CN1127993C - 一种透明玻璃钢面篮球板的制作方法 - Google Patents
一种透明玻璃钢面篮球板的制作方法 Download PDFInfo
- Publication number
- CN1127993C CN1127993C CN 00121534 CN00121534A CN1127993C CN 1127993 C CN1127993 C CN 1127993C CN 00121534 CN00121534 CN 00121534 CN 00121534 A CN00121534 A CN 00121534A CN 1127993 C CN1127993 C CN 1127993C
- Authority
- CN
- China
- Prior art keywords
- board
- fiber reinforced
- glass fiber
- resin
- reinforced plastic
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种透明玻璃钢面篮球板的制作方法,其特点是在原有的体育场(馆)的篮球板即木板表面嵌有一层带黑色边框、中间黑色方框和白色底面的有色玻璃钢板面结构基础上,采用加压模具,在有色玻璃钢板面上再设置一层树脂层即透明玻璃钢板。本发明篮球板的表面如玻璃一样的光亮、透明,立体感很强,而且保证篮球板各种颜色不褪色,永保鲜艳,其表面两层玻璃钢具有很强的附着力,强度也很高,是一种高档次的玻璃钢篮球板。
Description
技术领域
本发明属于运动器械领域,更具体地说,是一种安装有透明玻璃钢面的篮球板的制作方法。
背景技术
体育场(馆)通常使用的篮球板包括有机玻璃制造的篮球板、木制篮球板以及是在一块木板上安装有一层玻璃钢面,玻璃钢面上具有黑色边框、中间黑色方框和白色底面的玻璃钢篮球板,但是现有的玻璃钢篮球板光洁度不好且粗糙,使用一段时间后沾灰、褪色,失去光泽,直观效果不好。
发明内容
本发明的目的是改进现有的玻璃钢篮球板,提出一种光洁度好、不褪色、直观效果好的篮球板及其制造方法。
本发明的主要技术方案:在原有的体育场(馆)玻璃钢篮球板结构基础上,再设置一层质量优良、透明性好、强度高、施工方便的透明玻璃钢面。
本发明的篮球板的具体制作方法包括以下步骤:
(1)制作压面模具:用木条制成内框尺寸大于篮球板的长方型木框,然后将厚度为0.1~0.2mm的整张的聚脂薄板平整的固定在木框上即构成所需的加压模具,
(2)制作透明玻璃面,其过程依次为:
a.对已知的玻璃钢篮球板表面基本水平的有色玻璃钢面,用砂纸将面层打磨一遍并擦净表面,
b.将步骤(a)处理后的有色玻璃板面上倒入1.8~2.0公斤的糊状树脂,
c.将制作的加压模具迅速地盖上步骤(b)已倒入树脂的有色玻璃钢面,然后对木条方框均匀加压,
d.用胶滚筒在模具的聚脂薄板上来回均匀加压滚动,直至气泡被赶出并使树脂表面滚平,待24小时后树脂完全固化脱出模具,
e.将周边修平、修直即制成厚度为2~3mm的透明玻璃钢面篮球板。
本发明所述的已知的具有玻璃钢面的篮球板上的黑边框和板中间的黑框必须是玻璃钢材料,不能是油漆,否则树脂不能很好地附着在上面。
本发明所述的压面模具上的聚脂薄板一定要绷紧绷平,否则影响透明玻璃钢面的质量。
本发明所述的糊状树脂是江苏亚邦涂料股份有限公司生产的191树脂,该树脂是不饱和聚酯树脂,在室温下完成冷固化,适用制造玻璃钢制品,树脂内加有含环烷酸钴的T-8E促进剂和含过氧化环己酮引发剂H,其混合重量比为树脂∶T-8E∶H=50∶2∶2,树脂的性能:酸值16~24mgKOH/g,25℃下胶凝时间6~15分钟,固体含量61~67%。
本发明所述的胶滚筒为印刷用的胶滚筒,属已知工具。
本发明的优点和效果:
本发明由于在已有的具有黑色框和白色底面的玻璃钢面再加一层透明玻璃钢,致使篮球板的立体感效果非常好,而且保证篮球板各种颜色不褪色,永保鲜艳;本发明由于采用加压模具,模具上装有光洁度好的聚脂薄板,因此制成的透明玻璃钢如玻璃一样的光亮、透明,而且由于光洁度好,长时间的使用不会沾灰和显得陈旧;本发明由于已知的篮球板面全是玻璃钢,与本发明的透明玻璃钢有着很强的附着力,强度也很高,经过两年的球场试用,强度仍然很好,面层仍然很牢,卸下后用铲刀用力凿都不能将其分开。
附图说明
图1为已知篮球板侧面结构示意图;
图2为本发明篮球板侧面结构示意图。
具体实施方式
下面通过具体实施例进一步说明本发明的特点。
由图1所示,1为木板层,2为玻璃钢层,层面有黑色边框、中间有黑色方框,其它部分是白色的,其尺寸:长×宽×厚=1.8×1.05×0.03m。
首先用杉木条制成内框为长×宽=2.20×1.45m的长方型框,再将0.1mm厚的整张聚脂薄板钉在方框上,绷紧、绷直,制成加压模具;
将玻璃层2面上用360号砂纸打磨一遍,擦净表面杂物,再倒入配制好的191树脂,立即将前述的加压模具盖上已倒入树脂的有色玻璃钢面上,然后在模具的木条方框上均匀地压上总重为45公斤重的方砖,然后用胶滚筒在模具的聚脂薄板上来回人工加压滚动?遍,赶掉气泡,25小时脱模,再用铲刀将周边修平、修直即得到图2所示的本发明的具有透明玻璃钢面的篮球板,图2中3为透明玻璃钢面,其厚度为3毫米。
Claims (1)
1.一种透明玻璃钢面篮球板的制作方法,其特征在于制备过程如下:
(1)用木条制成内框尺寸大于篮球板的长方型木框,然后将厚度为0.1~0.2mm的整张的聚脂薄板平整的固定在木框上制成加压模具;
(2)对已知的平面基本水平的有色玻璃钢面,用砂纸将面层打磨一遍并擦净表面;
(3)将步骤(2)处理后的有色玻璃板面上倒入1.8~2.0公斤的糊状树脂,所述的糊状树脂为不饱和聚酯树酯;
(4)将步骤(1)制作的加压模具迅速地盖上步骤(3)已倒入不饱和聚酯树脂的有色玻璃钢面,然后对木条方框均匀加压;
(5)用胶滚筒在模具的聚脂薄板上来回均匀加压滚动,直至气泡被赶出并使树脂表面滚平,待24小时后树脂完全固化脱出模具;
(6)将周边修平、修直即制成具有厚度为2~3mm的透明玻璃钢面的篮球板。