CN109136954A - 一种金属环保型水基防锈剂 - Google Patents

一种金属环保型水基防锈剂 Download PDF

Info

Publication number
CN109136954A
CN109136954A CN201810877036.6A CN201810877036A CN109136954A CN 109136954 A CN109136954 A CN 109136954A CN 201810877036 A CN201810877036 A CN 201810877036A CN 109136954 A CN109136954 A CN 109136954A
Authority
CN
China
Prior art keywords
base
friendlywater
water
metal
rust inhibitor
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810877036.6A
Other languages
English (en)
Inventor
庞亚恒
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Tianjin New Materials Co Ltd
Original Assignee
Tianjin New Materials Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tianjin New Materials Co Ltd filed Critical Tianjin New Materials Co Ltd
Priority to CN201810877036.6A priority Critical patent/CN109136954A/zh
Publication of CN109136954A publication Critical patent/CN109136954A/zh
Pending legal-status Critical Current

Abstract

一种金属环保型水基防锈剂,其特征在于,包括如下重量份的各组份:纯水:75~90%、成膜剂:3~5%、碱性助剂:2~8%、金属缓释剂:2~10%、稳定剂:1~3%。按照国家轻工行业标准QB/T2117‑95《通用水基金属净洗剂》的要求进行防锈性试验,实验条件为:(35±2)℃,RH(90±2)%,试片材质为HT300铸铁,5%浓度的防锈剂工作液,进行连续测试实验。在达到规定时间后,铸铁拼啊表面无锈点、无明显变化,评定为0级,合格。

Description

一种金属环保型水基防锈剂
技术领域
本发明涉及一种防锈剂,具体涉及一种金属环保型水基防锈剂。
背景技术
水基防锈剂目前大多含有亚硝酸盐、铬酸盐或磷酸盐等成分,具有较强的毒性,容易造成环境污染及水体的富营养化。随着环保意识的提高,及环境监督的常态化,上述含有亚硝酸盐、铬酸盐及磷酸盐的水基防锈剂在使用和排放中受到严格限制,因此金属防护市场需要环保型的水基防锈剂。本发明的水基防锈剂配方不含亚硝酸盐、铬酸盐及磷酸盐等有毒有害物质,使用后的防锈剂经简单的中和处理后就可以排放,安全环保
发明内容
本发明主要解决的技术问题是:针对传统防锈剂防锈性能不佳的问题,提供了一种环保型水基防锈剂。
为了解决上述技术问题,本发明所采用的技术方案是:一种金属环保型水基防锈剂,其特征在于,包括如下重量份的各组份:
纯水:75~90%、成膜剂:3~5%、碱性助剂:2~8%、金属缓释剂:2~10%、稳定剂:1~3%
进一步,所述成膜剂为:甘油、羧甲基纤维素钠(CMC)、羧乙基纤维素、聚马来酸酐、聚丙烯酸酯中的一种或几种。
进一步,所述碱性助剂为:钼酸钠、钨酸钠、苯甲酸钠中的一种或多种。
进一步,所述金属缓蚀剂为:油酸酰胺、三乙醇胺、硼酸、乙二胺四乙酸、六次甲基四胺中的一种或它们的混合物。
进一步,所述稳定剂:乙醇、葡萄糖酸钠中的一种或多种。
本发明的有益效果是:
按照国家轻工行业标准QB/T2117-95《通用水基金属净洗剂》的要求进行防锈性试验,实验条件为:(35±2)℃,RH(90±2)%,试片材质为HT300铸铁,5%浓度的防锈剂工作液,进行连续测试实验。在达到规定时间后,铸铁拼啊表面无锈点、无明显变化,评定为0级,合格。
具体实施方式
实施例1:
水:86%
羧甲基纤维素钠:5%
钼酸钠:2%
苯甲酸钠:3%
三乙醇胺:2%
六次甲基四胺:1%
乙醇:1%
实施例2:
水:85%
羧乙基纤维素:3%
钨酸钠:6%
苯甲酸钠:1%
硼酸:1%
六次甲基四胺:2%
乙醇:1%
实施例3:
水:86%
羧甲基纤维素钠:5%
钼酸钠:2%
苯甲酸钠:3%
三乙醇胺:2%
六次甲基四胺:1%
乙醇:1%
最后应说明的是:以上各实施例仅用以说明本发明的技术方案,而非对其限制;尽管参照前述各实施例对本发明进行了详细的说明,本领域的普通技术人员应当理解:其依然可以对前述各实施例所记载的技术方案进行修改,或者对其中部分或者全部技术特征进行等同替换;而这些修改或者替换,并不使相应技术方案的本质脱离本发明各实施例技术方案的范围。

Claims (5)

1.一种金属环保型水基防锈剂,其特征在于,包括如下重量份的各组份:
纯水:75~90%、成膜剂:3~5%、碱性助剂:2~8%、金属缓释剂:2~10%、稳定剂:1~3%。
2.如权利要求1所述的一种金属环保型水基防锈剂,其特征在于,所述成膜剂为:甘油、羧甲基纤维素钠(CMC)、羧乙基纤维素、聚马来酸酐、聚丙烯酸酯中的一种或几种。
3.如权利要求1所述的一种金属环保型水基防锈剂,其特征在于,所述碱性助剂为:钼酸钠、钨酸钠、苯甲酸钠中的一种或多种。
4.如权利要求3所述的一种金属环保型水基防锈剂,其特征在于,所述金属缓蚀剂为:油酸酰胺、三乙醇胺、硼酸、乙二胺四乙酸、六次甲基四胺中的一种或它们的混合物。
5.如权利要求1所述的一种金属环保型水基防锈剂,其特征在于,所述稳定剂:乙醇、葡萄糖酸钠中的一种或多种。
CN201810877036.6A 2018-08-03 2018-08-03 一种金属环保型水基防锈剂 Pending CN109136954A (zh)