CN1730184A CN 200510017884 CN200510017884A CN1730184A CN 1730184 A CN1730184 A CN 1730184A CN 200510017884 CN200510017884 CN 200510017884 CN 200510017884 A CN200510017884 A CN 200510017884A CN 1730184 A CN1730184 A CN 1730184A
Authority
CN
China
Prior art keywords
steel plate
straight edge
roll
remained straight
rolls
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 200510017884
Other languages
English (en)
Inventor
李延广
郭呈方
王松海
刘新红
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
KELONG PETROCHEMICAL EQUIPMENT CO Ltd HENAN
Original Assignee
KELONG PETROCHEMICAL EQUIPMENT CO Ltd HENAN
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by KELONG PETROCHEMICAL EQUIPMENT CO Ltd HENAN filed Critical KELONG PETROCHEMICAL EQUIPMENT CO Ltd HENAN
Priority to CN 200510017884 priority Critical patent/CN1730184A/zh
Publication of CN1730184A publication Critical patent/CN1730184A/zh
Pending legal-status Critical Current

Links

Images

Landscapes

  • Bending Of Plates, Rods, And Pipes (AREA)

Abstract

本发明公开了一种对称式三辊卷板机筒体无剩余直边卷制工艺,它包括有将钢板放入上、下辊之间,将钢板卷成曲率相同的弧形板,一次行程后再将上辊下压一定距离,又驱动下辊,使钢板进一步受到弯卷,将钢板弯卷成C型;在钢板下料时,除掉剩余直边不计,按筒体中径下料;卷制时卷制曲率半径应再加一个附加量200-500mm;卷成C字型后,两端形成剩余直边,再卷至两个剩余直边合口,把合口对齐进行焊接,形成一个平板,而后置于卷板机上,消除剩余直边。本发明能够使利用对称式三辊卷板机卷制筒体时无剩余直边,节约钢板,且应用方便。

Description

对称式三辊卷板机筒体无剩余直边卷制工艺
技术领域
本发明属于基本上无切削的金属机械加工,尤其是一种利用对称式三辊卷板机卷制筒体无剩余直边的加工工艺。
背景技术
以往利用对称式三辊卷板机制筒体时,操作容易,成型较准确,但钢板的两端都不能通过最大的弯矩点,因此不能卷曲形成直边,产生边角废料,造成浪费。
发明内容
本发明旨在提供一种利用对称式三辊卷板机筒体时能够消除剩余直边的加工工艺,提高钢板的利用率,减少资源浪费,且应用方便。
本发明的目的是这样达到的,对称式三辊卷板机筒体无剩余直边卷制工艺,它包括有将钢板放入上、下辊之间,然后上辊向下将钢板压弯到一定程度,再驱动两下辊旋转,使钢板左右移动,将钢板卷成曲率相同的弧形板,一次行程后再将上辊下压一定距离,又驱动下辊,使钢板进一步受到弯卷,如此反复进行将钢板弯卷成C型,其特征在于:在钢板下料时,除掉剩余直边不计,按筒体中径下料;卷制时卷制曲率半径应再加一个附加量200-500mm;将钢板卷成C字型后,两端形成剩余直边,再卷至两个剩余直边合口,而后把合口对齐进行焊接,形成一个平板,将平板的两端分别置于两个下辊上,使上辊下压后再升至原位而后左右滚动成型,消除剩余直边。本发明能够使利用对称式三辊卷板机卷制筒体时无剩余直边,节约钢板,且应用方便。
附图说明
图1为本发明将钢板卷制C型状态时的示意图;图2为本发明将钢板卷制到合口状态时的示意图。
图中:1、上辊;2、下辊;3、钢板;4、剩余直边;5合口。
具体实施方式
对称式三辊卷板机主要有上辊和两个下辊组成,上辊可以在钢板上左右旋转移动,下辊即主动辊,可以正反旋转。以往卷制钢板的工艺是:将剩余直边计算在内的钢板,放入上辊1和下辊2之间,然后上辊1向下把钢板压弯,此时钢板弯曲部分的内层受压而外层受拉,在两个下辊2的中间弯距最大,达到塑性弯曲状态,再驱动两个下辊2旋转,并借助于钢板和辊子之间的磨擦力使钢板左右移动,与此同时上辊1随着转动,使钢板变成曲率相同的弧形板,一次行程后,再将上辊1下压,又驱动下辊2旋转,上辊1和下辊2同时转动,使钢板进一步弯卷成C型,如此反复进行,就将钢板弯卷到所需要的曲率半径,将剩余直边割去再合口即完成加工过程。
本发明是在原工艺基础上创造的,本发明在钢板下料时,除掉剩余直边不计,按筒体中径下料,计算公式为L=πD;卷制时曲率半径应再加一个附加量200-500mm,上辊1和下辊2旋转将钢板3卷制成C字型之后,形成两个剩余直边4,如图1所示,而后再卷至两个剩余直边4合口,把合口5严格对齐进行焊接形成平板,将平板的两端分别置于下辊2上,使上辊1下压后再升到原来位置,而后左右滚动,消除了剩余直边,校圆至卷制完成。

Claims (1)

1、对称式三辊卷板机筒体无剩余直边卷制工艺,它包括有将钢板放入上、下辊之间,然后上辊向下将钢板压弯到一定程度,再驱动两下辊旋转,使钢板左右移动,将钢板卷成曲率相同的弧形板,一次行程后再将上辊下压一定距离,又驱动下辊,使钢板进一步受到弯卷,如此反复进行将钢板弯卷成C型,其特征在于:在钢板下料时,除掉剩余直边不计,按筒体中径下料;卷制时卷制曲率半径应再加一个附加量200-500mm;将钢板卷成C字型后,两端形成剩余直边,再卷至两个剩余直边合口,而后把合口对齐进行焊接,形成一个平板,将平板的两端分别置于两个下辊上,使上辊下压后再升至原位而后左右滚动成型,消除剩余直边。
CN 200510017884 2005-08-11 2005-08-11 对称式三辊卷板机筒体无剩余直边卷制工艺 Pending CN1730184A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 200510017884 CN1730184A (zh) 2005-08-11 2005-08-11 对称式三辊卷板机筒体无剩余直边卷制工艺

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 200510017884 CN1730184A (zh) 2005-08-11 2005-08-11 对称式三辊卷板机筒体无剩余直边卷制工艺

Publications (1)

Publication Number Publication Date
CN1730184A true CN1730184A (zh) 2006-02-08

Family

ID=35962625

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 200510017884 Pending CN1730184A (zh) 2005-08-11 2005-08-11 对称式三辊卷板机筒体无剩余直边卷制工艺

Country Status (1)

Country Link
CN (1) CN1730184A (zh)

Cited By (13)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN100393439C (zh) * 2006-05-29 2008-06-11 张挺胜 增加水平下调式三辊卷板机预弯能力的方法
CN101579700B (zh) * 2009-06-24 2010-12-01 青岛北海船舶重工有限责任公司 超长超厚圆弧板制作方法
CN102350447A (zh) * 2011-08-16 2012-02-15 沈阳远大铝业工程有限公司 一种带边滚弧件的加工方法
CN102785057A (zh) * 2011-05-16 2012-11-21 中国二十冶集团有限公司 免预弯的钢板滚圆筒方法
CN102941264A (zh) * 2012-11-23 2013-02-27 贵州安大航空锻造有限责任公司 铝合金闪光焊薄壁环件的型材弯曲制坯方法
CN102941261A (zh) * 2012-11-23 2013-02-27 贵州安大航空锻造有限责任公司 α相钛合金闪光焊薄壁环件的型材弯曲制坯方法
CN103612068A (zh) * 2012-11-27 2014-03-05 国机重工(洛阳)有限公司 一种压路机轮圈卷制工艺
CN103659180A (zh) * 2013-11-18 2014-03-26 哈尔滨电机厂有限责任公司 大型水轮机主轴冷滚成型拼接制造工艺方法
CN104889208A (zh) * 2015-05-28 2015-09-09 南京皓威机械有限公司 多自由度三辊制管机
CN107263031A (zh) * 2017-06-26 2017-10-20 山东美陵化工设备股份有限公司 筒体无预弯卷圆成型工艺
CN110014058A (zh) * 2018-01-10 2019-07-16 李书军 一种曲面蜂窝芯板成型工艺
CN111451332A (zh) * 2019-12-20 2020-07-28 南通超力卷板机制造有限公司 三辊卷板机滚弯成形后圆筒体的圆度矫正方法
CN111589909A (zh) * 2020-04-28 2020-08-28 中船澄西船舶修造有限公司 一种对称式三辊卷板机卷制的带直边卷管的滚弯方法

Cited By (16)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN100393439C (zh) * 2006-05-29 2008-06-11 张挺胜 增加水平下调式三辊卷板机预弯能力的方法
CN101579700B (zh) * 2009-06-24 2010-12-01 青岛北海船舶重工有限责任公司 超长超厚圆弧板制作方法
CN102785057A (zh) * 2011-05-16 2012-11-21 中国二十冶集团有限公司 免预弯的钢板滚圆筒方法
CN102350447A (zh) * 2011-08-16 2012-02-15 沈阳远大铝业工程有限公司 一种带边滚弧件的加工方法
CN102941264B (zh) * 2012-11-23 2014-12-17 贵州安大航空锻造有限责任公司 铝合金闪光焊薄壁环件的型材弯曲制坯方法
CN102941261A (zh) * 2012-11-23 2013-02-27 贵州安大航空锻造有限责任公司 α相钛合金闪光焊薄壁环件的型材弯曲制坯方法
CN102941264A (zh) * 2012-11-23 2013-02-27 贵州安大航空锻造有限责任公司 铝合金闪光焊薄壁环件的型材弯曲制坯方法
CN102941261B (zh) * 2012-11-23 2014-12-17 贵州安大航空锻造有限责任公司 α相钛合金闪光焊薄壁环件的型材弯曲制坯方法
CN103612068A (zh) * 2012-11-27 2014-03-05 国机重工(洛阳)有限公司 一种压路机轮圈卷制工艺
CN103659180A (zh) * 2013-11-18 2014-03-26 哈尔滨电机厂有限责任公司 大型水轮机主轴冷滚成型拼接制造工艺方法
CN103659180B (zh) * 2013-11-18 2016-01-20 哈尔滨电机厂有限责任公司 大型水轮机主轴冷滚成型拼接制造工艺方法
CN104889208A (zh) * 2015-05-28 2015-09-09 南京皓威机械有限公司 多自由度三辊制管机
CN107263031A (zh) * 2017-06-26 2017-10-20 山东美陵化工设备股份有限公司 筒体无预弯卷圆成型工艺
CN110014058A (zh) * 2018-01-10 2019-07-16 李书军 一种曲面蜂窝芯板成型工艺
CN111451332A (zh) * 2019-12-20 2020-07-28 南通超力卷板机制造有限公司 三辊卷板机滚弯成形后圆筒体的圆度矫正方法
CN111589909A (zh) * 2020-04-28 2020-08-28 中船澄西船舶修造有限公司 一种对称式三辊卷板机卷制的带直边卷管的滚弯方法

Similar Documents

Publication Publication Date Title
CN1730184A (zh) 对称式三辊卷板机筒体无剩余直边卷制工艺
CN203426223U (zh) 瓦楞形板成型机组
CN202242311U (zh) 胶印机输纸前规压纸装置
CN206415525U (zh) 一种智能送料机构
CN201049365Y (zh) 数显卷板机
CN2933635Y (zh) 三弯三矫冷轧带钢拉伸矫直机
CN204220751U (zh) 汽车底盘冲压模具
CN202683676U (zh) 工作辊压下量单独控制的辊式矫直机
CN205763076U (zh) 一种斜辊矫直机
CN201287161Y (zh) 球壳网架围护用弧形柃条滚弯机
CN101985140A (zh) 圆形沿口型材的弯曲成型方法和装置
CN202447456U (zh) 槽钢弯曲机
CN2582774Y (zh) 无压痕折弯模
CN102941264A (zh) 铝合金闪光焊薄壁环件的型材弯曲制坯方法
CN202606562U (zh) 中板分条生产线
CN204685736U (zh) 板材平整机
CN102941259A (zh) 结构钢闪光焊薄壁环件的型材弯曲制坯方法
CN208373927U (zh) 一种层板凹边内压90度角的压边装置
CN207447030U (zh) 一种辊型生产线上的波纹板料水平夹送装置
CN104668367A (zh) 一种万能模具弯弧机及其加工方法
CN201376017Y (zh) 压弯式卷筒装置
CN205056666U (zh) 用于可逆轧机的去油辊
CN206382445U (zh) 一种卷料预处理装置
CN206588216U (zh) 一种用于生产汽车散热器b型管的产线
CN203484451U (zh) 一种辊扎折弯机

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication