CN1730397A - 小氧化铝厂溶出套管预热器的设置方法 - Google Patents
小氧化铝厂溶出套管预热器的设置方法 Download PDFInfo
- Publication number
- CN1730397A CN1730397A CN 200510200404 CN200510200404A CN1730397A CN 1730397 A CN1730397 A CN 1730397A CN 200510200404 CN200510200404 CN 200510200404 CN 200510200404 A CN200510200404 A CN 200510200404A CN 1730397 A CN1730397 A CN 1730397A
- Authority
- CN
- China
- Prior art keywords
- primary heater
- cannula primary
- dissolving
- factory
- standby
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种小氧化铝厂溶出套管预热器的设置方法,它是在原矿浆从158~172℃提温到260~280℃的温度段,增加一组套管预热器做备用,当在流程中运行的那组套管预热器需要出流程清洗时,将备用的整组套管预热器投入正常运行;将切换出流程的套管预热器清洗干净,留待备用;各组套管预热器成互为备用的关系。本发明能够大大提高小氧化铝厂的溶出装置运转率,从而提高全厂运转率和产量,提高经济效益。
Description
技术领域:
本发明涉及一种氧化铝生产工艺,特别是涉及小氧化铝厂溶出套管预热器的设置方法。
背景技术:
经过近几年的快速发展,我国拜尔法氧化铝生产线的设计规模已经成系列化了,目前有30kt/a、50kt/a、200kt/a、300kt/a、400~450kt/a共五种设计规模的拜尔法生产线。根据本行业的习惯,大家通常将产能小于200kt/a的氧化铝厂称为小氧化铝厂,产能在400kt/a以上的称为大型氧化铝厂。
由于生产规模不同,大厂与小厂使用的技术和装备是不同的。通常大厂的技术装备水平高、自动化程度高,而小厂的技术装备和自动化程度低一些。由于氧化铝生产物料的特殊性和设备规格相差悬殊,小厂的操作、管理比大厂反而更难,如氧化铝厂物料易在设备和管路上生成结疤,需要定期清理,小厂就比大厂困难很多。有的技术和设备在大厂使用很好,由于小厂物料流量小,则使用不上,如套管预热、压煮器间接加热、保温溶出技术(本行业也称A、P溶出技术)。由于小厂具有物料流量小的特点,在设计上选择工艺技术路线、技术经济指标和设计方案与大厂是有区别的。
溶出是拜尔法氧化铝生产过程中的核心工序,直接影响到全厂的产能及运转率,目前大厂选择的A、P溶出技术,其溶出装置的运转率可达到95%以上,而小厂选择的全单套管预热、熔盐加热、保温罐停留溶出技术,溶出装置的运转率仅67~80%,两者差距极大。
溶出装置运转率低,则全厂运转率也低,因为溶出装置停车清理时,后续的所有工序均无原料供应,只能处于停顿待产状态,由于后续设备内都装有物料,需要自身让槽罐内物料继续维持搅拌,以免发生沉积;另外,若停车时间太长,槽内物料会自然降温冷却,对生产极为不利。
如何提高小氧化铝厂的运转率,是提高全厂氧化铝产量、降低原材料消耗、提高经济效益的关键问题,在溶出装置的设计上应重点考虑。
A、P溶出技术运转率高,是由于它只采用了五~六级套管,套管预热温度为158~172℃,此温度段的结疤速度慢,且结疤为硅渣结疤为主,可采用较简单的化学清洗。一组套管预热器,用稀硫酸5小时左右就能清洗干净。而原矿浆从158~172℃提温到260℃温度段,采用了带加热管的压煮器提温,并在设计上考虑预留备用罐的办法,即当套管预热器清洗干净后,后面将备用罐投入运行,而退出流程待清洗的带加热管的压煮器,可待生产恢复后再清洗,不影响溶出装置正常工作,故A、P溶出技术运转率高。
小氧化铝厂由于溶出压煮器直径太小,无法在压煮器内设置加热管,只能采用全套管预热及加热,而高温段套管结疤速度快,且高温段套管壁上生成的钙钛结疤坚硬,此结疤不溶于酸,故不能用酸清洗,加之套管预热器无整体设备备用,而清洗一组整套的套管预热器要5~10天时间,故溶出装置运转率很低。
通过对大厂溶出装置运转率高的研究,结合小厂运转率低的原因分析,本发明提出小厂的套管预热器采用整体备用方案,可大幅度提高小厂溶出装置运转率,从而提高经济效益。
发明内容:
本发明的目的在于:采用新的套管预热器设备配置方法,提高小氧化铝厂溶出装置运转率,从而提高全厂运转率和产量,提高经济效益。
本发明是这样实现的:在原矿浆从158~172℃提温到260~280℃的温度段,增加一组套管预热器做备用,当在流程运行的那组套管预热器需要清洗时,将备用的整组套管预热器投入正常运行;将切换出流程的套管预热器清洗干净,留待备用;各组套管预热器成互为备用的关系。
在小氧化铝厂,溶出装置停车的主要原因是清洗套管预热器,通常情况下,当溶出装置运行1个月左右,套管预热器因结疤造成传热系数降低,加热温度达不到溶出温度的要求,溶出装置只能停车清洗套管,每次清洗时间为5~10天。若采用本发明的套管预热器整体备用的配置方法,可以消除套管清洗对溶出装置造成的不良影响,从而大幅度提高溶出装置运转率。
本发明的有益效果是:能够大大提高小氧化铝厂的溶出装置运转率,从而提高全厂运转率和产量,提高经济效益。
具体实施方式:
本发明的实施例1:
在原矿浆从158~172℃提温到260℃的温度段,增加一组套管预热器做备用;从高压隔膜泵来的原矿浆,进套管预热器进行预热和熔盐加热;当在流程运行的那组套管预热器需要清洗时,将备用的整组套管预热器投入正常运行;将切换出流程的套管预热器清洗干净,留待备用;各组套管预热器成互为备用的关系。
本发明的实施例2:
由于不同地方的铝土矿溶出性能有差异,有的溶出温度较高,需要将原矿浆温度从158~172℃提温到280℃,在此温度也可设置备用套管预热器,设置方法同实施1。
本发明的实施例3:
若氧化铝厂有两套溶出装置,为节约投资,两套溶出装置可共同备用一组套管预热器。生产组织管理时,两组溶出装置的清洗周期可错开进行,使其达到互为备用的目的。
Claims (1)
1.一种小氧化铝厂溶出套管预热器的设置方法,其特征是:在原矿浆从158~172℃提温到260~280℃的温度段,增加一组套管预热器做备用,当在流程运行的那组套管预热器需要清洗时,将备用的整组套管预热器投入正常运行;将切换出流程的套管预热器清洗干净,留待备用;各组套管预热器成互为备用的关系。