CN110607881A - 一种粉刷砂浆空鼓粘结再生技术 - Google Patents
一种粉刷砂浆空鼓粘结再生技术 Download PDFInfo
- Publication number
- CN110607881A CN110607881A CN201810623799.8A CN201810623799A CN110607881A CN 110607881 A CN110607881 A CN 110607881A CN 201810623799 A CN201810623799 A CN 201810623799A CN 110607881 A CN110607881 A CN 110607881A
- Authority
- CN
- China
- Prior art keywords
- grouting
- anchor
- determining
- outer sleeve
- holes
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种粉刷砂浆空鼓粘结再生技术,具体包括以下步骤:1、空鼓范围确定和空鼓层的确定;2、锚钉长度确定;布孔数确定,同时进行无尘无振动的打孔;3、清孔处理;4、安装注浆锚钉,锚钉脚膨胀;5、配置注浆料;6、注浆,注浆检查,注浆孔修补;7、养护,验收。该方法简单、质量稳定、成本低、效率高、安全可靠、资源节约、减少建筑垃圾、绿色环保。
Description
技术领域
本发明属于建筑修缮技术领域领域,具体涉及一种粉刷砂浆空鼓粘结再生技术。
背景技术
当出现粉刷砂浆空鼓后,现有技术是采用切割铲除空鼓区域,用界面剂处理该区域,然后重新配制新的粉刷砂浆或聚合物改性砂浆或砂浆中掺入纤维进行重新粉刷。
现有技术工艺流程:判断空鼓范围——沿空鼓周边切割——铲除空鼓层——清理基层——配制界面剂——涂刷界面剂——配置修复砂浆——粉刷修复砂浆。
但是也能够看到现有技术和工艺不能完全解决空鼓、开裂问题,易在切割断面开裂;重新粉刷修复砂浆仍然会出现空鼓或部分空鼓现象,不能解决安全隐患;同时铲除过程会产生很多建筑垃圾,费时费工。
发明内容
本发明针对背景技术所提出的问题,发明了一种粉刷砂浆空鼓粘结再生技术,该技术解决了空鼓、开裂问题,易在切割断面开裂的问题,杜绝安全隐患,同时更加便利,也减少了成本。
本发明的技术方案是:一种粉刷砂浆空鼓粘结再生技术,具体包括以下步骤:
1、空鼓范围确定和空鼓层的确定;
2、锚钉长度确定;布孔数确定,同时进行无尘无振动的打孔;
3、清孔处理;
4、安装注浆锚钉,促使锚钉脚膨胀;
5、配置注浆料;
6、注浆,注浆检查,注浆孔修补;
7、养护,验收。
其中,所述锚钉包括管形结构的外套部,所述外套部的侧壁上设有通孔或通槽,同时根部设置有与所述外套部内径相同的实心内衬部。
进一步的,所述所述外套部的端部设置有翻边,同时,所述翻边内设置有防水圈。
本发明的有益效果体现在:
1.该方法简单、质量稳定、成本低、效率高、安全可靠、资源节约、减少建筑垃圾、绿色环保。
附图说明
下面结合附图及实施例对本发明作进一步描述:
图1为所述锚钉的结构示意图;
图2为所述锚钉的张开结构示意图;
图3为实施例一中墙面的平面图;
图4为图3中A-A面的剖面图;
图5为实施例二中墙面的平面图;
图6为图5中A-A面的剖面图;
图中:1、外套部,2、内衬部,3、通槽,4、锚钉,5、注浆树脂,6、粉刷层,7、灌浆空鼓层,8、残余空鼓层,9、注浆孔,10、灌浆扩散区域,11、美化层。
具体实施方式
实施例:结合图1所示,为本发明提供的一种粉刷砂浆空鼓粘结再生技术,具体包括以下步骤:
1、空鼓范围确定和空鼓层的确定;
2、锚钉长度确定;布孔数确定,同时进行无尘无振动的打孔;
3、清孔处理;
4、安装注浆锚钉,锚钉脚膨胀;
5、配置注浆料;
6、注浆,注浆检查,注浆孔修补;
7、养护形成美化层,验收。
其中,所述空鼓范围通过钻孔取样或钻孔拍照的方式来确定,空鼓层通过打诊听声音或红外成像的方式来确认。
锚钉长度根据空鼓层的厚度来确定,具体为装钉时进入基础层25-30MM,同时锚钉孔比钉深5MM,不装钉的注浆孔超过空鼓层大于等于5MM。
布孔数为一平方米内打9-50个孔。
实施例一:一平米范围内打16个孔,全部为锚钉孔,通过锚钉向空鼓层内注入树脂,有树脂的地方形成灌浆空鼓层7,没有灌浆的地方为残余空鼓层,同时,灌浆后周围一圈为灌浆扩散区域10,灌完浆后通过美化层11来进行修饰。
实施例二:在该实施例中,打41个孔,为梅花式布置,41个孔中25个孔用于安装锚钉,其余16个不装锚钉孔,只是单纯的注浆孔,且每两个孔之间的间距不大于330mm,在打孔过程中先处理完装锚钉的25个孔,整体检查后,在依次完成不装锚钉的16个孔,全部打完后,再复查确定是否需要补充打孔,同时,打孔通过通过特殊的钻头与钻杆进行打孔,其中,所述钻杆端部设有收集装置用于收集钻孔所产生的污水和污物,同时,所述钻头为金刚砂材质。
配置注浆料时,采用专用的聚合物注浆料,使用水泥基聚合物或树脂作为原材料,粘度在100-100000,粘结强度大于0.7MPA,具体使用中依据空鼓层厚度和空鼓两侧材料选择使用。
当然上述实施例只为说明本发明的技术构思及特点,其目的在于让熟悉此项技术的人能够了解本发明的内容并据以实施,并不能以此限制本发明的保护范围。凡根据本发明主要技术方案的精神实质所做的修饰,都应涵盖在本发明的保护范围之内。
Claims (2)
1.一种粉刷砂浆空鼓粘结再生技术,具体包括以下步骤:
1、空鼓范围确定和空鼓层的确定;
2、锚钉长度确定;布孔数确定,同时进行无尘无振动的打孔;
3、清孔处理;
4、安装注浆锚钉,锚钉脚膨胀;
5、配置注浆料;
6、注浆,注浆检查,注浆孔修补;
7、养护,验收。
其中,所述锚钉包括管形结构的外套部,所述外套部的尾端侧壁上设有通孔或通槽,同时外套部内部设置有与所述外套部内径相同的实心内衬部。
2.根据权利要求1所述的一种粉刷砂浆空鼓粘结再生技术,其特征在于,所述所述外套部的端部设置有翻边,同时,所述翻边内设置有防水圈。