CN203221079U - 一种铝合金拉杆的复合热挤压模具结构 - Google Patents
一种铝合金拉杆的复合热挤压模具结构 Download PDFInfo
- Publication number
- CN203221079U CN203221079U CN 201320149667 CN201320149667U CN203221079U CN 203221079 U CN203221079 U CN 203221079U CN 201320149667 CN201320149667 CN 201320149667 CN 201320149667 U CN201320149667 U CN 201320149667U CN 203221079 U CN203221079 U CN 203221079U
- Authority
- CN
- China
- Prior art keywords
- mould
- plate
- die
- lower bolster
- punch
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种铝合金拉杆的复合热挤压模具结构,包括上模板和下模板,其特征在于:所述上模板下方设有上垫板,所述上垫板下方设有凸模固定板,所述凸模固定板内设有凸模,所述凸模为中空结构,所述下模板上方设有下垫板,所述下垫板内设有顶杆,所述顶杆横穿下模板与下垫板底部连接,所述下垫板上方设有凹模预紧圈,所述凹模预紧圈内设有凹模,所述凹模内底部设有顶件器,所述顶件器上方设有制件,所述凸模贯穿凸模固定板插入凹模内,所述制件贯穿凹模与凸模中空部分吻合连接。本实用新型结构简单、能提高材料的利用率、减少成本、提高生产效率。
Description
技术领域
本实用新型涉及一种模具结构,具体涉及一种铝合金拉杆的复合热挤压模具结构。
背景技术
在高压电器零部件的制造中,铝合金材料因其导电导热性好、力学性能优良,而且比强度高、密度小,所以得到广泛采用,传统的拉杆的挤压件采用棒料直接切削加工而成,材料的利用率一般在 16%-40%,浪费严重、效率低,且模具寿命不长。
发明内容
本实用新型所要解决的技术问题在于提供一种结构简单、能提高材料的利用率、减少成本、提高生产效率的铝合金拉杆的复合热挤压模具结构。
本实用新型所要解决的技术问题采用以下技术方案来实现:
一种铝合金拉杆的复合热挤压模具结构,包括上模板和下模板,其特征在于:所述上模板下方设有上垫板,所述上垫板下方设有凸模固定板,所述凸模固定板内设有凸模,所述凸模为中空结构。
所述下模板上方设有下垫板,所述下垫板内设有顶杆,所述顶杆横穿下模板与下垫板底部连接,所述下垫板上方设有凹模预紧圈,所述凹模预紧圈内设有凹模,所述凹模内底部设有顶件器,所述顶件器上方设有制件。
所述凸模贯穿凸模固定板插入凹模内。
所述制件贯穿凹模与凸模中空部分吻合连接。
本实用新型的有益效果是:结构简单、能提高材料的利用率、减少成本、提高生产效率。
附图说明
图1为本实用新型结构示意图。
具体实施方式
为了使本实用新型实现的技术手段、创作特征、达成目的与功效易于明白了解,下面结合具体图示,进一步阐述本实用新型。
如图1所示,一种铝合金拉杆的复合热挤压模具结构,包括上模板1和下模板2,上模板1下方设有上垫板3,上垫板3下方设有凸模固定板4,凸模固定板4内设有凸模5,凸模5为中空结构。
下模板2上方设有下垫板6,下垫板6内设有顶杆7,顶杆7横穿下模板2与下垫板6底部连接,下垫板6上方设有凹模预紧圈8,凹模预紧圈8内设有凹模9,凹模9内底部设有顶件器10,顶件器10上方设有制件11。
凸模5贯穿凸模固定板4插入凹模9内。
制件11贯穿凹模9与凸模5中空部分吻合连接。
本实用新型是这样实施的:挤压时.先将坯料放入凹模型腔内.随着凸模下移,坯料在组合式凹模内正挤成形,同时杆部反挤成形,随着挤压变形力逐渐增大,当金属正向流动到顶件器时,头部成形结束,此时金属反向继续流动,当挤压完成后,上模回程,工件留在凹模中,压力机下缸动作,通过顶杆将头部大直径部分顶出凹模,即可完成脱模。
以上显示和描述了本实用新型的基本原理和主要特征和本实用新型的优点。本行业的技术人员应该了解,本实用新型不受上述实施例的限制,上述实施例和说明书中描述的只是说明本实用新型的原理,在不脱离本实用新型精神和范围的前提下,本实用新型还会有各种变化和改进,这些变化和改进都落入要求保护的本实用新型范围内。本实用新型要求保护范围由所附的权利要求书及其等效物界定。
Claims (3)
1.一种铝合金拉杆的复合热挤压模具结构,包括上模板和下模板,其特征在于:所述上模板下方设有上垫板,所述上垫板下方设有凸模固定板,所述凸模固定板内设有凸模,所述凸模为中空结构,所述下模板上方设有下垫板,所述下垫板内设有顶杆,所述顶杆横穿下模板与下垫板底部连接,所述下垫板上方设有凹模预紧圈,所述凹模预紧圈内设有凹模,所述凹模内底部设有顶件器,所述顶件器上方设有制件。
2.根据权利要求1所述一种铝合金拉杆的复合热挤压模具结构,其特征在于:所述凸模贯穿凸模固定板插入凹模内。
3.根据权利要求1所述一种铝合金拉杆的复合热挤压模具结构,其特征在于:所述制件贯穿凹模与凸模中空部分吻合连接。