CN1921184A - 锂离子电池用多元掺杂锰酸锂正极活性材料 - Google Patents
锂离子电池用多元掺杂锰酸锂正极活性材料 Download PDFInfo
- Publication number
- CN1921184A CN1921184A CNA2005100109791A CN200510010979A CN1921184A CN 1921184 A CN1921184 A CN 1921184A CN A2005100109791 A CNA2005100109791 A CN A2005100109791A CN 200510010979 A CN200510010979 A CN 200510010979A CN 1921184 A CN1921184 A CN 1921184A
- Authority
- CN
- China
- Prior art keywords
- oxide
- active material
- anode active
- limn
- lithium ion
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (2)