CN1557733A - 活性炭电极电解回收废水中镍(ⅱ)的方法 - Google Patents

活性炭电极电解回收废水中镍(ⅱ)的方法 Download PDF

Info

Publication number
CN1557733A
CN1557733A CNA200410023427XA CN200410023427A CN1557733A CN 1557733 A CN1557733 A CN 1557733A CN A200410023427X A CNA200410023427X A CN A200410023427XA CN 200410023427 A CN200410023427 A CN 200410023427A CN 1557733 A CN1557733 A CN 1557733A
Authority
CN
China
Prior art keywords
nickel
activated carbon
electrode
waste water
cathode
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CNA200410023427XA
Other languages
English (en)
Other versions
CN100390075C (zh
Inventor
欣 张
张欣
喻宗仁
吴仁涛
张明让
张超
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Taishan University
Original Assignee
Taishan University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Taishan University filed Critical Taishan University
Priority to CNB200410023427XA priority Critical patent/CN100390075C/zh
Publication of CN1557733A publication Critical patent/CN1557733A/zh
Application granted granted Critical
Publication of CN100390075C publication Critical patent/CN100390075C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本发明公开了一种从废水中回收镍(II)的新工艺方法,属于电化学应用技术领域,其解决的技术关键是采用活性炭做阴极,增大了对电解时生成氢氧化镍的吸附性能,使回收的氢氧化镍比较纯净,镍(II)的回收率可达99%以上。该工艺简单易操作,耗电量较少,成本低,减少了废水对环境的污染,可用于电镀废水、化学镀废水及一切含镍(II)废水中镍(II)的回收,用来生产化工原料或化学试剂。

Description

活性炭电极电解回收废水中镍(II)的方法
技术领域:
本发明属于电化学应用新工艺方法。
背景技术:
对于从废水中回收镍(II)目前主要采取沉淀气浮法,该方法工艺复杂需要消耗大量的碱、气浮剂及压缩空气,而且生成的氢氧化镍沉淀物气浮后不好收集,沉淀物中含杂质较多,后续处理困难。
发明内容:
利用活性炭做阴极,用金属铅做阳极,在废水中加入少量硫酸钠进行电解,当直流电通过电极时,由于在阴极上有氢气析出而造成阴极附近pH值升高,当镍(II)离子在电场作用下移动到阴极附近,来不及发生电化学还原反应就以氢氧化镍的形态沉积在活性炭及阴极套表面上。将活性炭电极从废水中取出用稀硫酸(稀盐酸或稀硝酸)溶解就得到相应的镍盐溶液,再经净化、浓缩、结晶工艺过程可得到纯净的相应固体镍盐。反应式如下:
                       
                    
                     
                   
该方法的优点是:简化了从废水中回收镍(II)的工艺过程,提高了回收氢氧化镍的纯度;从废水中回收镍(II)速度快;镍(II)的回收率高;能从
含镍(II)浓度较低的废水中回收镍(II);耗电少;生产成本低。
附图说明:
阴极用金属铅做导电骨架,骨架四周填装30目-50目的活性炭,把骨架和活性炭装在阴极套中。阴极套可用涤纶布制作。如图1所示。
具体实施方式:
下面是采用本发明回收废水中镍(II)生产化学试剂硫酸镍的一个具体实施例:
向含镍(II)废水中加入少量硫酸钠(因废水中一般含镍(II)浓度较低,加入硫酸钠增加溶液导电性,而且使铅阳极变成不溶性电极),将废水pH值调控在6~8之间,通以直流电,电流密度控制在0.05A/cm2(骨架面积),当直流电通过电极时,由于阴极上有氢气析出而造成阴极附近pH值升高,当镍(II)离子在电场作用下移动到阴极附近,来不及发生还原反应就以氢氧化镍的形态沉积在活性炭的表面及电极套的表面上,定时将活性炭阴极从废水中取出,用稀硫酸溶解氢氧化镍即可制成相应的硫酸镍溶液,再经如图2工艺流程即可得到较纯净的硫酸镍固体。

Claims (2)

1、一种从废水中回收镍(II)的新工艺方法,其特征是利用活性炭阴极和铅阳极,在废水中加入少量硫酸钠在通直流电的情况下,使废水中的镍(II)以氢氧化镍的形态沉积在活性炭及阴极套表面上,经过酸溶解、净化、浓缩、结晶以固体镍盐加以回收。
2、根据权力要求1所述,使用活性炭电极采用电化学法从废水中回收镍(II),其特征是采用金属铅作为活性炭电极导电骨架,将电极骨架装在用涤纶布制作的阴极套内,并在导电骨架四周填装30目~50目的活性炭。
CNB200410023427XA 2004-01-12 2004-01-12 活性炭电极电解回收废水中二价镍的方法 Expired - Fee Related CN100390075C (zh)