CN108555228A - 一种用于铝合金涂料 - Google Patents

一种用于铝合金涂料 Download PDF

Info

Publication number
CN108555228A
CN108555228A CN201711276083.7A CN201711276083A CN108555228A CN 108555228 A CN108555228 A CN 108555228A CN 201711276083 A CN201711276083 A CN 201711276083A CN 108555228 A CN108555228 A CN 108555228A
Authority
CN
China
Prior art keywords
parts
aluminium alloy
alloy coating
schmigel
attapulgite
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN201711276083.7A
Other languages
English (en)
Inventor
俞爱斌
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anhui Jinda Energy Saving Materials Development Co Ltd
Original Assignee
Anhui Jinda Energy Saving Materials Development Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anhui Jinda Energy Saving Materials Development Co Ltd filed Critical Anhui Jinda Energy Saving Materials Development Co Ltd
Priority to CN201711276083.7A priority Critical patent/CN108555228A/zh
Publication of CN108555228A publication Critical patent/CN108555228A/zh
Withdrawn legal-status Critical Current

Abstract

本发明公开了一种用于铝合金涂料,按照重量份由以下原料组成:凹凸棒土30‑40份、乙烯‑醋酸乙烯酯10‑20份、附着力促进剂1‑3份、刚玉粉25‑30份、乙醇30‑40份、海藻酸钠0.8‑1.0份和硅溶胶3.5‑4.0份。本发明一种用于铝合金涂料具备较好的粘度,良好的高温抗裂性和高温强度,能有效地防止铸造缺陷。

Description

一种用于铝合金涂料
技术领域
本发明涉及机械制造领域,具体是一种用于铝合金涂料。
背景技术
作为结构材料,与钢铁相比,铝合金具有密度小,比强度高等优点,在航空、航天、汽车、医疗器械等领域用量日益增加。在铝合金铸件生产过程中,尤其是在带有孔的铝合金铸件制造过程中,在孔结构附近会产生大量的孔洞缺陷,造成铝合金铸件性能尤其力学性能与密封性能的大幅下降,导致成品率低,大量能源浪费,给生产带来损失。对于铝合金中孔洞缺陷的研究早已经成为铸造用铝合金的研究热点,但是一直没有很有效的工艺方法以控制或消除此类孔洞缺陷。
发明内容
本发明的目的在于提供一种用于铝合金涂料,解决上述技术缺陷。
为实现上述目的,本发明提供如下技术方案:
一种用于铝合金涂料,按照重量份由以下原料组成:凹凸棒土30-40份、乙烯-醋酸乙烯酯10-20份、附着力促进剂1-3份、刚玉粉25-30份、乙醇30-40份、海藻酸钠0.8-1.0份和硅溶胶3.5-4.0份。
上述一种用于铝合金涂料,按照重量份由以下原料组成:凹凸棒土30-38份、乙烯-醋酸乙烯酯10-18份、附着力促进剂1-2份、刚玉粉25-28份、乙醇30-38份、海藻酸钠0.8-0.9份和硅溶胶3.5-3.8份。
上述一种用于铝合金涂料,按照重量份由以下原料组成:凹凸棒土35份、乙烯-醋酸乙烯酯15份、附着力促进剂2份、刚玉粉28份、乙醇35份、海藻酸钠0.9份和硅溶胶3.8份。
与现有技术相比,本发明的有益效果是:
本发明一种用于铝合金涂料具备较好的粘度,良好的高温抗裂性和高温强度,能有效地防止铸造缺陷。
具体实施方式
下面结合具体实施方式对本专利的技术方案作进一步详细地说明。
实施例1
一种用于铝合金涂料,按照重量份由以下原料组成:凹凸棒土30份、乙烯-醋酸乙烯酯10份、附着力促进剂1份、刚玉粉25份、乙醇30份、海藻酸钠0.8份和硅溶胶3.5份。
实施例2
一种用于铝合金涂料,按照重量份由以下原料组成:凹凸棒土40份、乙烯-醋酸乙烯酯20份、附着力促进剂3份、刚玉粉30份、乙醇40份、海藻酸钠1.0份和硅溶胶4.0份。
实施例3
一种用于铝合金涂料,按照重量份由以下原料组成:凹凸棒土35份、乙烯-醋酸乙烯酯15份、附着力促进剂2份、刚玉粉28份、乙醇35份、海藻酸钠0.9份和硅溶胶3.8份。
本发明一种用于铝合金涂料具备较好的粘度,良好的高温抗裂性和高温强度,能有效地防止铸造缺陷。
上面对本专利的较佳实施方式作了详细说明,但是本专利并不限于上述实施方式,在本领域的普通技术人员所具备的知识范围内,还可以在不脱离本专利宗旨的前提下做出各种变化。

Claims (3)

1.一种用于铝合金涂料,其特征在于,按照重量份由以下原料组成:凹凸棒土30-40份、乙烯-醋酸乙烯酯10-20份、附着力促进剂1-3份、刚玉粉25-30份、乙醇30-40份、海藻酸钠0.8-1.0份和硅溶胶3.5-4.0份。
2.根据权利要求1所述一种用于铝合金涂料,其特征在于,按照重量份由以下原料组成:凹凸棒土30-38份、乙烯-醋酸乙烯酯10-18份、附着力促进剂1-2份、刚玉粉25-28份、乙醇30-38份、海藻酸钠0.8-0.9份和硅溶胶3.5-3.8份。
3.根据权利要求1所述一种用于铝合金涂料,其特征在于,按照重量份由以下原料组成:凹凸棒土35份、乙烯-醋酸乙烯酯15份、附着力促进剂2份、刚玉粉28份、乙醇35份、海藻酸钠0.9份和硅溶胶3.8份。
CN201711276083.7A 2017-12-06 2017-12-06 一种用于铝合金涂料 Withdrawn CN108555228A (zh)