新型内容
本实用新型的目的在于提供一种清除连铸坯表面积渣的装置,其结构合理,可以在线清除连铸机输送辊道上红热铸坯表面的积渣,改善产品质量,提高设备的使用寿命,减低工人的劳动强度。
本实用新型的目的是这样实现的:一种清除连铸坯表面积渣的装置,包括连铸机均布的输送辊和与输送辊相配合的红热铸坯,在均布输送辊之间的红热铸坯上面分别通过支架设置着相对应的吹扫管道,在吹扫管道的出口上设置着金属喷头。
本改进设计是在红热铸坯表面架设高压空气吹扫管道,将积渣从铸坯表面吹走,使渣子在铸坯表面无法停留,可有效防止积渣,以及积渣导致的铸坯表面质量问题。
本实用新型产生的积极效果:
(1)提高连铸作业率。当扇形段发生积渣后,无需停机处理,只需将积渣人工清理,然后将吹扫管道压缩空气气源打开,即可防止积渣。前期出现这种情况连铸只能停机处理,改进后不需要停机处理,作业率提高至83%以上。
(2)消除积渣造成的划伤。极大地改善了产品质量,将划伤造成的废品杜绝为零。
(3)延长了扇形段辊子的使用寿命,改造前积渣问题造成扇形段辊子损坏严重,改进处理方法后扇形段辊子数量更换率减少5%。
(4)降低了工人劳动强度,降低物料消耗。前期出现划伤铸坯,出坯工必须使用火焰清理枪处理铸坯,工人劳动强度大,物料消耗大,目前已被完全杜绝。
本实用新型结构合理,实现了在线清除连铸机输送辊道上红热铸坯表面上的积渣,改善了产品质量,提高了设备的使用寿命,降低了工人的劳动强度。
附图说明
下面将结合附图对本实用新型作进一步的描述,图1为本实用新型的立体结构示意图。
具体实施方式
一种清除连铸坯表面积渣的装置,如图1所示,包括连铸机均布的输送辊1和与输送辊1相配合的红热铸坯2,在均布输送辊1之间的红热铸坯2上面分别通过支架设置着相对应的吹扫管道3,在吹扫管道3的出口上设置着金属喷头4。 

Claims (1)

1.一种清除连铸坯表面积渣的装置,包括连铸机均布的输送辊(1)和与输送辊(1)相配合的红热铸坯(2),其特征是:在均布输送辊(1)之间的红热铸坯(2)上面分别通过支架设置着相对应的吹扫管道(3),在吹扫管道(3)的出口上设置着金属喷头(4)。
CN 201320464984 2013-08-01 2013-08-01 一种清除连铸坯表面积渣的装置 Expired - Fee Related CN203356560U (zh)